# US 2022/0037150 A1 · Spin on carbon composition and method of manufacturing a semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0037150 A1
- Document ID: US20220037150A1
- Status: Published application
- Kind: A1
- Application number: 16/984,070
- Filed: 2020-08-03
- Published: 2022-02-03
- Earliest claimed: 2020-08-03
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Co., Ltd.
- Inventors: Jing Hong HUANG; Ching-Yu CHANG; Wei-Han LAI
- Web page: https://patentgrep.com/patent/US20220037150A1

## CPC

- H10P 14/6342: {Liquid deposition, e.g. spin-coating, sol-gel techniques or spray coating}
- H10P 14/6905: {being a silicon carbide or silicon carbonitride and not containing oxygen, e.g. SiC or SiC:H}
- G03F 7/0042: {with inorganic or organometallic light-sensitive compounds not otherwise provided for, e.g. inorganic resists (G03F7/075 takes precedence)}
- G03F 7/0043: {Chalcogenides; Silicon, germanium, arsenic or derivatives thereof; Metals, oxides or alloys thereof (G03F7/0044 takes precedence)}
- G03F 7/0752: {in non photosensitive layers or as additives, e.g. for dry lithography}
- G03F 7/094: {Multilayer resist systems, e.g. planarising layers}
- H10P 14/6516: {of treatments performed after formation of the materials}
- H10P 14/683: {carbon-based polymeric organic materials, e.g. polyimides, poly cyclobutene or PVC}
- H10P 14/6902: {composed of carbon, e.g. alpha-C, diamond or hydrogen doped carbon}
- H10P 76/20: of masks comprising organic materials
- H10P 76/405: {characterised by their composition, e.g. multilayer masks}
- C09D 125/18: Homopolymers or copolymers of aromatic monomers containing elements other than carbon and hydrogen
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)

## Abstract

A method of manufacturing a semiconductor device includes forming a spin on carbon layer comprising a spin on carbon composition over a semiconductor substrate. The spin on carbon layer is first heated at a first temperature to partially crosslink the spin on carbon layer. The spin on carbon layer is second heated at a second temperature to further crosslink the spin on carbon layer. An overlayer is formed over the spin on carbon layer. The second temperature is higher than the first temperature.

## Claims

### Claim 1

A method of manufacturing a semiconductor device, comprising:
forming a spin on carbon layer comprising a spin on carbon composition over a semiconductor substrate;
first heating the spin on carbon layer at a first temperature to partially crosslink the spin on carbon layer;
second heating the spin on carbon layer at a second temperature to further crosslink the spin on carbon layer; and
forming an overlayer over the spin on carbon layer,
wherein the second temperature is higher than the first temperature.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the spin on carbon composition comprises a carbon backbone polymer, a first crosslinker, and a second crosslinker, wherein the first and second crosslinkers are different from each other.

### Claim 3 (depends on 2)

The method according to claim 2, wherein the first crosslinker is one or more selected from the group consisting of A-(OR)x, A-(NR)x,
where A is a monomer, oligomer, or a polymer having a molecular weight ranging from 100 to 20,000;
R is an alkyl group, cycloalkyl group, cycloalkylepoxy group, or C3-C15 heterocyclic group;
OR is an alkyloxy group, cycloalkyloxy group, carbonate group, alkylcarbonate group, alkyl carboxylate group, tosylate group, or mesylate group;
NR is an alkylamide group or an alkylamino group; and
x ranges from 2 to 1000.

### Claim 4 (depends on 3)

The method according to claim 3, wherein R, OR, and NR each comprise a chain structure, a ring structure, or a 3-D structure.

### Claim 5 (depends on 2)

The method according to claim 2, wherein the second crosslinker is one or more selected from the group consisting of A-(OH)x, A-(OR′)x, A-(C═C)x, and A-(C≡C)x,
where A is a monomer, oligomer, or a polymer having a molecular weight ranging from 100 to 20,000;
R′ is an alkyloxy group, an alkenyl group, or an alkynyl group; and
x ranges from 2 to 1000.

### Claim 6 (depends on 2)

The method according to claim 2, wherein a concentration of the first and second crosslinkers in the spin on carbon composition ranges from 20 wt. % to 50 wt. % of the total weight of the first and second crosslinkers and the carbon backbone polymer.

### Claim 7 (depends on 2)

The method according to claim 2, wherein the first crosslinker reacts with the carbon backbone polymer during the first heating to partially crosslink the carbon backbone polymer.

### Claim 8 (depends on 7)

The method according to claim 7, wherein the second crosslinker reacts with the first polymer during the second heating to further crosslink the carbon backbone polymer.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the first temperature ranges from 100° C. to 170° C.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the second temperature ranges from 180° C. to 300° C.

### Claim 11

A method of manufacturing a semiconductor device, comprising:
forming a bottom layer over a semiconductor substrate,
wherein the bottom layer comprises:
a carbon backbone polymer;
a first crosslinker; and
a second crosslinker;
first heating the bottom layer at a first temperature to partially crosslink the bottom layer via the first crosslinker;
second heating the bottom layer at a second temperature higher than the first temperature to further crosslink the bottom layer via the second crosslinker;
forming a middle layer over the bottom layer; and
forming a photoresist layer over the middle layer,
wherein the middle layer has a different composition than the bottom layer and photoresist layer.

### Claim 12 (depends on 11)

The method according to claim 11, wherein the first crosslinker is one or more selected from the group consisting of A-(OR)x, A-(NR)x,
where A is a monomer, oligomer, or a polymer having a molecular weight ranging from 100 to 20,000;
R is an alkyl group, cycloalkyl group, cycloalkylepoxy group, or C3-C15 heterocyclic group;
OR is an alkyloxy group, cycloalkyloxy group, carbonate group, alkylcarbonate group, alkyl carboxylate group, tosylate group, or mesylate group;
NR is an alkylamide group or an alkylamino group; and
x ranges from 2 to 1000.

### Claim 13 (depends on 11)

The method according to claim 11, wherein the second crosslinker is one or more selected from the group consisting of A-(OH)x, A-(OR′)x, A-(C═C)x, and A-(C≡C)x,
where A is a monomer, oligomer, or a polymer having a molecular weight ranging from 100 to 20,000;
R′ is an alkyloxy group, an alkenyl group, or an alkynyl group; and
x ranges from 2 to 1000.

### Claim 14 (depends on 11)

The method according to claim 11, wherein the middle layer comprises at least one selected from the group consisting of a silicon-containing material containing an inorganic polymer, a siloxane polymer, silicon oxide, silicon nitride, silicon oxynitride, polycrystalline silicon, and a metal-containing organic polymer material.

### Claim 15 (depends on 11)

The method according to claim 11, further comprising:
selectively exposing the photoresist layer to actinic radiation;
developing the selectively exposed photoresist layer to form a photoresist pattern;
extending the pattern into the middle layer and bottom layer to expose the substrate;
etching the substrate; and
removing the photoresist layer, middle layer, and bottom layer.

### Claim 16

A spin on carbon composition, comprising:
a carbon backbone polymer;
a first crosslinker; and
a second crosslinker,
wherein the first crosslinker reacts with the carbon backbone polymer to partially crosslink the first polymer at a first temperature, and the second crosslinker reacts with the first polymer to further crosslink the carbon backbone polymer at a second temperature higher than the first temperature.

### Claim 17 (depends on 16)

The spin on carbon composition of claim 16, wherein the first crosslinker is one or more selected from the group consisting of A-(OR)x, A-(NR)x,
where A is a monomer, oligomer, or a second polymer having a molecular weight ranging from 100 to 20,000;
R is an alkyl group, cycloalkyl group, cycloalkylepoxy group, or C3-C15 heterocyclic group;
OR is an alkyloxy group, cycloalkyloxy group, carbonate group, alkylcarbonate group, alkyl carboxylate group, tosylate group, or mesylate group;
NR is an alkylamide group or an alkylamino group; and
x ranges from 2 to 1000.

### Claim 18 (depends on 16)

The spin on carbon composition of claim 16, wherein the second crosslinker is one or more selected from the group consisting of A-(OH)x, A-(OR′)x, A-(C═C)x, and A-(C≡C)x,
where A is a monomer, oligomer, or a second polymer having a molecular weight ranging from 100 to 20,000;
R′ is an alkyloxy group, an alkenyl group, or an alkynyl group; and
x ranges from 2 to 1000.

### Claim 19 (depends on 16)

The spin on carbon composition of claim 16, wherein a concentration of the first and second crosslinkers ranges from 20 wt. % to 50 wt. % of the total weight of the first and second crosslinkers and the first polymer.

### Claim 20 (depends on 16)

The spin on carbon composition of claim 16, further comprising a solvent.