# US 2022/0034235 A1 · Compressor assembly with nonstick coating and method of manufacturing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0034235 A1
- Document ID: US20220034235A1
- Status: Published application
- Kind: A1
- Application number: 16/943,070
- Filed: 2020-07-30
- Published: 2022-02-03
- Earliest claimed: 2020-07-30
- Assignees: GM Global Technology Operations LLC
- Applicants: GM Global Technology Operations LLC
- Inventors: Jeremy R. Kirklin; Carnell E. Williams; Anil K. Sachdev
- Web page: https://patentgrep.com/patent/US20220034235A1

## CPC

- F01D 25/007: {Preventing corrosion}
- B05D 3/0254: {After-treatment}
- B05D 5/083: {involving the use of fluoropolymers}
- B05D 7/14: to metal, e.g. car bodies (involving a chemical reaction between the metal and the coating C23)
- C22C 21/08: with silicon
- C22C 21/10: with zinc as the next major constituent
- C22C 21/16: with magnesium
- C22F 1/047: of alloys with magnesium as the next major constituent
- C22F 1/053: of alloys with zinc as the next major constituent
- C22F 1/057: of alloys with copper as the next major constituent
- F01D 5/288: {Protective coatings for blades}
- F01D 25/005: {Selecting particular materials}
- F02B 39/00: Component parts, details, or accessories relating to, driven charging or scavenging pumps, not provided for in groups F02B33/00 - F02B37/00
- B05D 1/02: performed by spraying
- B05D 2202/25: based on Al
- B05D 2506/15: Polytetrafluoroethylene [PTFE]
- B05D 2518/12: Ceramic precursors (polysiloxanes, polysilazanes)
- F05D 2220/40: in turbochargers
- F05D 2230/90: Coating; Surface treatment
- F05D 2240/24: for turbines
- F05D 2300/173: Aluminium alloys, e.g. AlCuMgPb
- F05D 2300/20: Oxide or non-oxide ceramics
- F05D 2300/43: Synthetic polymers, e.g. plastics; Rubber
- F05D 2300/432: PTFE [PolyTetraFluorEthylene]
- F01D: NON-POSITIVE DISPLACEMENT MACHINES OR ENGINES, e.g. STEAM TURBINES (machines or engines for liquids F03; non-positive displacement pumps F04D)
- B05D: PROCESSES FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (conveying articles or workpieces through baths of liquid B65G, e.g. B65G49/02)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- F02B: INTERNAL-COMBUSTION PISTON ENGINES; COMBUSTION ENGINES IN GENERAL (gas-turbine plants F02C; hot-gas or combustion-product positive-displacement engine plants F02G)
- F05D: INDEXING SCHEME FOR ASPECTS RELATING TO NON-POSITIVE-DISPLACEMENT MACHINES OR ENGINES, GAS-TURBINES OR JET-PROPULSION PLANTS

## Abstract

A compressor assembly may include a compressor housing and a compressor impeller disposed within the compressor housing. The compressor housing may have an internal aerodynamic surface that defines a circumferentially extending volute, and the compressor impeller may have an external aerodynamic surface that faces toward at least a portion of the internal aerodynamic surface of the compressor housing. A nonstick coating may be formed on the internal aerodynamic surface of the compressor housing or on the external aerodynamic surface of the compressor impeller. The nonstick coating may prevent foreign material introduced into the compressor assembly from collecting on the internal aerodynamic surface of the compressor housing or on the external aerodynamic surface of the compressor impeller.

## Claims

### Claim 1

A compressor assembly configured to pressurize an airflow for delivery to an internal combustion engine having one or more cylinders, the compressor assembly comprising:
a compressor housing having an internal aerodynamic surface that defines a circumferentially extending volute;
a compressor impeller disposed within the compressor housing and having an external aerodynamic surface that faces toward at least a portion of the internal aerodynamic surface of the compressor housing; and
a nonstick coating formed on the internal aerodynamic surface of the compressor housing or on the external aerodynamic surface of the compressor impeller,
wherein the nonstick coating comprises a polymeric material, a ceramic material, or a combination thereof.

### Claim 2 (depends on 1)

The assembly of claim 1 wherein the nonstick coating comprises a fluoropolymer, a polysiloxane, or a combination thereof.

### Claim 3 (depends on 1)

The assembly of claim 1 wherein the nonstick coating comprises polytetrafluoroethylene, polyvinylidene fluoride, a perfluoroalkoxy polymer, fluorinated ethylene-propylene, or polyethylenetetrafluoroethylene.

### Claim 4 (depends on 1)

The assembly of claim 1 wherein the nonstick coating has a thickness in a range of 15 μm to 100 μm.

### Claim 5 (depends on 1)

The assembly of claim 1 wherein at least one of the compressor housing or the compressor impeller are made of an aluminum-based material.

### Claim 6 (depends on 5)

The assembly of claim 5 wherein the aluminum-based material comprises an aluminum alloy that includes at least one alloying element selected from the group consisting of silicon (Si), copper (Cu), chromium (Cr), magnesium (Mg), manganese (Mn), zirconium (Zr), or zinc (Zn).

### Claim 7 (depends on 1)

The assembly of claim 1 wherein the nonstick coating prevents foreign material introduced into the compressor assembly along with the airflow from collecting on the internal aerodynamic surface of the compressor housing or on the external aerodynamic surface of the compressor impeller.

### Claim 8

A method of manufacturing a component of a compressor assembly, the method comprising:
providing an aluminum alloy body having an aerodynamic surface;
applying a precursor coating composition to at least a portion of the aerodynamic surface of the aluminum alloy body; and then
curing precursor coating composition and form a nonstick coating on the aerodynamic surface of the aluminum alloy body,
wherein the nonstick coating comprises a polymeric material, a ceramic material, or a combination thereof.

### Claim 9 (depends on 8)

The method of claim 8 wherein the nonstick coating comprises a fluoropolymer, a polysiloxane, or a combination thereof.

### Claim 10 (depends on 8)

The method of claim 8 wherein the aluminum alloy body is provided in the form of a compressor housing having an internal aerodynamic surface that defines a circumferentially extending volute, and wherein the nonstick coating is formed on at least a portion of the internal aerodynamic surface of the compressor housing.

### Claim 11 (depends on 8)

The method of claim 8 wherein the aluminum alloy body is provided in the form of a compressor impeller having an external aerodynamic surface, and wherein the nonstick coating is formed on at least a portion of the external aerodynamic surface of the compressor impeller.

### Claim 12 (depends on 8)

The method of claim 8 wherein the precursor coating composition is heat-curable, and wherein the precursor coating composition is cured by heating the aluminum alloy body to a temperature and for a duration sufficient to cure the precursor coating composition and form the nonstick coating on the aerodynamic surface of the aluminum alloy body.

### Claim 13 (depends on 12)

The method of claim 12 wherein the aluminum alloy body comprises a heat-treatable aluminum alloy that includes an alloy of aluminum and at least one alloying element.

### Claim 14 (depends on 13)

The method of claim 13 wherein the at least one alloying element is selected from the group consisting of silicon (Si), copper (Cu), chromium (Cr), magnesium (Mg), manganese (Mn), zirconium (Zr), or zinc (Zn).

### Claim 15 (depends on 13)

The method of claim 13 further comprising:
prior to applying the precursor coating composition to at least a portion of the aerodynamic surface of the aluminum alloy body, heating the aluminum alloy body to a first temperature below a solidus temperature of the alloy for a duration sufficient to cause the at least one alloying element to enter into a homogenous solid solution with the aluminum.

### Claim 16 (depends on 15)

The method of claim 15 further comprising:
after the precursor coating composition is applied to the aerodynamic surface of the aluminum alloy body, heating the aluminum alloy body to a second temperature below the first temperature for a duration sufficient to cause the at least one alloying element to precipitate from the solid solution and form a precipitate phase within an aluminum alloy matrix phase in the aluminum alloy body,
wherein, heating the aluminum alloy body to the second temperature cures the precursor coating composition and transforms the precursor coating composition into the nonstick coating.

### Claim 17 (depends on 8)

The method of claim 8 wherein the precursor coating composition is applied to at least a portion of the aerodynamic surface of the aluminum alloy body using a high-volume, low pressure spraying process, an electrostatic spraying process, a thermal evaporation process, or during an anodization process.

### Claim 18 (depends on 8)

The method of claim 8 wherein the precursor coating composition is applied to at least a portion of the aerodynamic surface of the aluminum alloy body in the form of a solid powder or as an aqueous or non-aqueous liquid.

### Claim 19

A method of manufacturing a component of a compressor assembly, the method comprising:
providing an aluminum alloy body having an aerodynamic surface, wherein the aluminum alloy body comprises an alloy of aluminum and at least one alloying element;
heating the aluminum alloy body to a first temperature below a solidus temperature of the alloy for a duration sufficient to cause the at least one alloying element to enter into a homogenous solid solution with the aluminum;
quenching the aluminum alloy body to ambient temperature to hold the at least one alloying element in the form of a supersaturated solid solution with the aluminum, wherein the supersaturated solid solution includes an aluminum matrix phase;
applying a heat-curable precursor coating composition to at least a portion of the aerodynamic surface of the aluminum alloy body; and then
heating the aluminum alloy body to a second temperature below the first temperature for a duration sufficient to cause the at least one alloying element to precipitate from the aluminum alloy matrix phase and form a precipitate phase within the aluminum alloy matrix phase,
wherein, heating the aluminum alloy body to the second temperature cures the heat-curable precursor coating composition and transforms the heat-curable precursor coating composition into a nonstick coating on the aerodynamic surface of the aluminum alloy body.

### Claim 20 (depends on 19)

The method of claim 19 wherein the first temperature comprises a temperature in a range of 450° C. to 575° C., and wherein the second temperature comprises a temperature in a range of 75° C. to 350° C.