# US 2022/0037151 A1 · Composition and methods using same for carbon doped silicon containing films

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0037151 A1
- Document ID: US20220037151A1
- Status: Published application
- Kind: A1
- Application number: 17/501,903
- Filed: 2021-10-14
- Published: 2022-02-03
- Earliest claimed: 2016-07-27
- Assignees: Versum Materials US, LLC
- Applicants: Versum Materials US, LLC
- Inventors: HARIPIN CHANDRA; XINJIAN LEI; ANUPAMA MALLIKARJUNAN; MOO-SUNG KIM
- Web page: https://patentgrep.com/patent/US20220037151A1

## CPC

- H10P 14/6681: {the precursor containing a compound comprising Si}
- C23C 16/308: {Oxynitrides}
- C23C 16/345: {Silicon nitride}
- C23C 16/402: {Silicon dioxide}
- C23C 16/45525: {Atomic layer deposition [ALD]}
- C23C 16/45553: {characterized by the use of precursors specially adapted for ALD}
- C23C 16/56: After-treatment
- H10P 14/6339: {deposition by cyclic CVD, e.g. ALD, ALE or pulsed CVD}
- H10P 14/6522: {introduced into a nitride material, e.g. changing SiN to SiON}
- H10P 14/6529: {by exposure to a gas or vapour}
- H10P 14/6532: {by exposure to a plasma}
- H10P 14/6682: {the compound being a silane, e.g. disilane, methylsilane or chlorosilane}
- H10P 14/683: {carbon-based polymeric organic materials, e.g. polyimides, poly cyclobutene or PVC}
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10P 14/6922: {the material containing Si, O and at least one of H, N, C, F or other non-metal elements, e.g. SiOC, SiOC:H or SiONC}
- H10P 14/69433: {the material being a silicon nitride not containing oxygen, e.g. SixNy or SixByNz}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

A composition and method for using the composition in the fabrication of an electronic device are disclosed. Compounds, compositions and methods for depositing a low dielectric constant (<4.0) and high oxygen ash resistance silicon-containing film such as, without limitation, a carbon doped silicon oxide, are disclosed.

## Claims

### Claim 1

A method for forming a carbon doped silicon oxide film having carbon content ranging from 15 at. % to 30 at. % via a thermal ALD process, the method comprising:
a) placing one or more substrates comprising a surface feature into a reactor;
b) heating to reactor to one or more temperatures ranging from ambient temperature to about 550° C. and optionally maintaining the reactor at a pressure of 100 torr or less;
c) introducing into the reactor at least one silicon precursor having two Si—C—Si linkages selected from the group consisting of 1-chloro-1,3-disilacyclobutane, 1-bromo-1,3-disilacyclobutane, 1,3-dichloro-1,3-1,3-disilacyclobutane, 1,3-dibromo-1,3-disilacyclobutane, 1,1,3-trichloro-1,3-disilacyclobutane, 1,1,3-tribromo-1,3-disilacyclobutane, 1,1,3,3-tetrachloro-1,3-disilacyclobutane, 1,1,3,3-tetrabromo-1,3-disilacyclobutane, 1,3-dichloro-1,3-dimethyl-1,3-disilacyclobutane, 1,3-bromo-1,3-dimethyl-1,3-disilacyclobutane, 1,1,1,3,3,5,5,5-octachloro-1,3,5-trisilapentane, 1,1,3,3,5,5-hexachloro-1,5-dimethyl-1,3,5-trisilapentane, 1,1,1,5,5,5-hexachloro-3,3-dimethyl-1,3,5-trisilapentane, 1,1,3,5,5-pentachloro-1,3,5-trimethyl-1,3,5-trisilapentane, 1,1,1,5,5,5-hexachloro-1,3,5-trisilapentane, 1,1,5,5-tetraachloro-1,3,5-trisilapentane;
d) purging with an inert gas;
e) providing a nitrogen source into the reactor to react with the surface to form a carbon doped silicon nitride film;
f) purging with inert gas to remove reaction by-products;
g) repeating steps c to f to provide a desired thickness of a resulting carbon doped silicon nitride;
h) treating the resulting carbon doped silicon nitride film with an oxygen source at one or more temperatures ranging from about ambient temperature to 1000° C. to convert the carbon doped silicon nitride film into a carbon doped silicon oxide film; and
i) providing post-deposition exposing the carbon doped silicon oxide film to a plasma comprising hydrogen.

### Claim 2 (depends on 1)

A film formed according to the method of claim 1 having a dielectric constant of less than about 4, and a carbon content of at least about 10 at. %.

### Claim 3 (depends on 1)

A film formed according to the method of claim 1 having an etch rate of at least 0.5 times less than thermal silicon oxide, wherein the etch rate is measured with diluted HF.

### Claim 4 (depends on 1)

A film formed according to the method of claim 1 having an etch rate of at least 0.1 times less than thermal silicon oxide, wherein the etch rate is measured with diluted HF.

### Claim 5 (depends on 1)

A film formed according to the method of claim 1 having an etch rate of at least 0.05 times less than thermal silicon oxide, wherein the etch rate is measured with diluted HF.

### Claim 6 (depends on 1)

A film formed according to the method of claim 1 having an etch rate of at least 0.01 times less than thermal silicon oxide, wherein the etch rate is measured with diluted HF.

### Claim 7 (depends on 1)

A film formed according to the method of claim 1 having a damage layer of 50 Å or less following an oxygen ashing process.

### Claim 8 (depends on 1)

A film formed according to the method of claim 1 having a damage layer of 20 Å or less following an oxygen ashing process.

### Claim 9 (depends on 1)

A film formed according to the method of claim 1 having a damage layer of 10 Å or less following an oxygen ashing process.

### Claim 10 (depends on 1)

A film formed according to the method of claim 1 having a damage layer of 5 Å or less following an oxygen ashing process.

### Claim 11 (depends on 1)

The method according to claim 1 wherein the step h) of treating the resulting carbon doped silicon nitride film with an oxygen source is performed at one or more temperatures ranging from or from about 100° C. to 400° C.

### Claim 12

A method for forming a carbon doped silicon oxide film having carbon content ranging from 15 at % to 30 at. % via a thermal ALD process, the method comprising the method comprising:
a. placing one or more substrates comprising a surface feature into a reactor;
b. heating the reactor to one or more temperatures ranging from ambient temperature to about 150° C. and optionally maintaining the reactor at a pressure of 100 torr or less;
c. introducing into the reactor at least precursor having two Si—C—Si linkages selected from the group consisting of 1-chloro-1,3-disilacyclobutane, 1-bromo-1,3-disilacyclobutane, 1,3-dichloro-1,3-1,3-disilacyclobutane, 1,3-dibromo-1,3-disilacyclobutane, 1,1,3-trichloro-1,3-disilacyclobutane, 1,1,3-tribromo-1,3-disilacyclobutane, 1,1,3,3-tetrachloro-1,3-disilacyclobutane, 1,1,3,3-tetrabromo-1,3-disilacyclobutane, 1,3-dichloro-1,3-dimethyl-1,3-disilacyclobutane, 1,3-bromo-1,3-dimethyl-1,3-disilacyclobutane, 1,1,1,3,3,5,5,5-octachloro-1,3,5-trisilapentane, 1,1,1,3,3,5,5,5-octachloro-1,3,5-trisilapentane, 1,1,1,3,3,5,5,5-octachloro-1,5-dimethyl-1,3,5-trisilapentane, 1,1,1,5,5,5-hexachloro-3,3-dimethyl-1,3,5-trisilapentane, 1,1,3,5,5,5-pentachloro-1,3,5-trimethyl-1,3,5-trisilapentane, 1,1,1,5,5,5-hexachloro-1,3,5-trisilapentane, 1,1,5,5-tetraachloro-1,3,5-trisilapentane and a catalyst;
d. purging with an inert gas
e. providing vapors of water into the reactor to react with the precursor as well as a catalyst to form a carbon doped silicon oxide as-deposited film; and
f. purging with inert gas to remove reaction by-products;
wherein steps c to f are repeated to provide a desired thickness of carbon doped silicon oxide.

### Claim 13 (depends on 12)

The method of claim 12 further comprising post-deposition treatment of the carbon doped silicon oxide film with a thermal anneal at temperatures from 300 to 700° C.

### Claim 14 (depends on 12)

The method of claim 12 further comprising hydrogen plasma treatment of the carbon doped silicon oxide film with a plasma comprising hydrogen.