# US 2022/0037160 A1 · Processing method of wafer, protective sheet, and protective sheet laying method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0037160 A1
- Document ID: US20220037160A1
- Status: Published application
- Kind: A1
- Application number: 17/381,784
- Filed: 2021-07-21
- Published: 2022-02-03
- Earliest claimed: 2020-07-29
- Assignees: Disco Corporation
- Applicants: Disco Corporation
- Inventors: Kazuma SEKIYA
- Web page: https://patentgrep.com/patent/US20220037160A1

## CPC

- H10P 52/00: Grinding, lapping or polishing of wafers, substrates or parts of devices
- H10P 72/7402: {Wafer tapes, e.g. grinding or dicing support tapes}
- H10P 54/00: Cutting or separating of wafers, substrates or parts of devices
- H10P 72/7404: {the wafer tape being a laminate of three or more layers, e.g. including additional layers beyond a base layer and an uppermost adhesive layer}
- H10P 90/123: {by grinding or lapping}
- H10P 72/7416: {used during dicing or grinding}
- H10P 72/7422: {used to protect an active side of a device or wafer}
- H10W 72/07533: {Ultrasonic bonding, e.g. thermosonic bonding}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

There is provided a processing method of a wafer. The processing method includes a protective sheet preparation step of preparing a protective sheet including a first sheet that is thermocompression-bonded to a surface of the wafer by heating, a second sheet that is laid on the first sheet and has fluidity due to the heating, and a third sheet that is laid on the second sheet and keeps flatness even with the heating. The processing method also includes a protective sheet laying step of causing a side of the first sheet to face a front surface of the wafer and executing heating to execute thermocompression bonding to lay the protective sheet on the front surface of the wafer and a grinding step of causing a side of the protective sheet to be held by a holding surface of a chuck table and grinding a back surface of the wafer.

## Claims

### Claim 1

A processing method of a wafer, the processing method comprising:
a protective sheet preparation step of preparing a protective sheet including
a first sheet that is thermocompression-bonded to a surface of the wafer by heating,
a second sheet that is laid on the first sheet and has fluidity due to the heating, and
a third sheet that is laid on the second sheet and keeps flatness even with the heating;
a protective sheet laying step of causing a side of the first sheet to face a front surface of the wafer and executing heating to execute thermocompression bonding to lay the protective sheet on the front surface of the wafer; and
a grinding step of causing a side of the protective sheet to be held by a holding surface of a chuck table and grinding a back surface of the wafer.

### Claim 2

A protective sheet laid on a surface of a wafer, the protective sheet comprising:
a first sheet that is thermocompression-bonded to the surface of the wafer by heating;
a second sheet that is laid on the first sheet and has fluidity due to the heating; and
a third sheet that is laid on the second sheet and is allowed to keep flatness even with the heating.

### Claim 3 (depends on 2)

The protective sheet according to claim 2, wherein
the first sheet and the second sheet are configured by a polyolefin-based resin, and the third sheet is configured by a polyester-based resin.

### Claim 4 (depends on 3)

The protective sheet according to claim 3, wherein
the first sheet is configured by polypropylene, the second sheet is configured by polyethylene, and the third sheet is configured by polyethylene terephthalate.

### Claim 5

A protective sheet laying method for laying a protective sheet on a wafer by thermocompression bonding, the protective sheet including a first sheet that is thermocompression-bonded to a surface of the wafer by heating, a second sheet that is laid on the first sheet and has fluidity due to the heating, and a third sheet that is laid on the second sheet and is allowed to keep flatness even with the heating, the protective sheet laying method comprising:
a protective sheet placement step of placing the protective sheet on an upper surface of the wafer; and
a thermocompression bonding step of executing thermocompression bonding through pressing the protective sheet placed on the upper surface of the wafer and heating the protective sheet, wherein
a heating temperature when the thermocompression bonding of the protective sheet is executed in the thermocompression bonding step is a temperature at which the first sheet exerts an adhesive force, the second sheet has fluidity, and the third sheet keeps flatness.