# US 2022/0033947 A1 · Aluminum alloy products and a method of preparation

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0033947 A1
- Document ID: US20220033947A1
- Status: Published application
- Kind: A1
- Application number: 17/450,796
- Filed: 2021-10-13
- Published: 2022-02-03
- Earliest claimed: 2014-10-28
- Assignees: Novelis Inc.
- Applicants: Novelis Inc.
- Inventors: Michael Bull; Rajeev G. Kamat
- Web page: https://patentgrep.com/patent/US20220033947A1

## CPC

- C22F 1/043: of alloys with silicon as the next major constituent
- B22D 7/005: {from non-ferrous metals}
- B22D 15/00: Casting using a mould or core of which a part significant to the process is of high thermal conductivity, e.g. chill casting; Moulds or accessories specially adapted therefor
- B22D 21/007: {with low melting point, e.g. Al 659 degrees C, Mg 650 degrees C}
- C22C 21/02: with silicon as the next major constituent
- C22C 21/08: with silicon
- C22C 21/14: with silicon
- C22C 21/16: with magnesium
- C22F 1/047: of alloys with magnesium as the next major constituent
- C22F 1/05: of alloys of the Al-Si-Mg type, i.e. containing silicon and magnesium in approximately equal proportions
- C22F 1/057: of alloys with copper as the next major constituent
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

The present invention relates to aluminum alloy products that can be riveted and possess excellent ductility and toughness properties. The present invention also relates to a method of producing the aluminum alloy products. In particular, these products have application in the automotive industry.

## Claims

### Claim 1

A method of producing a metal sheet, comprising:
casting an aluminum alloy to form an ingot, wherein the aluminum alloy comprises Cu 0.40-0.80 wt. %, Fe 0-0.40 wt. %, Mg 0.40-0.90 wt. %, Mn 0-0.40 wt. %, Si 0.40-0.7 wt. %, Cr 0-0.2 wt. %, Zn 0-0.1 wt. % and Ti 0-0.20 wt. % with trace element impurities 0.10 wt. % maximum, and Al;
homogenizing the ingot;
hot rolling the ingot to produce a hot band; and
cold rolling the hot band to a sheet having a final gauge thickness.

### Claim 2 (depends on 1)

The method of claim 1, further comprising subjecting the sheet to a solution heat treatment temperature from 450° C. to 575° C.

### Claim 3 (depends on 2)

The method of claim 2, wherein the solution heat treatment temperature ranges from 500° C. to 550° C.

### Claim 4 (depends on 2)

The method of claim 2, wherein the sheet is artificially aged to a T6, T8, or T9 temper.

### Claim 5 (depends on 2)

The method of claim 2, further comprising quenching the sheet to a temperature from 25° C. to 50° C. following solution heat treatment.

### Claim 6 (depends on 5)

The method of claim 5, wherein quenching comprises quenching the sheet at a quench rate from 100° C./s to 450° C./s.

### Claim 7 (depends on 1)

The method of claim 1, wherein homogenizing the ingot comprises heating the ingot to a peak metal temperature of from 500° C. to 580° C.

### Claim 8 (depends on 7)

The method of claim 7, wherein the ingot is soaked at the peak metal temperature for up to 15 hours.

### Claim 9 (depends on 7)

The method of claim 7, further comprising cooling the ingot to room temperature after homogenization.

### Claim 10 (depends on 1)

The method of claim 1, wherein hot rolling the ingot comprises hot rolling the ingot to a range from 250° C. to 530° C.

### Claim 11 (depends on 1)

The method of claim 1, wherein the aluminum alloy comprises Cu 0.45-0.75 wt. %, Fe 0.1-0.35 wt. %, Mg 0.45-0.85 wt. %, Mn 0.1-0.35 wt. %, Si 0.45-0.65 wt. %, Cr 0.02-0.18 wt. %, Zn 0-0.1 wt. % and Ti 0.05-0.15 wt. % with trace element impurities 0.10 wt. % maximum, and Al.

### Claim 12 (depends on 1)

The method of claim 1, wherein the aluminum alloy comprises Cu 0.45-0.65 wt. %, Fe 0.1-0.3 wt. %, Mg 0.5-0.8 wt. %, Mn 0.15-0.35 wt. %, Si 0.45-0.65 wt. %, Cr 0.02-0.14 wt. %, Zn 0.0-0.1 wt. % and Ti 0.05-0.12 wt. % with trace element impurities 0.10 wt. % maximum, and Al.

### Claim 13 (depends on 1)

The method of claim 1, wherein the aluminum alloy comprises Cu 0.51-0.59 wt. %, Fe 0.22-0.26 wt. %, Mg 0.66-0.74 wt. %, Mn 0.18-0.22 wt. %, Si 0.57-0.63 wt. %, Cr 0.06-0.1 wt. %, Zn 0.0-0.1 wt. % and Ti 0-0.08 wt. % with trace element impurities 0.10 wt. % maximum, and Al.

### Claim 14 (depends on 1)

The method of claim 1, wherein the aluminum alloy comprises Cu 0.51-0.59 wt. %, Fe 0.22-0.26 wt. %, Mg 0.66-0.74 wt. %, Mn 0.18-0.22 wt. %, Si 0.55-0.6 wt. %, Cr 0.06-0.1 wt. %, Zn 0.0-0.1 wt. % and Ti 0-0.08 wt. % with trace element impurities 0.10 wt. % maximum, and Al.

### Claim 15 (depends on 1)

The method of claim 1, wherein the aluminum alloy has a strength of at least 250 MPa.

### Claim 16 (depends on 1)

The method of claim 1, wherein the aluminum alloy has a sufficient ductility or toughness to meet an r/t bendability of 0.8 or less.

### Claim 17 (depends on 1)

The method of claim 1, wherein the aluminum alloy has a sufficient ductility or toughness to meet an r/t bendability of 0.4 or less and having a strength of least 290 MPa.

### Claim 18 (depends on 1)

The method of claim 1, wherein casting comprises direct chill casting.

### Claim 19 (depends on 1)

An aluminum sheet made according to the method of claim 1.

### Claim 20 (depends on 19)

The aluminum sheet of claim 19, wherein the aluminum alloy sheet is used to produce an automotive part or a transportation part.