# US 2022/0037153 A1 · Method for manufacturing semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0037153 A1
- Document ID: US20220037153A1
- Status: Published application
- Kind: A1
- Application number: 17/500,149
- Filed: 2021-10-13
- Published: 2022-02-03
- Earliest claimed: 2009-07-10
- Assignees: Semiconductor Energy Laboratory Co., Ltd.
- Applicants: Semiconductor Energy Laboratory Co., Ltd.
- Inventors: Shunpei YAMAZAKI; Miyuki HOSOBA; Kosei NODA; Hiroki OHARA; Toshinari SASAKI; Junichiro SAKATA
- Web page: https://patentgrep.com/patent/US20220037153A1

## CPC

- H10D 99/00: Subject matter not provided for in other groups of this subclass
- H10D 30/6755: {Oxide semiconductors, e.g. zinc oxide, copper aluminium oxide or cadmium stannate}
- H10P 95/90: Thermal treatments, e.g. annealing or sintering
- H10D 86/423: {comprising semiconductor materials not belonging to the Group IV, e.g. InGaZnO}
- H10D 86/60: wherein the TFTs are in active matrices
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A highly reliable semiconductor device which includes a thin film transistor having stable electric characteristics, and a manufacturing method thereof. In the manufacturing method of the semiconductor device which includes a thin film transistor where a semiconductor layer including a channel formation region is an oxide semiconductor layer, heat treatment which reduces impurities such as moisture to improve the purity of the oxide semiconductor layer and oxidize the oxide semiconductor layer (heat treatment for dehydration or dehydrogenation) is performed. Not only impurities such as moisture in the oxide semiconductor layer but also those existing in a gate insulating layer are reduced, and impurities such as moisture existing in interfaces between the oxide semiconductor layer and films provided over and under and in contact with the oxide semiconductor layer are reduced.

## Claims

### Claim 1

(canceled)

### Claim 2

A method of manufacturing a liquid crystal display comprising steps of:
forming a gate electrode over a substrate having an insulating surface;
forming a gate insulating film over the gate electrode;
forming an oxide semiconductor layer containing In, Ga, and Zn over the gate insulating film;
performing a first heat treatment on the oxide semiconductor layer in a first atmosphere;
cooling the oxide semiconductor layer in a second atmosphere after the first heat treatment;
forming a source electrode and a drain electrode over the oxide semiconductor layer after the step of cooling the oxide semiconductor layer;
forming an oxide insulating layer over the source electrode, the drain electrode and the oxide semiconductor layer;
performing a second heat treatment after forming the oxide insulating layer; and
forming a pixel electrode after the second heat treatment,
wherein the oxide insulating layer is in contact with the oxide semiconductor layer,
wherein the pixel electrode is electrically connected to the source electrode or the drain electrode, and
wherein in each of the first atmosphere and the second atmosphere a concentration of moisture or a concentration of hydrogen is low.

### Claim 3

A method of manufacturing a liquid crystal display comprising steps of:
forming a gate electrode over a substrate having an insulating surface;
forming a gate insulating film over the gate electrode;
forming an oxide semiconductor layer containing In, Ga, and Zn over the gate insulating film;
performing a first heat treatment on the oxide semiconductor layer in a first atmosphere;
cooling the oxide semiconductor layer in a second atmosphere after the first heat treatment;
forming a source electrode and a drain electrode over the oxide semiconductor layer after the step of cooling the oxide semiconductor layer;
forming an oxide insulating layer over the source electrode, the drain electrode and the oxide semiconductor layer;
performing a second heat treatment after forming the oxide insulating layer; and
forming a pixel electrode after the second heat treatment,
wherein the oxide insulating layer is in contact with the oxide semiconductor layer,
wherein the pixel electrode is electrically connected to the source electrode or the drain electrode, and
wherein moisture or hydrogen is removed from each of the first atmosphere and the second atmosphere.

### Claim 4

A method of manufacturing a liquid crystal display comprising steps of:
forming a gate electrode over a substrate having an insulating surface;
forming a gate insulating film over the gate electrode;
forming an oxide semiconductor layer containing In, Ga, and Zn over the gate insulating film;
performing a first heat treatment on the oxide semiconductor layer;
cooling the oxide semiconductor layer after the first heat treatment;
forming a source electrode and a drain electrode over the oxide semiconductor layer after the step of cooling the oxide semiconductor layer;
forming an oxide insulating layer over the source electrode, the drain electrode and the oxide semiconductor layer;
performing a second heat treatment after forming the oxide insulating layer; and
forming a pixel electrode after the second heat treatment,
wherein the oxide insulating layer is in contact with the oxide semiconductor layer,
wherein the pixel electrode is electrically connected to the source electrode or the drain electrode, and
wherein the first heating and the cooling are performed in an atmosphere in which a concentration of moisture or a concentration of hydrogen is reduced by an apparatus for removing moisture or hydrogen.

### Claim 5

A method of manufacturing a liquid crystal display comprising steps of:
forming a gate electrode over a substrate having an insulating surface;
forming a gate insulating film over the gate electrode;
forming an oxide semiconductor layer containing In, Ga, and Zn over the gate insulating film;
performing a first heat treatment on the oxide semiconductor layer;
cooling the oxide semiconductor layer after the first heat treatment;
forming a source electrode and a drain electrode over the oxide semiconductor layer after the step of cooling the oxide semiconductor layer;
forming an oxide insulating layer over the source electrode, the drain electrode and the oxide semiconductor layer;
performing a second heat treatment after forming the oxide insulating layer; and
forming a pixel electrode after the second heat treatment,
wherein the oxide insulating layer is in contact with the oxide semiconductor layer,
wherein the pixel electrode is electrically connected to the source electrode or the drain electrode, and
wherein the first heating and the cooling are performed in an atmosphere from which moisture or hydrogen has been removed by an apparatus for removing moisture or hydrogen.

### Claim 6 (depends on 2)

The method of manufacturing according claim 2,
wherein the first heating is heating for dehydration or dehydrogenation of the oxide semiconductor layer.

### Claim 7 (depends on 2)

The method of manufacturing according claim 2,
wherein the first heat treatment is performed at a temperature equal to or higher than 400° C. and equal to or lower than 700° C.

### Claim 8 (depends on 2)

The method of manufacturing according claim 2,
wherein the cooling of the oxide semiconductor layer is performed at a temperature higher than or equal to room temperature and lower than 100° C.

### Claim 9 (depends on 3)

The method of manufacturing according claim 3,
wherein the first heating is heating for dehydration or dehydrogenation of the oxide semiconductor layer.

### Claim 10 (depends on 3)

The method of manufacturing according claim 3,
wherein the first heat treatment is performed at a temperature equal to or higher than 400° C. and equal to or lower than 700° C.

### Claim 11 (depends on 3)

The method of manufacturing according claim 3,
wherein the cooling of the oxide semiconductor layer is performed at a temperature higher than or equal to room temperature and lower than 100° C.

### Claim 12 (depends on 4)

The method of manufacturing according claim 4,
wherein the first heating is heating for dehydration or dehydrogenation of the oxide semiconductor layer.

### Claim 13 (depends on 4)

The method of manufacturing according claim 4,
wherein the first heat treatment is performed at a temperature equal to or higher than 400° C. and equal to or lower than 700° C.

### Claim 14 (depends on 4)

The method of manufacturing according claim 4,
wherein the cooling of the oxide semiconductor layer is performed at a temperature higher than or equal to room temperature and lower than 100° C.

### Claim 15 (depends on 5)

The method of manufacturing according claim 5,
wherein the first heating is heating for dehydration or dehydrogenation of the oxide semiconductor layer.

### Claim 16 (depends on 5)

The method of manufacturing according claim 5,
wherein the first heat treatment is performed at a temperature equal to or higher than 400° C. and equal to or lower than 700° C.

### Claim 17 (depends on 5)

The method of manufacturing according claim 5,
wherein the cooling of the oxide semiconductor layer is performed at a temperature higher than or equal to room temperature and lower than 100° C.