# US 2022/0035984 A1 · Methods of estimating warpage of interposers and methods of manufacturing semiconductor package by using the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0035984 A1
- Document ID: US20220035984A1
- Status: Published application
- Kind: A1
- Application number: 17/213,538
- Filed: 2021-03-26
- Published: 2022-02-03
- Earliest claimed: 2020-07-30
- Assignees: Samsung Electronics Co., Ltd.
- Applicants: Samsung Electronics Co., Ltd.
- Inventors: Wonji Park; Jeonghoon Ahn; Jihyung Kim; Jaehee Oh; Yunki Choi; Minguk Kang
- Web page: https://patentgrep.com/patent/US20220035984A1

## CPC

- G06F 30/398: Design verification or optimisation, e.g. using design rule check [DRC], layout versus schematics [LVS] or finite element methods [FEM] (optical proximity correction [OPC] design processes G03F1/36)
- G06F 30/392: Floor-planning or layout, e.g. partitioning or placement
- H10P 74/203: {Structural properties, e.g. testing or measuring thicknesses, line widths, warpage, bond strengths or physical defects}
- H10P 74/23: {characterised by multiple measurements, corrections, marking or sorting processes}
- G06F 2111/10: Numerical modelling
- G06F 2113/18: Chip packaging
- G06F 2119/08: Thermal analysis or thermal optimisation
- G06F 2119/18: Manufacturability analysis or optimisation for manufacturability
- H10W 42/121: {protecting against mechanical damage (H10W76/00, H10W74/00 take precedence)}
- G06F: ELECTRIC DIGITAL DATA PROCESSING (computer systems based on specific computational models G06N)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method of estimating warpage of an interposer and a method of manufacturing a semiconductor package by using the same are disclosed. The interposer includes a through electrode passing through a substrate, and a plurality of metal wiring layers and a plurality of insulating layers on the substrate, and the method of estimating warpage of an interposer includes: performing a temperature sweep test by using sample interposers, and measuring warpages according to temperatures; deriving a warpage slope, as a function of temperature, of each of the sample interposers; deriving a warpage model by linearly fitting the warpage slope with respect to an average pattern density of metal wiring layers in each of the sample interposers; and calculating a room temperature warpage reference value of the interposer based on the warpage model.

## Claims

### Claim 1

A method of estimating warpage of an interposer, the interposer comprising a through electrode passing through a substrate, and a plurality of metal wiring layers and a plurality of insulating layers on the substrate, the method comprising:
performing a temperature sweep test at a plurality of temperatures by using sample interposers, and measuring warpages of the sample interposers according to the plurality of temperatures;
deriving a warpage slope, as a function of temperature, of each of the sample interposers;
deriving a warpage model by linearly fitting the warpage slope with respect to an average pattern density of the metal wiring layers in each of the sample interposers; and
calculating a room temperature warpage reference value of the interposer based on the warpage model.

### Claim 2 (depends on 1)

The method of claim 1, wherein the deriving of the warpage model comprises linearly fitting the warpage slope with respect to the average pattern density of the metal wiring layers according to a first equation:
WS=a*PD+b,
wherein WS is the warpage slope, PD is the average pattern density, a is a first constant, and b is a second constant.

### Claim 3 (depends on 2)

The method of claim 2, wherein, in the linearly fitting of the warpage slope, a temperature sweep test is performed on a plurality of the sample interposers having different average pattern densities, and
wherein a quantity of the plurality of the sample interposers is 5 to 50.

### Claim 4 (depends on 3)

The method of claim 3, wherein, in the linearly fitting of the warpage slope, a value of a determination coefficient R2 of the sample interposers is 0.8 or more.

### Claim 5 (depends on 2)

The method of claim 2, wherein the deriving of the warpage model further comprises deriving the average pattern density of the metal wiring layers in each of the sample interposers, and
wherein the deriving of the average pattern density of the metal wiring layers comprises dividing a bottom surface to a top surface of the plurality of insulating layers into m segments in a direction orthogonal to the substrate, calculating densities of the metal wiring layers in the respective segments, and deriving an average value of the densities calculated with respect to the m segments.

### Claim 6 (depends on 5)

The method of claim 5, wherein the average pattern density of the metal wiring layers is approximately 5% to approximately 40%.

### Claim 7 (depends on 2)

The method of claim 2, wherein the calculating of the room temperature warpage reference value comprises:
obtaining a target warpage slope corresponding to an average pattern density of the interposer;
obtaining a warpage profile of the interposer as a function of temperature by using the target warpage slope; and
obtaining the room temperature warpage reference value using the warpage profile.

### Claim 8 (depends on 7)

The method of claim 7, wherein the obtaining of the warpage profile as a function of the temperature is performed according to a second equation: WX=WST*T+c,
wherein WX is the warpage profile, T is the temperature, WST is the target warpage slope, and c denotes a constant that is calculated by using a warpage limit value at a high temperature, and
wherein the warpage limit value at the high temperature is within a range of −200 micrometers to −300 micrometers at a temperature of 100° C. to 130° C.

### Claim 9

A method of manufacturing a semiconductor package comprising an interposer comprising a through electrode passing through a substrate, and a plurality of metal wiring layers and a plurality of insulating layers on the substrate, the method comprising:
deriving a warpage reference value by using sample interposers; and
deriving an expected cumulative warpage of the interposer so that the interposer has an expected warpage that is greater than or equal to the warpage reference value,
wherein the deriving of the warpage reference value comprises:
performing a temperature sweep test at a plurality of temperatures by using the sample interposers with different pattern densities of the metal wiring layers, and measuring warpages according to the plurality of temperatures;
deriving a warpage slope, as a function of temperature, of each of the sample interposers;
deriving a warpage model by linearly fitting the warpage slope with respect to an average pattern density of the metal wiring layers in each of the sample interposers; and
calculating a room temperature warpage reference value of the interposer based on the warpage model.

### Claim 10 (depends on 9)

The method of claim 9, wherein the deriving of the warpage model comprises linearly fitting the warpage slope with respect to the average pattern density of the metal wiring layers according to a first equation:
WS=a*PD+b,
wherein WS is the warpage slope, PD is the average pattern density, a denotes a first constant, and b denotes a second constant.

### Claim 11 (depends on 10)

The method of claim 10, wherein, in the linearly fitting of the warpage slope, the temperature sweep test is performed on a plurality of the sample interposers having different average pattern densities, and
wherein a quantity of the plurality of the sample interposers is 5 to 50.

### Claim 12 (depends on 9)

The method of claim 9, further comprising:
modifying a design of the interposer so as to change a material in at least one of the plurality of insulating layers responsive to a comparison of the expected cumulative warpage to the room temperature warpage reference value; and
fabricating the interposer based on the modified design.

### Claim 13 (depends on 10)

The method of claim 10, wherein the deriving of the warpage model further comprises deriving the average pattern density of the metal wiring layers in each of the sample interposers, and
wherein the deriving of the average pattern density of the metal wiring layers comprises dividing a bottom surface to a top surface of the plurality of insulating layers into m segments in a direction orthogonal to the substrate, calculating densities of the metal wiring layers in the respective segments, and deriving an average value of the densities calculated with respect to the m segments.

### Claim 14 (depends on 13)

The method of claim 13, wherein the average pattern density of the metal wiring layers is approximately 5% to approximately 40%.

### Claim 15 (depends on 10)

The method of claim 10, wherein the calculating of the room temperature warpage reference value comprises:
obtaining a target warpage slope corresponding to an average pattern density of the interposer;
obtaining a warpage profile of the interposer as a function of temperature by using the target warpage slope; and
obtaining the room temperature warpage reference value by using the warpage profile.

### Claim 16 (depends on 15)

The method of claim 15, wherein the obtaining of the warpage profile as a function of the temperature is performed according to a second equation: WX=WST*T+c,
wherein WX is the warpage profile, T is the temperature, WST is the target warpage slope, and c is a constant that is calculated by using a warpage limit value at a high temperature, and
wherein the warpage limit value at the high temperature is within a range of −200 micrometers to −300 micrometers at a temperature of 100° C. to 130° C.

### Claim 17 (depends on 15)

The method of claim 15, wherein the deriving of the expected cumulative warpage of the interposer comprises deriving the expected cumulative warpage by calculating a total sum of warpage variants applied to the interposer in all unit processes to form the plurality of metal wiring layers and the plurality of insulating layers.

### Claim 18 (depends on 17)

The method of claim 17, wherein the deriving of the expected cumulative warpage further comprises:
dividing a process of fabricating the interposer into n unit steps;
measuring an initial warpage of the interposer;
calculating a first step warpage by adding a first warpage variant in a first unit step to the initial warpage;
calculating a second step warpage by adding a second warpage variant in a second unit step to the first step warpage;
calculating a kth step warpage by adding a kth warpage variant in a kth unit step to a (k−1)th step warpage; and
repeating calculating the kth step warpage until k reaches n.

### Claim 19 (depends on 18)

The method of claim 18, wherein the deriving of the expected cumulative warpage further comprises:
comparing the expected cumulative warpage of the interposer with the room temperature warpage reference value;
modifying a design of the interposer so as to change a material in at least one of the plurality of insulating layers responsive to the expected cumulative warpage being less than the room temperature warpage reference value; and
deriving the expected cumulative warpage of the interposer of the modified design.

### Claim 20

A method of manufacturing a semiconductor package comprising an interposer comprising a through electrode passing through a substrate, and a plurality of metal wiring layers and a plurality of insulating layers on the substrate, the method of forming the interposer comprising:
deriving a warpage reference value by using sample interposers;
deriving an expected cumulative warpage of the interposer so that the interposer has the expected cumulative warpage that is greater than or equal to the warpage reference value; and
manufacturing the interposer,
wherein the deriving of the warpage reference value comprises:
performing a temperature sweep test at a plurality of temperatures by using the sample interposers with different pattern densities of the metal wiring layers, and measuring warpages according to the plurality of temperatures;
deriving a warpage slope, as a function of temperature, of each of the sample interposers;
deriving a warpage model by linearly fitting the warpage slope with respect to an average pattern density of the metal wiring layers in each of the sample interposers; and
calculating a room temperature warpage reference value of the interposer based on the warpage model,
wherein the deriving of the warpage model comprises linearly fitting the warpage slope with respect to the average pattern density of the metal wiring layers according to an equation: WS=a*PD+b,
wherein WS is the warpage slope, PD is the average pattern density, a is a first constant, and b is a second constant.