# US 2022/0036919 A1 · Cobalt ferrite magnetic powder, method of producing the same, and magnetic recording medium

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0036919 A1
- Document ID: US20220036919A1
- Status: Published application
- Kind: A1
- Application number: 17/430,874
- Filed: 2020-02-14
- Published: 2022-02-03
- Earliest claimed: 2019-02-15
- Assignees: Sony Group Corporation
- Applicants: Sony Group Corporation
- Inventors: Natsuki ICHISE; Masaru TERAKAWA; Katsunori MAESHIMA; Takashi KATAGUCHI; Takeshi TAKAHASHI
- Web page: https://patentgrep.com/patent/US20220036919A1

## CPC

- G11B 5/70678: {Ferrites}
- C01G 51/66: containing alkaline earth metals, e.g. SrCoO3
- H01F 1/11: in the form of particles {(for magnetic record carriers G11B5/70626)}
- H01F 1/344: {Ferrites, e.g. having a cubic spinel structure (X2+O)(Y23+O3), e.g. magnetite Fe3O4}
- C01P 2002/72: by d-values or two theta-values, e.g. as X-ray diagram
- C01P 2004/64: Nanometer sized, i.e. from 1-100 nanometer
- C01P 2006/42: Magnetic properties
- G11B: INFORMATION STORAGE BASED ON RELATIVE MOVEMENT BETWEEN RECORD CARRIER AND TRANSDUCER (recording measured values in a way that does not require playback through a transducer G01D9/00; recording or playback apparatus using mechanically marked tape, e.g. punched paper tape, or using unit records, e.g. punched or magnetically marked cards G06K; transferring data from one type of record carrier to another G06K1/18; circuits for coupling output of reproducer to radio receiver H04B1/20; gramophone pick-ups or like acoustic electromechanical transducers or circuits therefor H04R)
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS

## Abstract

[Object] A cobalt ferrite magnetic powder includes magnetic particles that have a uniaxial crystal magnetic anisotropy and contain cobalt ferrite. A peak top 2θ of a (3, 1, 1) plane determined by powder X-ray diffractometry using a CoKα ray is 41.3° or more and 41.5° or less. Some Cos contained in the magnetic particles are substituted with at least one selected from the group consisting of Zn, Ge, and a transition metal element other than Fe.

## Claims

### Claim 1

A cobalt ferrite magnetic powder, comprising:
magnetic particles that have a uniaxial crystal magnetic anisotropy and contain cobalt ferrite, wherein
a peak top 2θ of a (3, 1, 1) plane determined by powder X-ray diffractometry using a CoKα ray is 41.3° or more and 41.5° or less, and
some Cos contained in the cobalt ferrite are substituted with at least one selected from the group consisting of Zn, Ge, and a transition metal element other than Fe.

### Claim 2 (depends on 1)

The cobalt ferrite magnetic powder according to claim 1, wherein
a molar ratio (Co/Fe) of Co to Fe is 0.2 or more and less than 0.5.

### Claim 3 (depends on 1)

The cobalt ferrite magnetic powder according to claim 1, wherein
the transition metal element include at least one selected from the group consisting of Mn, Ni, Cu, Ta, and Zr.

### Claim 4 (depends on 1)

The cobalt ferrite magnetic powder according to claim 1, wherein
the transition metal element includes Cu.

### Claim 5 (depends on 1)

The cobalt ferrite magnetic powder according to claim 1, wherein
an average particle size is 25 nm or less.

### Claim 6 (depends on 1)

The cobalt ferrite magnetic powder according to claim 1, wherein
a relative standard deviation of a particle size is 50% or less.

### Claim 7 (depends on 1)

The cobalt ferrite magnetic powder according to claim 1, wherein
a coercive force Hc is 2500 Oe or more.

### Claim 8 (depends on 1)

The cobalt ferrite magnetic powder according to claim 1, wherein
SFD (Switching Field Distribution) is 2.0 or less.

### Claim 9 (depends on 1)

A tape-shaped magnetic recording medium, comprising:
a magnetic layer including the cobalt ferrite magnetic powder according to claim 1.

### Claim 10

A method of producing a cobalt ferrite magnetic powder, comprising:
melting a component for forming glass and a component for forming a cobalt ferrite magnetic powder and then quenching the components to prepare an amorphous body; and
performing heat treatment on the amorphous body to precipitate the cobalt ferrite magnetic powder, wherein
the cobalt ferrite magnetic powder includes magnetic particles containing cobalt ferrite,
some Cos contained in the cobalt ferrite are substituted with at least one selected from the group consisting of Zn, Ge, and a transition metal element other than Fe, and
oxygen partial pressure during the heat treatment is 1.0 kPa or less.

### Claim 11 (depends on 10)

The method of producing a cobalt ferrite magnetic powder according to claim 10, wherein
the component for forming glass contains sodium borate.

### Claim 12 (depends on 11)

The method of producing a cobalt ferrite magnetic powder according to claim 11, wherein
the component for forming glass further contains at least one of an oxide of an alkaline earth metal or a precursor of the oxide.

### Claim 13 (depends on 12)

The method of producing a cobalt ferrite magnetic powder according to claim 12, wherein
the oxide of an alkaline earth metal includes at least one of calcium oxide, strontium oxide, or barium oxide.

### Claim 14 (depends on 12)

The method of producing a cobalt ferrite magnetic powder according to claim 12, wherein
the oxide of an alkaline earth metal includes at least one of strontium oxide or barium oxide.

### Claim 15 (depends on 11)

The method of producing a cobalt ferrite magnetic powder according to claim 11, wherein
a ratio of the sodium borate to a total amount of the component for forming glass and the component for forming a cobalt ferrite magnetic powder is 35 mol % or more and 60 mol % or less.

### Claim 16 (depends on 10)

The method of producing a cobalt ferrite magnetic powder according to claim 10, wherein
the component for forming a cobalt ferrite magnetic powder contains
at least one of cobalt oxide or a precursor of the cobalt oxide,
iron oxide, and
at least one selected from the group consisting of an oxide of a transition metal element other than Co and Fe, a precursor of the oxide of a transition metal element other than Co and Fe, zinc oxide, a precursor of zinc oxide, germanium oxide, and a precursor of germanium oxide.

### Claim 17 (depends on 10)

The method of producing a cobalt ferrite magnetic powder according to claim 10, wherein
the oxygen partial pressure during the heat treatment is 0.9 kPa or less.

### Claim 18 (depends on 10)

The method of producing a cobalt ferrite magnetic powder according to claim 10, wherein
a temperature of the heat treatment is 550° C. or more and 670° C. or less.

### Claim 19 (depends on 16)

The method of producing a cobalt ferrite magnetic powder according to claim 16, wherein
the transition metal element is at least one selected from the group consisting of Mn, Ni, Cu, Ta, and Zr.