# US 2022/0037378 A1 · Method for manufacturing array substrate, array substrate and display device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0037378 A1
- Document ID: US20220037378A1
- Status: Published application
- Kind: A1
- Application number: 17/159,445
- Filed: 2021-01-27
- Published: 2022-02-03
- Earliest claimed: 2020-07-28
- Assignees: Beihai Hkc Optoelectronics Technology Co., Ltd.; Hkc Corporation Limited
- Applicants: Beihai Hkc Optoelectronics Technology Co., Ltd.; Hkc Corporation Limited
- Inventors: Yuming XIA; En-tsung CHO; Wei LI
- Web page: https://patentgrep.com/patent/US20220037378A1

## CPC

- H10D 86/0231: {using masks, e.g. half-tone masks}
- G03F 7/70066: {Size and form of the illuminated area in the mask plane, e.g. reticle masking blades or blinds}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)

## Abstract

Disclosed are a method for manufacturing an array substrate, an array substrate and a display device. The method includes the following operations: sequentially forming a gate, a gate insulation layer, an active layer, an ohmic contact layer and a metal layer on a base substrate; forming a photolithography mask on the metal layer, a thickness of the photolithography mask being between 1.7 μm and 1.8 μm; exposing the photolithography mask through a mask plate to make a uniformity of the photolithography mask in a half-exposed area of the mask plate reach a preset uniformity; and manufacturing the array substrate based on the exposed photolithography mask.

## Claims

### Claim 1

A method for manufacturing an array substrate, comprising the following operations:
sequentially forming a gate, a gate insulation layer, an active layer, an ohmic contact layer and a metal layer on a base substrate;
forming a photolithography mask on the metal layer, a thickness of the photolithography mask being between 1.7 μm and 1.8 μm;
exposing the photolithography mask through a mask plate to make a uniformity of the photolithography mask in a half-exposed area of the mask plate reach a preset uniformity; and
manufacturing the array substrate based on the exposed photolithography mask.

### Claim 2 (depends on 1)

The method of claim 1, wherein the operation of exposing the photolithography mask through a mask plate to make a uniformity of the photolithography mask in a half-exposed area of the mask plate reach a preset uniformity comprises:
exposing the photolithography mask through the mask plate and a photolithography machine to make the uniformity of the photolithography mask in the half-exposed area of the mask plate reach the preset uniformity, a depth of focus of the photolithography machine being between 1.8 μm and 2.0 μm.

### Claim 3 (depends on 1)

The method of claim 1, wherein the preset uniformity is between 20% and 40%.

### Claim 4 (depends on 1)

The method of claim 1, further comprising:
after exposing the photolithography mask, a thickness of the photolithography mask in the half-exposed area reaches 0.4 μm to 0.5 μm.

### Claim 5 (depends on 1)

The method of claim 1, wherein the operation of manufacturing the array substrate based on the exposed photolithography mask comprises:
etching the metal layer, the ohmic contact layer and the active layer beyond the exposed photolithography mask;
ashing the photolithography mask to remove the photolithography mask in the half-exposed area; and
sequentially etching the metal layer, the ohmic contact layer and the active layer based on the ashed photolithography mask to form the array substrate.

### Claim 6 (depends on 5)

The method of claim 5, wherein the operation of ashing the photolithography mask to remove the photolithography mask in the half-exposed area comprises:
ashing the photolithography mask for 70 seconds to 80 seconds by using oxygen to remove the photolithography mask in the half-exposed area.

### Claim 7 (depends on 5)

The method of claim 5, wherein the operation of ashing the photolithography mask to remove the photolithography mask in the half-exposed area comprises:
ashing the photolithography mask for 80 seconds to 100 seconds by using a first preset amount of sulfur hexafluoride and a second preset amount of oxygen to remove the photolithography mask in the half-exposed area, a ratio of the first preset amount and the second preset amount ranging from 1:1 to 3:1.

### Claim 8 (depends on 7)

The method of claim 7, wherein a value of the first preset amount is between 10000 sccm and 24000 sccm, and a value of the second preset amount is between 8000 sccm and 10000 sccm.

### Claim 9

An array substrate, wherein the array substrate is manufactured by a method for manufacturing the array substrate, the method comprising the following operations:
sequentially forming a gate, a gate insulation layer, an active layer, an ohmic contact layer and a metal layer on a base substrate;
forming a photolithography mask on the metal layer, a thickness of the photolithography mask being between 1.7 μm and 1.8 μm;
exposing the photolithography mask through a mask plate to make a uniformity of the photolithography mask in a half-exposed area of the mask plate reach a preset uniformity; and
manufacturing the array substrate based on the exposed photolithography mask.

### Claim 10 (depends on 9)

The array substrate of claim 9, wherein the operation of exposing the photolithography mask through a mask plate to make a uniformity of the photolithography mask in a half-exposed area of the mask plate reach a preset uniformity comprises:
exposing the photolithography mask through the mask plate and a photolithography machine to make the uniformity of the photolithography mask in the half-exposed area of the mask plate reach the preset uniformity, a depth of focus of the photolithography machine being between 1.8 μm and 2.0 μm.

### Claim 11 (depends on 9)

The array substrate of claim 9, wherein the preset uniformity is between 20% and 40%.

### Claim 12 (depends on 9)

The array substrate of claim 9, further comprising:
after exposing the photolithography mask, a thickness of the photolithography mask in the half-exposed area reaches 0.4 μm to 0.5 μm.

### Claim 13 (depends on 9)

The array substrate of claim 9, wherein the operation of manufacturing the array substrate based on the exposed photolithography mask comprises:
etching the metal layer, the ohmic contact layer and the active layer beyond the exposed photolithography mask;
ashing the photolithography mask to remove the photolithography mask in the half-exposed area; and
sequentially etching the metal layer, the ohmic contact layer and the active layer based on the ashed photolithography mask to form the array substrate.

### Claim 14 (depends on 13)

The array substrate of claim 13, wherein the operation of ashing the photolithography mask to remove the photolithography mask in the half-exposed area comprises:
ashing the photolithography mask for 70 seconds to 80 seconds by using oxygen to remove the photolithography mask in the half-exposed area.

### Claim 15 (depends on 13)

The array substrate of claim 13, wherein the operation of ashing the photolithography mask to remove the photolithography mask in the half-exposed area comprises:
ashing the photolithography mask for 80 seconds to 100 seconds by using a first preset amount of sulfur hexafluoride and a second preset amount of oxygen to remove the photolithography mask in the half-exposed area, a ratio of the first preset amount and the second preset amount ranging from 1:1 to 3:1.

### Claim 16 (depends on 15)

The array substrate of claim 15, wherein a value of the first preset amount is between 10000 sccm and 24000 sccm, and a value of the second preset amount is between 8000 sccm and 10000 sccm.

### Claim 17 (depends on 9)

A display device, wherein the display device comprises the array substrate of claim 9.