# US 2022/0037392 A1 · Display panel and manufacturing method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0037392 A1
- Document ID: US20220037392A1
- Status: Published application
- Kind: A1
- Application number: 17/358,012
- Filed: 2021-06-25
- Published: 2022-02-03
- Earliest claimed: 2020-07-29
- Assignees: Beihai Hkc Optoelectronics Technology Co., Ltd.; Hkc Corporation Limited
- Applicants: Beihai HKC Optoelectronics Technology Co., Ltd.; HKC Corporation Limited
- Inventors: EN-TSUNG CHO; Jie Ding; Je-Hao Hsu; Lidan Ye
- Web page: https://patentgrep.com/patent/US20220037392A1

## CPC

- C25D 11/08: containing inorganic acids
- C25D 11/10: containing organic acids
- C25D 11/12: Anodising more than once, e.g. in different baths
- C25D 11/16: Pretreatment {, e.g. desmutting}
- G06V 40/1318: {using electro-optical elements or layers, e.g. electroluminescent sensing}
- H10F 39/024: {of coatings or optical elements}
- H10F 39/806: {Optical elements or arrangements associated with the image sensors}
- H10K 59/65: OLEDs integrated with inorganic image sensors
- H10K 59/878: {comprising reflective means}
- H10K 71/00: Manufacture or treatment specially adapted for the organic devices covered by this subclass
- H10K 2102/00: Constructional details relating to the organic devices covered by this subclass
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- G06V: IMAGE OR VIDEO RECOGNITION OR UNDERSTANDING
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- H10K: ORGANIC ELECTRIC SOLID-STATE DEVICES

## Abstract

The present application discloses a display panel and a manufacturing method therefor, and the method includes steps of: forming a photosensitive element layer, forming a light collimating layer on the photosensitive element layer, and forming an active light-emitting matrix layer on the light collimating layer; where the step of forming the light collimating layer includes: providing a metal substrate, putting the metal substrate into an electrolyte, and preparing a porous oxidized metal as the light collimating layer by a two-step oxidation method.

## Claims

### Claim 1

A manufacturing method for a display panel, comprising steps of:
forming a photosensitive element layer;
forming a light collimating layer on the photosensitive element layer; and
forming an active light-emitting matrix layer on the light collimating layer;
wherein the step of forming a light collimating layer on the photosensitive element layer comprises:
providing a metal substrate; and
putting the metal substrate into an electrolyte, and preparing a porous oxidized metal as the light collimating layer by a two-step oxidation method.

### Claim 2 (depends on 1)

The manufacturing method for a display panel according to claim 1, wherein before the step of putting the metal substrate into an electrolyte and preparing a porous oxidized metal as the light collimating layer by a two-step oxidation method, the method further comprises steps of:
putting the metal substrate into ethanol, and carrying out ultrasonic oscillation for a first preset time; and
taking out the metal substrate, annealing the metal substrate in an oven at a preset temperature for a second preset time, and taking out the metal substrate after cooling.

### Claim 3 (depends on 2)

The manufacturing method for a display panel according to claim 2, wherein the first preset time is 3-6 minutes, the second preset time is 1-3 hours, and the preset temperature is 400-600° C.

### Claim 4 (depends on 1)

The manufacturing method for a display panel according to claim 1, wherein the electrolyte comprises any one of phosphoric acid, oxalic acid and sulfuric acid.

### Claim 5 (depends on 4)

The manufacturing method for a display panel according to claim 4, wherein the phosphoric acid has a concentration of 0.1-0.5 mol/L, the oxalic acid has a concentration of 0.2-0.8 mol/L, and the sulfuric acid has a concentration of 0.2-0.6 mol/L.

### Claim 6 (depends on 1)

The manufacturing method for a display panel according to claim 1, wherein the current density of the electrolysis is 1-35 A/cm2.

### Claim 7 (depends on 1)

The manufacturing method for a display panel according to claim 1, wherein the metal substrate comprises an aluminum substrate, the aluminum substrate has a purity of 99.99% or greater, and the porous oxidized metal comprises a porous alumina.

### Claim 8

A manufacturing method for a display panel, comprising steps of:
forming a photosensitive element layer;
forming a light collimating layer on the photosensitive element layer; and
forming an active light-emitting matrix layer on the light collimating layer;
wherein the step of forming a light collimating layer comprises:
providing an aluminum substrate, putting the aluminum substrate into ethanol, and carrying out ultrasonic oscillation for 5 minutes;
taking out the aluminum substrate, annealing the aluminum substrate in an oven at 500° C. for 2 hours, and taking out the aluminum substrate after cooling; and
putting the aluminum substrate into an electrolyte, and preparing a porous alumina as the light collimating layer by a two-step oxidation method.

### Claim 9 (depends on 8)

The manufacturing method for a display panel according to claim 8, wherein the electrolyte comprises any one of phosphoric acid, oxalic acid and sulfuric acid.

### Claim 10 (depends on 9)

The manufacturing method for a display panel according to claim 9, wherein the phosphoric acid has a concentration of 0.1-0.5 mol/L, the oxalic acid has a concentration of 0.2-0.8 mol/L, and the sulfuric acid has a concentration of 0.2-0.6 mol/L.

### Claim 11 (depends on 9)

The manufacturing method for a display panel according to claim 9, wherein the current density of the electrolysis is 1-10 A/cm2.

### Claim 12

A display panel, comprising:
a photosensitive element layer;
a light collimating layer formed on the photosensitive element layer; and
an active light-emitting matrix layer formed on the light collimating layer;
wherein the light collimating layer is a porous oxidized metal.

### Claim 13 (depends on 12)

The display panel according to claim 12, wherein the light collimating layer comprises a plurality of through pores perpendicular to the photosensitive element layer, the through pore having a pore diameter of 10-70 um and a pore depth of 70-500 um.

### Claim 14 (depends on 12)

A display panel according to claim 12, wherein the light collimating layer comprises a plurality of through pores perpendicular to the photosensitive element layer, the photosensitive element layer comprises a plurality of photosensitive elements, and the photosensitive elements are disposed in one-to-one correspondence with the through pores.

### Claim 15 (depends on 12)

The display panel according to claim 12, wherein the light collimating layer comprises a plurality of through pores perpendicular to the photosensitive element layer and having uniform gaps therebetween, the through pores are light transmission regions capable of filtering light to be detected into parallel light or quasi-parallel light, and regions of the light collimating layer except the through pores are non-light transmission regions.

### Claim 16 (depends on 14)

The display panel according to claim 14, wherein the active light-emitting matrix layer comprises non-light transmission regions and light transmission regions, the light transmission regions comprise light-emitting circuits, the active light-emitting matrix layer further comprises a first transparent layer and a second transparent layer, the light-emitting circuits are disposed between the first transparent layer and the second transparent layer, and the plurality of through pores are disposed in one-to-one correspondence with the plurality of light transmission regions.

### Claim 17 (depends on 12)

The display panel according to claim 12, wherein a total thickness of the active light-emitting matrix layer and the light collimating layer is less than 5 mm.

### Claim 18 (depends on 12)

The display panel according to claim 12, wherein the light collimating layer has a thickness of 70-500 um.