# US 2022/0037476 A1 · Manufacturing method for gate electrode and thin film transistor and display panel

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0037476 A1
- Document ID: US20220037476A1
- Status: Published application
- Kind: A1
- Application number: 17/383,394
- Filed: 2021-07-22
- Published: 2022-02-03
- Earliest claimed: 2020-07-30
- Assignees: Beihai Hkc Optoelectronics Technology Co., Ltd.; Hkc Corporation Limited
- Applicants: Beihai HKC Optoelectronics Technology Co., Ltd.; Hkc Corporation Limited
- Inventors: En-Tsung CHO; Yuming XIA; Wei LI
- Web page: https://patentgrep.com/patent/US20220037476A1

## CPC

- H10D 64/01: Manufacture or treatment
- C23C 14/14: Metallic material, boron or silicon
- C23C 14/35: by application of a magnetic field, e.g. magnetron sputtering {(C23C14/3457 takes precedence)}
- C23C 14/5873: {Removal of material}
- C23C 16/14: Deposition of only one other metal element
- C23C 16/16: from metal carbonyl compounds
- C23C 16/45527: {characterized by the ALD cycle, e.g. different flows or temperatures during half-reactions, unusual pulsing sequence, use of precursor mixtures or auxiliary reactants or activations}
- C23C 16/45553: {characterized by the use of precursors specially adapted for ALD}
- C23C 16/56: After-treatment
- C23C 28/02: only coatings {only including layers} of metallic material
- C23C 28/023: {only coatings of metal elements only}
- H10D 30/673: {characterised by the shapes, relative sizes or dispositions of the gate electrodes}
- H10D 30/6739: {Conductor-insulator-semiconductor electrodes}
- H10D 86/40: characterised by multiple TFTs
- H10D 86/60: wherein the TFTs are in active matrices
- G02F 1/13439: {characterised by their electrical, optical, physical properties; materials therefor; method of making}
- G02F 1/1368: in which the switching element is a three-electrode device {(G02F1/136277 takes precedence)}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS

## Abstract

The present application discloses a manufacturing method for a gate electrode and a thin film transistor, and a display panel, including: depositing an aluminum film on a substratum by physical vapor deposition; depositing a molybdenum film over the aluminum film by atomic layer deposition; and etching the aluminum film and the molybdenum film to form the gate electrode of a predetermined pattern.

## Claims

### Claim 1

A manufacturing method for a gate electrode, comprising:
depositing an aluminum film on a substratum by physical vapor deposition;
depositing a molybdenum film over the aluminum film by atomic layer deposition; and
etching the aluminum film and the molybdenum film to form the gate electrode of a predetermined pattern.

### Claim 2 (depends on 1)

The manufacturing method for the gate electrode according to claim 1, wherein the thickness of the deposited aluminum film is 3500 Å-4500 Å.

### Claim 3 (depends on 1)

The manufacturing method for the gate electrode according to claim 1, wherein depositing the molybdenum film over the aluminum film by atomic layer deposition comprising:
placing the substratum with the aluminum film in a reaction chamber of an atomic layer deposition apparatus;
continuously introducing a molybdenum precursor for a preset time period into the atomic layer deposition apparatus, remaining the molybdenum precursor for a preset time period after the introduction, and introducing an inert gas for purging;
continuously introducing a reducing gas for a preset time into the atomic layer deposition apparatus, remaining the reducing gas for a preset time period after the introduction, and introducing the inert gas for purging; and
repeating the steps B and C for a preset number of times to form the molybdenum film.

### Claim 4 (depends on 3)

The manufacturing method for the gate electrode according to claim 3, wherein the molybdenum precursor is at least one of molybdenum hexacarbonyl, molybdenum chloride, molybdenum fluoride; the reducing gas comprises a plasma H2;
the inert gas comprises at least one of argon and helium.

### Claim 5 (depends on 3)

The manufacturing method for the gate electrode according to claim 3, wherein the temperature in the reaction chamber of the atomic layer deposition apparatus is 400-600° C., and the vacuum degree in the reaction chamber of the atomic layer deposition apparatus is 0.01-0.05 torr.

### Claim 6 (depends on 3)

The manufacturing method for the gate electrode according to claim 3, wherein the preset time period for continuously introducing the molybdenum precursor is between 0.01 and 0.5 seconds;
the preset time period for remaining the molybdenum precursor after the introduction is 2-20 s;
the preset time period for introducing the reducing gas is between 0.005 and 0.3 seconds;
the preset time period for remaining the reducing gas after the introduction is 2-20 s;
the time for introducing the inert gas for purging is between 5 and 30 seconds;
the preset number of times is 30-1000.

### Claim 7 (depends on 6)

The manufacturing method for the gate electrode according to claim 6, wherein the preset time period for continuously introducing the molybdenum precursor is 0.02 s.

### Claim 8 (depends on 6)

The manufacturing method for the gate electrode according to claim 6, wherein the rate for introducing the molybdenum precursor is 20 sccm, and the molybdenum precursor and the reducing gas are introduced at the same rate.

### Claim 9 (depends on 6)

The manufacturing method for the gate electrode according to claim 6, wherein the preset number of cycles is 50.

### Claim 10 (depends on 6)

The manufacturing method for the gate electrode according to claim 6, wherein the reducing gas reduces the molybdenum precursor to elemental molybdenum, and the reducing gas is carbon monoxide.

### Claim 11 (depends on 1)

The manufacturing method for the gate electrode according to claim 1, wherein the thickness of the aluminum film is greater than that of the molybdenum film.

### Claim 12 (depends on 1)

The manufacturing method for the gate electrode according to claim 1, wherein the thickness of the deposited aluminum film is 100 Å-450 Å.

### Claim 13 (depends on 1)

The manufacturing method for the gate electrode according to claim 1, wherein the physical vapor deposition is performed by magnetron sputtering, the magnetron sputtering employs DC/AC sputtering, and argon is used as the sputtering gas.

### Claim 14

A manufacturing method for a thin film transistor, comprising:
forming an aluminum film on a substrate through magnetron sputtering;
placing the substratum with the aluminum film in a reaction chamber of an atomic layer deposition apparatus;
continuously introducing a precursor for a preset time period into the atomic layer deposition apparatus, remaining for a preset time period after the introduction, and introducing an inert gas for purging;
continuously introducing a reducing gas for a preset time into the atomic layer deposition apparatus, remaining for a preset time period after the introduction, and introducing the inert gas for purging;
repeating the steps S3 and S4 for a preset number of times to form the molybdenum film;
etching the aluminum film and the molybdenum film to form the gate electrode of a predetermined pattern; and
sequentially forming an insulating layer, a semiconductor layer, source and drain electrodes and a passivation layer above the gate electrode to form the thin film transistor.

### Claim 15

A display panel comprising a thin film transistor, the display panel comprising:
a first substrate, and
a second substrate disposed opposite to the first substrate, wherein
the second substrate is provided with a plurality of the thin film transistors, the second substrate comprises a substratum;
the thin film transistor comprises a gate electrode, an insulating layer, a semiconductor layer, source and drain electrodes and a passivation layer,
the insulating layer, the semiconductor layer, the source and drain electrodes and the passivation layer are sequentially positioned above the gate electrode,
the gate electrode comprises an aluminum film and a molybdenum film, the aluminum film is provided above the substrate, and the molybdenum film is provided above the aluminum film; and
the aluminum film is formed by physical vapor deposition, and the molybdenum film is formed by atomic layer deposition.

### Claim 16 (depends on 15)

The display panel according to claim 15, wherein the insulating layer is a gate insulating layer, and the semiconductor layer is an active layer and an ohmic contact layer.

### Claim 17 (depends on 15)

The display panel according to claim 15, wherein the source and drain electrodes have a stack-up structure of an aluminum film and a molybdenum film, the aluminum film is formed by physical vapor deposition, and the molybdenum film is formed as a laminated structure of a molybdenum film by atomic layer deposition.