# US 2022/0035247 A1 · Underlayer for photoresist adhesion and dose reduction

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0035247 A1
- Document ID: US20220035247A1
- Status: Published application
- Kind: A1
- Application number: 17/310,635
- Filed: 2021-01-11
- Published: 2022-02-03
- Earliest claimed: 2020-01-15
- Assignees: Lam Research Corporation
- Applicants: Lam Research Corporation
- Inventors: Samantha S.H. Tan; Jun Xue; Mary Anne Manumpil; Jengyi Yu; Da Li
- Web page: https://patentgrep.com/patent/US20220035247A1

## CPC

- G03F 7/094: {Multilayer resist systems, e.g. planarising layers}
- C23C 16/047: {using irradiation by energy or particles}
- C23C 16/22: characterised by the deposition of inorganic material, other than metallic material
- C23C 16/505: using radio frequency discharges
- G03F 1/22: Masks or mask blanks for imaging by radiation of 100nm or shorter wavelength, e.g. X-ray masks, extreme ultraviolet [EUV] masks; Preparation thereof
- G03F 7/0042: {with inorganic or organometallic light-sensitive compounds not otherwise provided for, e.g. inorganic resists (G03F7/075 takes precedence)}
- G03F 7/091: {characterised by antireflection means or light filtering or absorbing means, e.g. anti-halation, contrast enhancement}
- G03F 7/11: having cover layers or intermediate layers, e.g. subbing layers {(G03F7/091 - G03F7/093, B41N3/03 take precedence)}
- G03F 7/167: {from the gas phase, by plasma deposition (G03F7/2035 takes precedence)}
- G03F 7/2004: {characterised by the use of a particular light source, e.g. fluorescent lamps or deep UV light}
- G03F 7/70033: {by plasma extreme ultraviolet [EUV] sources}
- H01J 37/32357: {Generation remote from the workpiece, e.g. down-stream}
- H01J 37/32449: {Gas control, e.g. control of the gas flow}
- H01J 37/32522: {Temperature}
- H01J 37/32651: {Shields, e.g. dark space shields, Faraday shields}
- H10P 14/6336: {in the presence of a plasma [PECVD]}
- H10P 14/6339: {deposition by cyclic CVD, e.g. ALD, ALE or pulsed CVD}
- H10P 14/6902: {composed of carbon, e.g. alpha-C, diamond or hydrogen doped carbon}
- H10P 50/285: {of materials not containing Si, e.g. PZT or Al2O3}
- H10P 72/0421: {for drying etching}
- H10P 72/0474: {comprising at least one lithography chamber}
- H10P 76/2041: {Photolithographic processes}
- H10P 76/405: {characterised by their composition, e.g. multilayer masks}
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

This disclosure relates generally to a patterning structure including an underlayer and an imaging layer, as well as methods and apparatuses thereof. In particular embodiments, the underlayer provides an increase in radiation absorptivity and/or patterning performance of the imaging layer.

## Claims

### Claim at position 1

-8. (canceled)

### Claim 9

A patterning structure, comprising:
a substrate comprising a partially fabricated semiconductor device film stack;
a radiation-sensitive imaging layer disposed over the substrate; and
an underlayer disposed between the substrate and the imaging layer,
wherein the underlayer comprises a vapor deposited film of hydronated carbon doped with oxygen (O), silicon (Si), nitrogen (N), tungsten (W), boron (B), iodine (I), chlorine (Cl), or a combination of two or more of any of these, and
wherein the film has a thickness of no more than about 25 nm or a thickness of about 2 to 20 nm.

### Claim 10 (depends on 9)

The patterning structure of claim 9, wherein the substrate further comprises an optionally doped amorphous carbon hardmask disposed thereon.

### Claim 11 (depends on 9)

The patterning structure of claim 9, wherein the underlayer comprises 0-30 atomic % oxygen (O) and/or about 20-50 atomic % hydrogen (H); and/or wherein a surface of the underlayer comprises hydroxyl groups, carboxyl groups, peroxy groups, sp2 carbons, sp carbons, and/or unsaturated carbon-containing bonds.

### Claim 12

A method of making a patterning structure, comprising:
providing a substrate;
depositing an underlayer on the substrate, wherein the underlayer is configured to increase adhesion between the substrate and the photoresist and/or reduce radiation dose for effective photoresist exposure; and
forming a radiation-sensitive imaging layer on the underlayer, wherein
the substrate is a partially fabricated semiconductor device film stack;
the substrate further comprises or is a hardmask, amorphous carbon film, amorphous hydrogenated carbon film, silicon oxide film, silicon nitride film, silicon oxynitride film, silicon carbide film, silicon boronitride film, amorphous silicon film, polysilicon film, or a combination thereof;
the imaging layer comprises a tin oxide-based photoresist or a tin oxide hydroxide-based photoresist; and
the underlayer comprises a vapor deposited film of hydronated carbon doped with oxygen (O), silicon (Si), nitrogen (N), tungsten (W), boron (B), iodine (I), chlorine (Cl), or a combination of two or more of any of these, wherein the film has a thickness of no more than 25 nm.

### Claim 13

(canceled)

### Claim 14 (depends on 12)

The method of claim 12, wherein the underlayer is vapor deposited on the substrate using a hydrocarbon precursor in the presence or absence of an oxocarbon precursor, thereby providing a carbon-containing film; and optionally wherein the oxocarbon precursor co-reacts with hydrogen (H2) or a hydrocarbon and optionally further co-reacts with a silicon (Si) source dopant.

### Claim 15 (depends on 14)

The method of claim 14, wherein the hydrocarbon precursor comprises an alkane, an alkene, or an alkyne.

### Claim 16 (depends on 14)

The method of claim 14, wherein the underlayer is vapor deposited using the hydrocarbon precursor in the presence of a nitrogen-containing precursor, a tungsten-containing precursor, a boron-containing precursor, and/or an iodine-containing precursor, thereby providing a doped film.

### Claim 17 (depends on 16)

The method of claim 16, wherein the doped film comprises iodine; a combination of iodine and silicon; or a combination of iodine, silicon, and nitrogen.

### Claim 18 (depends on 12)

The method of claim 12, wherein the underlayer is vapor deposited on the substrate by using a silicon (Si)-containing precursor that co-reacts with an oxidizer and wherein the Si-containing precursor optionally further co-reacts with a carbon (C) source dopant.

### Claim 19 (depends on 12)

The method of claim 12, wherein said depositing further comprises applying a bias at a bias power of 0 W to about 1000 W and using a duty cycle of about 5% to 100%.

### Claim 20 (depends on 19)

The method of claim 19, wherein said applying the bias provides the underlayer having an increased density, as compared to an underlayer formed without applying the bias.

### Claim 21 (depends on 12)

The method of claim 12, wherein the underlayer is vapor deposited on the substrate by PECVD as a termination operation of a vapor deposition on the substrate.

### Claim 22 (depends on 12)

The method of claim 12, wherein the underlayer is vapor deposited on the substrate by plasma enhanced chemical vapor deposition (PECVD) or atomic layer deposition (ALD).

### Claim 23 (depends on 12)

The method of claim 12, further comprising, after said depositing, modifying the underlayer to provide a roughened surface and optionally exposing the underlayer or the roughened surface to an oxygen-containing plasma to provide an oxygen-containing surface.

### Claim 24

A method of depositing an underlayer, the method comprising:
providing a substrate in a process chamber; and
depositing by a plasma enhanced chemical vapor deposition (PECVD) process a hydronated carbon film on a surface of the substrate, wherein the hydronated carbon film is a low density film.

### Claim 25 (depends on 24)

The method of claim 24, wherein the PECVD process comprises introducing a carbon-containing precursor selected from methane (CH4), acetylene (C2H2), ethylene (C2H4), propylene (C3H6), propyne (C3H4), allene (C3H4), cyclopropene (C3H4), butane (C4H10), cyclohexane (C6H12), benzene (C6H6), and toluene (C7H8).

### Claim 26 (depends on 25)

The method of claim 25, wherein the PECVD process further comprises introducing a nitrogen-containing precursor, a tungsten-containing precursor, a boron-containing precursor, and/or an iodine-containing precursor, thereby providing a doped film.

### Claim 27 (depends on 24)

The method of claim 24, wherein the PECVD process comprises a transformer coupled plasma (TCP) or an inductively coupled plasma (ICP).

### Claim 28 (depends on 27)

The method of claim 27, wherein a TCP power is about 100-1000 W with no bias.

### Claim 29 (depends on 27)

The method of claim 27, wherein the PECVD process further comprises a pressure of about 10-1000 mTorr and/or a temperature of about 0-100° C.

### Claim 30 (depends on 27)

The method of claim 27, wherein the PECVD process further comprises an applied pulsed bias comprising a power of about 10-1000 W or an applied continuous wave bias comprising a power of about 10-500 W.

### Claim 31 (depends on 30)

The method of claim 30, wherein the applied pulsed bias comprises a duty cycle of about 1-99% and a pulsing frequency of about 10-2000 Hz.

### Claim 32 (depends on 24)

The method of claim 24, further comprising, after said depositing, modifying the hydronated carbon film to provide a roughened surface and optionally exposing the roughened surface to an oxygen-containing plasma to provide an oxygen-containing surface.

### Claim 33

(canceled)

### Claim 34 (depends on 9)

The patterning structure of claim 9, wherein the hydronated carbon doped with iodine is configured to improve generation of secondary electrons upon exposure to radiation.

### Claim 35 (depends on 9)

The patterning structure of claim 9, wherein the underlayer comprises a density of about 0.7 to 2.9 g/cm3; optionally wherein the underlayer further provides increased etch selectivity; and optionally wherein the underlayer further provides decreased line edge and line width roughness and/or decreased dose to size.

### Claim 36 (depends on 9)

The patterning structure of claim 9, wherein the underlayer further comprises beta hydrogen atoms configured to be released upon exposure to radiation and/or oxygen atoms configured to form oxygen bonds to an atom in the imaging layer.

### Claim 37 (depends on 9)

The patterning structure of claim 9, wherein the imaging layer comprises an Extreme Ultraviolet (EUV)-sensitive inorganic photoresist layer, a chemical vapor deposited (CVD) film, a spin-on film, a tin oxide film, or a tin oxide hydroxide film.

### Claim 38 (depends on 9)

The patterning structure of claim 9, wherein the imaging layer comprises a vapor deposited organometallic imaging layer.

### Claim 39 (depends on 38)

The patterning structure of claim 38, wherein the vapor deposited organometallic imaging layer comprises tin.

### Claim 40 (depends on 38)

The patterning structure of claim 38, wherein the vapor deposited organometallic imaging layer comprises organotin.

### Claim 41 (depends on 9)

The patterning structure of claim 9, wherein the imaging layer comprises a spin-on organometallic imaging layer.

### Claim 42 (depends on 41)

The patterning structure of claim 41, wherein the spin-on organometallic imaging layer comprises tin.

### Claim 43 (depends on 41)

The patterning structure of claim 41, wherein the spin-on organometallic imaging layer comprises organotin.

### Claim 44 (depends on 41)

The patterning structure of claim 41, further comprising a hard mask between the substrate and the underlayer.

### Claim 45 (depends on 44)

The patterning structure of claim 44, wherein the hard mask is ashable.

### Claim 46 (depends on 12)

The method of claim 12, wherein the hydronated carbon doped with iodine is configured to improve generation of secondary electrons upon exposure to radiation.

### Claim 47 (depends on 12)

The method of claim 12, wherein the underlayer comprises about 0-30 atomic % oxygen (O) and/or about 20-50 atomic % hydrogen (H); and/or wherein a surface of the underlayer comprises hydroxyl groups, carboxyl groups, peroxy groups, sp2 carbons, sp carbons, and/or unsaturated carbon-containing bonds.

### Claim 48 (depends on 12)

The method of claim 12, wherein the underlayer comprises a density of about 0.7 to 2.9 g/cm3; optionally wherein the underlayer further provides increased etch selectivity; and optionally wherein the underlayer further provides decreased line edge and line width roughness and/or decreased dose to size.

### Claim 49 (depends on 12)

The method of claim 12, wherein the underlayer further comprises beta hydrogen atoms configured to be released upon exposure to radiation and/or oxygen atoms configured to form oxygen bonds to an atom in the imaging layer.

### Claim 50 (depends on 12)

The method of claim 12, wherein said depositing comprises a plasma enhanced chemical vapor deposition (PECVD) process.

### Claim 51 (depends on 12)

The method of claim 12, wherein the imaging layer comprises an Extreme Ultraviolet (EUV)-sensitive inorganic photoresist layer, a chemical vapor deposited (CVD) film, a spin-on film, a tin oxide film, or a tin oxide hydroxide film.

### Claim 52 (depends on 12)

The method of claim 12, wherein said forming comprises vapor depositing an imaging layer on the underlayer or spin-coating an imaging layer on the underlayer.

### Claim 53 (depends on 52)

The method of claim 52, wherein the imaging layer comprises a vapor deposited organometallic imaging layer.

### Claim 54 (depends on 53)

The method of claim 53, wherein the vapor deposited organometallic imaging layer comprises tin.

### Claim 55 (depends on 53)

The method of claim 53, wherein the vapor deposited organometallic imaging layer comprises organotin.

### Claim 56 (depends on 52)

The method of claim 52, wherein the imaging layer comprises a spin-on organometallic imaging layer.

### Claim 57 (depends on 56)

The method of claim 56, wherein the organometallic imaging layer comprises tin.

### Claim 58 (depends on 56)

The method of claim 56, wherein the organometallic imaging layer comprises organotin.

### Claim 59 (depends on 52)

The method of claim 52, further comprising, after said forming:
exposing the organometallic imaging layer to Extreme Ultraviolet (EUV) radiation.

### Claim 60 (depends on 59)

The method of claim 59, further comprising, after said exposing:
developing the organometallic imaging layer using dry development.

### Claim 61 (depends on 59)

The method of claim 59, further comprising, after said exposing:
developing the organometallic imaging layer using wet development.

### Claim 62 (depends on 61)

The method of claim 61, wherein the wet development is performed using an alkaline developer, an ammonium-based ionic liquid, a glycol ether, an organic acid, a ketone, or an alcohol.

### Claim 63 (depends on 61)

The method of claim 61, wherein the wet development is performed using tetramethylammonium hydroxide (TMAH).

### Claim 64 (depends on 61)

The method of claim 61, wherein the wet development is performed using propylene glycol methyl ether (PGME) or propylene glycol methyl ether acetate (PGMEA).

### Claim 65 (depends on 61)

The method of claim 61, wherein the wet development is performed using an organic acid.

### Claim 66 (depends on 61)

The method of claim 61, wherein the wet development is performed using 2-heptanone.

### Claim 67 (depends on 61)

The method of claim 61, wherein the wet development is performed using ethanol.

### Claim 68 (depends on 52)

The method of claim 52, further comprising, after said spin-coating:
performing a post-application bake at a temperature below 200° C.

### Claim 69 (depends on 59)

The method of claim 59, further comprising, after said exposing:
performing a post-exposure bake at a temperature below 200° C.

### Claim 70 (depends on 61)

The method of claim 61, further comprising, after said developing:
performing a post-development bake at a temperature below 200° C.

### Claim 71 (depends on 12)

The method of claim 12, further comprising:
providing a hard mask between the substrate and the underlayer.

### Claim 72 (depends on 71)

The method of claim 71, wherein the hard mask is an ashable hard mask.

### Claim 73 (depends on 24)

The method of claim 24, further comprising, after said depositing:
vapor depositing or spin-coating an organometallic imaging layer on the hydronated carbon film.

### Claim 74 (depends on 73)

The method of claim 73, wherein the organometallic imaging layer comprises tin.

### Claim 75 (depends on 73)

The method of claim 73, wherein the organometallic imaging layer comprises organotin.

### Claim 76 (depends on 73)

The method of claim 73, further comprising, after said spin-coating:
exposing the organometallic imaging layer to Extreme Ultraviolet (EUV) radiation.

### Claim 77 (depends on 76)

The method of claim 76, further comprising, after said exposing:
developing the organometallic imaging layer using dry development.

### Claim 78 (depends on 76)

The method of claim 76, further comprising, after said exposing:
developing the organometallic imaging layer using wet development.

### Claim 79 (depends on 78)

The method of claim 78, wherein the wet development is performed using an alkaline developer, an ammonium-based ionic liquid, a glycol ether, an organic acid, a ketone, or an alcohol.

### Claim 80 (depends on 78)

The method of claim 78, wherein the wet development is performed using tetramethylammonium hydroxide (TMAH).

### Claim 81 (depends on 78)

The method of claim 78, wherein the wet development is performed using propylene glycol methyl ether (PGME) or propylene glycol methyl ether acetate (PGMEA).

### Claim 82 (depends on 78)

The method of claim 78, wherein the wet development is performed using an organic acid.

### Claim 83 (depends on 78)

The method of claim 78, wherein the wet development is performed using 2-heptanone.

### Claim 84 (depends on 78)

The method of claim 78, wherein the wet development is performed using ethanol.

### Claim 85 (depends on 73)

The method of claim 73, further comprising, after said spin-coating:
performing a post-application bake at a temperature below 200° C.

### Claim 86 (depends on 76)

The method of claim 76, further comprising, after said exposing:
performing a post-exposure bake at a temperature below 200° C.

### Claim 87 (depends on 78)

The method of claim 78, further comprising, after said developing:
performing a post-development bake at a temperature below 200° C.

### Claim 88 (depends on 24)

The method of claim 24, further comprising:
providing a hard mask between the substrate and hydronated carbon film.

### Claim 89 (depends on 88)

The method of claim 88, wherein the hard mask is an ashable hard mask.