# US 2022/0037402 A1 · Efficient fabrication of memory structures

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0037402 A1
- Document ID: US20220037402A1
- Status: Published application
- Kind: A1
- Application number: 16/940,774
- Filed: 2020-07-28
- Published: 2022-02-03
- Earliest claimed: 2020-07-28
- Assignees: Micron Technology, Inc.
- Applicants: Micron Technology, Inc.
- Inventors: Don Koun Lee; Kevin Lee Baker; Lei Wei
- Web page: https://patentgrep.com/patent/US20220037402A1

## CPC

- H10B 63/84: {arranged in a direction perpendicular to the substrate, e.g. 3D cell arrays}
- H10N 70/063: {by etching of pre-deposited switching material layers, e.g. lithography}
- H10N 70/231: {based on solid-state phase change, e.g. between amorphous and crystalline phases, Ovshinsky effect}
- H10N 70/826: {adapted for essentially vertical current flow, e.g. sandwich or pillar type devices}
- H10N 70/841: {Electrodes}
- H10N 70/882: {Compounds of sulfur, selenium or tellurium, e.g. chalcogenides}
- H10B: ELECTRONIC MEMORY DEVICES
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR

## Abstract

Methods, systems, and devices for efficient fabrication of memory structures are described. A multi-deck memory device may be fabricated using a sequence of fabrication steps that include depositing a first metal layer, depositing a cell layer on the first metal layer to form memory cells of the first memory deck, and depositing a second metal layer on the cell layer. The second metal layer may be deposited using a single deposition process rather than using multiple deposition processes. A second memory deck may be formed on the second metal layer such that stacked memory cells from the first and second deck share the use of the second metal layer. Using a single deposition process for the second metal layer may decrease the quantity of fabrication steps used to fabricate the multi-deck memory array and reduce or eliminate the exposure of the cell material to metal etchants.

## Claims

### Claim 1

A method, comprising:
depositing a first metal material on a substrate to form a first metal layer corresponding to a first access line associated with accessing a first memory cell;
depositing at least a first cell material on the first metal layer to form a cell layer comprising the first memory cell;
depositing, using a single deposition process, a second metal material on the cell layer to form a second metal layer corresponding to a second access line associated with accessing the first memory cell; and
forming a second memory cell on a portion of the second metal layer, wherein the second access line is further associated with accessing the second memory cell.

### Claim 2 (depends on 1)

The method of claim 1, wherein depositing the at least the first cell material comprises:
depositing a first electrode material on the first metal layer to form a first electrode layer;
depositing a cell storage material on the first electrode layer to form a cell storage layer; and
depositing a second electrode material on the cell storage layer to form a second electrode layer, wherein the cell layer comprises the first electrode layer, the cell storage layer, and the second electrode layer.

### Claim 3 (depends on 2)

The method of claim 2, further comprising:
depositing, before forming the second memory cell, a first mask material on the second metal layer to form a first mask layer;
performing a first etching process before forming the second memory cell to remove a first portion of the first mask layer, a first portion of the second metal layer, a first portion of the first electrode layer, a first portion of the cell storage layer, and a first portion of the second electrode layer; and
wherein the first memory cell comprises a second portion of the first electrode layer, a second portion of the cell storage layer, and a second portion of the second electrode layer.

### Claim 4 (depends on 3)

The method of claim 3, further comprising:
depositing, after performing the first etching process, a sealing material on a surface of a first stack comprising a remaining portion of the first mask layer, a remaining portion of the first metal layer, and the first memory cell; and
performing a removal procedure to remove a first portion of the sealing material and the remaining portion of the first mask layer to expose a surface of the remaining portion of the second metal layer, wherein forming the second memory cell on the second metal layer comprises forming the second memory cell on the surface of the second metal layer.

### Claim 5 (depends on 4)

The method of claim 4, further comprising:
depositing a dielectric material on the sealing material before performing the removal procedure, wherein the performing the removal procedure comprises removing a first portion of the dielectric material.

### Claim 6 (depends on 5)

The method of claim 5, wherein:
performing the removal procedure comprises performing a planarization process to generate a planar surface comprising the surface of the remaining portion of the second metal layer and a surface of a remaining portion of the dielectric material.

### Claim 7 (depends on 6)

The method of claim 6, wherein forming the second memory cell comprises:
depositing the first electrode material on the planar surface to form a third electrode layer;
depositing the cell storage material on the third electrode layer to form a second cell storage layer;
depositing the second electrode material on the second cell storage layer to form the second electrode layer;
depositing the first mask material on the second electrode layer to form a second mask layer; and
performing a second etching process to remove a first portion of the second mask layer, a first portion of the third electrode layer, a first portion of the second cell storage layer, and a first portion of a fourth electrode layer, wherein the second memory cell comprises a remaining portion of the third electrode layer, a remaining portion of the second cell storage layer, and a remaining portion of the fourth electrode layer.

### Claim 8 (depends on 7)

The method of claim 7, further comprising:
depositing, after performing the second etching process, a second sealing material on a surface of a second stack comprising a remaining portion of the second mask layer and the second memory cell;
depositing a second dielectric material on the second sealing material; and
performing a second removal procedure to remove a first portion of the second sealing material, the remaining portion of the second mask layer, and a first portion of the second dielectric material to expose a second surface.

### Claim 9 (depends on 8)

The method of claim 8, further comprising:
depositing a third metal material on the second surface to form a third metal layer corresponding to a third access line associated with accessing the second memory cell.

### Claim 10 (depends on 2)

The method of claim 2, wherein the first electrode material comprises a conductive carbon material and the second electrode material comprises the conductive carbon material.

### Claim 11 (depends on 2)

The method of claim 2, wherein the cell storage material comprises a chalcogenide material.

### Claim 12 (depends on 1)

The method of claim 1, wherein the second metal layer comprises a quantity of the second metal material deposited using the single deposition process and excludes any additional quantity of the second metal material.

### Claim 13 (depends on 1)

The method of claim 1, wherein the first metal material and the second metal material comprise tungsten.

### Claim 14

An apparatus, comprising:
a first metal layer formed on a substrate based at least in part on a first deposition process, the first metal layer corresponding to a first access line associated with accessing a first memory cell;
the first memory cell formed on the first metal layer;
a second metal layer formed, using a single second deposition process, on the first memory cell, the second metal layer corresponding to a second access line associated with the first memory cell; and
a second memory cell formed on the second metal layer.

### Claim 15 (depends on 14)

The apparatus of claim 14, wherein the second access line is further associated with accessing the second memory cell.

### Claim 16 (depends on 14)

The apparatus of claim 14, wherein the single second deposition process comprises a deposition of a quantity of a metal material and excludes any additional quantity of the metal material.

### Claim 17 (depends on 14)

The apparatus of claim 14, further comprising:
a third metal layer formed on the second memory cell, the third metal layer corresponding to a third access line associated with accessing the second metal layer.

### Claim 18 (depends on 14)

The apparatus of claim 14, wherein the first memory cell comprises a chalcogenide material for storing a state of the first memory cell.

### Claim 19 (depends on 14)

The apparatus of claim 14, wherein the first metal layer and the second metal layer comprise tungsten.

### Claim 20 (depends on 14)

The apparatus of claim 14, wherein the first access line comprises a word line or a bit line.

### Claim 21 (depends on 14)

The apparatus of claim 14, wherein the second access line comprises a word line or a bit line.

### Claim 22

A memory device, comprising:
a plurality of pillars arranged in a three-dimensional cross-point architecture, each pillar comprising;
a first memory cell coupled with a first access line and with a second access line; and
a second memory cell coupled with the second access line and with a third access line, wherein the second access line comprises a quantity of a metal material deposited during a single deposition process.

### Claim 23 (depends on 22)

The memory device of claim 22, wherein the first access line, the second access line, and the third access line each correspond to one of a word line or a bit line.

### Claim 24 (depends on 22)

The memory device of claim 22, wherein the first access line comprises a second quantity of the metal material deposited during a second deposition process before the single deposition process.

### Claim 25 (depends on 22)

The memory device of claim 22, wherein the first memory cell comprises a chalcogenide material for storing a state of the first memory cell, and the metal material comprises tungsten.