# US 2022/0036228 A1 · Increasing grain size of polycrystalline superconducting materials for superconducting circuits

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0036228 A1
- Document ID: US20220036228A1
- Status: Published application
- Kind: A1
- Application number: 16/945,571
- Filed: 2020-07-31
- Published: 2022-02-03
- Earliest claimed: 2020-07-31
- Assignees: International Business Machines Corporation
- Applicants: International Business Machines Corporation
- Inventors: Christian Lavoie; Benjamin Wymore; Markus Brink; Sweet Jean L.
- Web page: https://patentgrep.com/patent/US20220036228A1

## CPC

- G06N 10/00: Quantum computing, i.e. information processing based on quantum-mechanical phenomena
- G06N 10/40: Physical realisations or architectures of quantum processors or components for manipulating qubits, e.g. qubit coupling or qubit control
- H03K 17/92: by the use, as active elements, of superconductive devices
- H03K 19/195: using superconductive devices
- G06N: COMPUTING ARRANGEMENTS BASED ON SPECIFIC COMPUTATIONAL MODELS
- H03K: PULSE TECHNIQUE (measuring pulse characteristics G01R; modulating sinusoidal oscillations with pulses H03C; transmission of digital information H04L; discriminator circuits detecting phase difference between two signals by counting or integrating cycles of oscillation H03D3/04; automatic control, starting, synchronisation or stabilisation of generators of electronic oscillations or pulses where the type of generator is irrelevant or unspecified H03L; coding, decoding or code conversion, in general H03M)

## Abstract

A method of increasing grain size of polycrystalline superconducting materials for superconducting circuits, includes forming an initial superconducting epitaxial layer lattice matched to a substrate formed of a substrate material, the initial superconducting epitaxial layer formed of a compound including the substrate material and a first metal; and forming a second layer of the first metal on the initial superconducting epitaxial layer and heating the layers to increase a thickness of the initial superconducting epitaxial layer formed of the compound.

## Claims

### Claim 1

A quantum circuit including:
a waveguide circuit arranged to provide electromagnetic radiation to a qubit,
wherein at least one of the qubit and the waveguide circuit is formed to have elements including a superconducting epitaxial layer lattice matched to a substrate formed of a substrate material, the superconducting epitaxial layer formed of a compound including the substrate material and a first material.

### Claim 2 (depends on 1)

The quantum circuit of claim 1, wherein the superconducting epitaxial layer is formed of the compound including the substrate material selected from the group consisting of silicon, germanium, sapphire, and diamond, and the first material selected from the group consisting of Co, V, Pt and Nb.

### Claim 3

A method of increasing grain size of polycrystalline superconducting materials for superconducting circuits, comprising:
forming an initial superconducting epitaxial layer lattice matched to a substrate formed of a substrate material, the initial superconducting epitaxial layer formed of a compound including the substrate material and a first metal; and
forming a second layer of the first metal on the initial superconducting epitaxial layer and heating the layers to increase a thickness of the initial superconducting epitaxial layer formed of the compound.

### Claim 4 (depends on 3)

The method of claim 3, wherein the substrate material comprises a semiconductor material.

### Claim 5 (depends on 4)

The method of claim 4, wherein the semiconductor material comprises at least one of silicon, germanium, or combinations of silicon and germanium.

### Claim 6 (depends on 3)

The method of claim 3, wherein the initial superconducting epitaxial layer comprises a silicide or a germanide.

### Claim 7 (depends on 6)

The method of claim 6, wherein the silicide comprises cobalt silicide.

### Claim 8 (depends on 3)

The method of claim 3, wherein the forming the second layer of the first metal comprises depositing the second layer on the initial superconducting epitaxial layer.

### Claim 9 (depends on 8)

The method of claim 8, wherein the heating the layers to increase a thickness of the initial superconducting epitaxial layer is performed after depositing the second layer of the first metal.

### Claim 10 (depends on 8)

The method of claim 8, wherein the heating the layers to increase a thickness of the initial superconducting epitaxial layer is performed while depositing the second layer of the first metal.

### Claim 11 (depends on 3)

The method of claim 3, wherein forming the superconducting layer comprises forming the superconducting layer using physical vapor deposition or chemical vapor deposition.

### Claim 12

A method of increasing grain size of polycrystalline superconducting materials for superconducting circuits, comprising:
forming a diffusion enhancer layer, comprising a first superconducting metal, on a substrate;
depositing a second superconducting material on the diffusion enhancer layer at a deposition temperature in a temperature range including the melting temperature of the diffusion enhancer layer such that diffusion of the second superconducting material is enhanced within the diffusion enhancer layer, and a grain size of the second superconducting material is increased.

### Claim 13 (depends on 12)

The method of claim 12, wherein the deposition temperature of the second superconducting metal is such that a distance between nucleation sites for nucleation of the second superconducting material is increased.

### Claim 14 (depends on 12)

The method of claim 12, wherein the diffusion enhancer layer comprises at least one of Al, In or Sn.

### Claim 15 (depends on 12)

The method of claim 12, wherein the second superconducting material comprises Nb.

### Claim 16 (depends on 12)

The method of claim 12, wherein the diffusion enhancer layer is thinner than the second superconducting material.

### Claim 17 (depends on 12)

The method of claim 12, wherein the temperature range of the deposition of the second superconducting material includes temperatures above or below the melting point of the diffusion enhancer layer.

### Claim 18 (depends on 12)

The method of claim 12, wherein the temperature range of the deposition temperature is between 100° C. and 250° C.

### Claim 19

A method of increasing grain size of polycrystalline superconducting materials for superconducting circuits, comprising:
setting a grain structure of superconducting elements in a quantum circuit using a separation of phase of elements in the superconducting elements which are fully miscible at higher temperatures and not miscible at lower temperatures.

### Claim 20 (depends on 19)

The method of claim 19, wherein a microstructure of phase separated elements is controlled by a rate of cooling.

### Claim 21 (depends on 19)

The method of claim 19, wherein the superconducting elements in the quantum circuit comprise Nb—Zr alloys.

### Claim 22

A method of increasing grain size of polycrystalline superconducting materials for superconducting circuits, comprising:
heating a mixture, the mixture including a first superconducting material and a second material that does not form intermetallic and are not miscible at room temperature, to a first temperature where the first superconducting material and the second material become miscible; and
cooling the mixture to a second temperature where the first superconducting material and the second material are not miscible any longer, wherein the cooling is performed such that two materials phase separate into their respective crystal structures.

### Claim 23 (depends on 22)

The method of claim 22, wherein the mixture comprises a Nb—Zr alloy.

### Claim 24 (depends on 22)

The method of claim 22, further comprising forming a diffusion barrier on a substrate; and forming the mixture on the diffusion barrier.

### Claim 25 (depends on 24)

The method of claim 24, wherein the substrate comprises a material selected from the group consisting of silicon, germanium, sapphire, and diamond.