# US 2022/0037058 A1 · Manufacturing method for graphene film and display panel

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0037058 A1
- Document ID: US20220037058A1
- Status: Published application
- Kind: A1
- Application number: 17/383,381
- Filed: 2021-07-22
- Published: 2022-02-03
- Earliest claimed: 2020-07-29
- Assignees: Beihai Hkc Optoelectronics Technology Co., Ltd.; Hkc Corporation Limited
- Applicants: Beihai HKC Optoelectronics Technology Co., Ltd.; HKC Corporation Limited
- Inventors: Yuming Xia; En-Tsung Cho; Lidan Ye
- Web page: https://patentgrep.com/patent/US20220037058A1

## CPC

- H01B 13/0036: {Details}
- C01B 32/184: Preparation
- C08K 3/042: {Graphene or derivatives, e.g. graphene oxides}
- C25B 1/135: Carbon
- H01B 1/04: mainly consisting of carbon-silicon compounds, carbon or silicon
- H01B 1/08: oxides
- H01B 5/14: comprising conductive layers or films on insulating-supports
- H10D 86/441: {Interconnections, e.g. scanning lines}
- H10D 86/60: wherein the TFTs are in active matrices
- C08K 2201/001: Conductive additives
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C25B: ELECTROLYTIC OR ELECTROPHORETIC PROCESSES FOR THE PRODUCTION OF COMPOUNDS OR NON-METALS; APPARATUS THEREFOR (anodic or cathodic protection C23F13/00; single-crystal growth C30B)
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

The present application discloses a manufacturing method for a graphene film, a manufacturing method for a graphene material and a display panel. The manufacturing method for the graphene film includes steps of: obtaining a graphene oxide dispersion; reducing the graphene oxide dispersion to a graphene material by an electrochemical deposition method; preparing the graphene material into the graphene film.

## Claims

### Claim 1

A manufacturing, method for a graphene film, comprising steps of:
obtaining a graphene oxide dispersion;
reducing the graphene oxide dispersion to a graphene material by an electrochemical deposition method; and
preparing the graphene material into the graphene film.

### Claim 2 (depends on 1)

The manufacturing method for the graphene film according to claim 1, wherein the step of reducing the graphene oxide dispersion to a graphene material by an electrochemical deposition method comprises sub-steps of:
preparing the graphene oxide dispersion into an electrochemical deposition solution;
inserting a cathode and an anode in the electrochemical deposition solution, and conducting the cathode and the anode with a power supply to enable graphene to be attached on the cathode; and
removing the cathode to obtain the graphene material.

### Claim 3 (depends on 2)

The manufacturing method for the graphene film according to claim 2, wherein the cathode is made of nickel, and the anode is made of platinum or titanium.

### Claim 4 (depends on 2)

The manufacturing method for the graphene film according to claim 2, wherein the power supply is a pulse power supply that provides pulse voltage at a frequency of 10000 HZ to 50000 HZ, with a duty of 10% to 60%.

### Claim 5 (depends on 2)

The manufacturing method for the graphene film according to claim 2, wherein the step of removing the cathode to obtain the graphene material comprises sub-steps of:
placing the cathode with the graphene attached thereon in a ferric chloride solution for reaction to form a solid-liquid mixture;
separating solids from the solid-liquid mixture to obtain the graphene material.

### Claim 6 (depends on 2)

The manufacturing method for the graphene film according to claim 2, wherein the electrochemical deposition solution consists of the graphene oxide dispersion and a pH regulator, which is citric acid and sodium citrate with a pH value of 2 to 6.

### Claim 7 (depends on 1)

The manufacturing method for the graphene film according to claim 1, wherein the step of obtaining a graphene oxide dispersion comprises sub-steps of:
preparing graphite as a raw material into a graphite oxide; and
preparing the graphite oxide into the graphene oxide dispersion.

### Claim 8 (depends on 7)

The manufacturing method for the graphene film according to claim 7, wherein the step of preparing the graphite oxide into the graphene oxide dispersion comprises sub-steps of:
mixing the graphite oxide in an acid solution for reaction to obtain a graphite oxide mixture; and
ultrasonically dispersing the graphite oxide mixture to obtain a graphene oxide dispersion.

### Claim 9 (depends on 7)

The manufacturing method for the graphene film according to claim 7, wherein the step of preparing graphite as a raw material into a graphite oxide comprises sub-steps of:
adding a mixture of graphite powder and sodium nitrate to concentrated sulfuric acid for reaction to obtain a first mixture;
adding potassium permanganate to the first mixture for reaction to obtain a second mixture;
adding deionized water to the second mixture for reaction to obtain a third mixture; and
adding hydrogen peroxide to the third mixture, and drying to obtain the graphite oxide.

### Claim 10 (depends on 1)

The manufacturing method for the graphene film according to claim 1, wherein the step of preparing the graphene material into the graphene film comprises sub-steps of:
preparing the graphene material into a graphene solution, and uniformly dispersing;
dropping the graphene solution on a substrate; and
dispersing the graphene solution dropped on the substrate into the graphene film.

### Claim 11 (depends on 9)

The manufacturing method for the graphene film according to claim 9, wherein the step of preparing the first mixture comprises placing a beaker in an ice-water bath, adding 23-30 mL of concentrated sulfuric acid, and controlling the temperature at 0-5° C.; and adding a solid mixture of 1-2 g of graphite powder and 0.2-1 g of sodium nitrate while stirring to obtain the first mixture.

### Claim 12 (depends on 9)

The manufacturing method for the graphene film according to claim 9, wherein the step of preparing the second mixture comprises adding 1-4 g of potassium permanganate in portions, controlling the reaction temperature within 20° C., removing the water bath after adding potassium permanganate, and then heating to 30-50° C. to obtain the second mixture.

### Claim 13 (depends on 12)

The manufacturing method for the graphene film according to claim 12, wherein the step of preparing the third mixture comprises stirring the second mixture for 10-60 min, then adding 400-800 mL of deionized water slowly, and heating to 50-100° C. for reaction for 10-60 min to obtain the third mixture.

### Claim 14 (depends on 13)

The manufacturing method for the graphene film according to claim 13, wherein the step of preparing the graphite oxide comprises diluting the third mixture to 100-200 mL, adding a proper amount of 30% hydrogen peroxide, stirring well, then filtering, washing awl drying to obtain the graphite oxide.

### Claim 15 (depends on 8)

The manufacturing method for the graphene film according to claim 8, wherein the acid solution is phosphoric acid, hydrochloric acid, acetic acid or other acid solution.

### Claim 16 (depends on 4)

The manufacturing method for the graphene film according to claim 4, wherein pulse waveforms of the pulse power supply are divided into rectangular waves, sawtooth waves and triangular waves.

### Claim 17 (depends on 1)

A display panel, comprising a transparent conductive layer which is a graphene film prepared by the manufacturing method for the graphene film according to claim 1 and used as pixel electrodes or common electrodes of display panels.