# US 2022/0033939 A1 · Ferritic stainless steel and ferritic stainless steel pipe with improved mechanical properties of welding portion

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0033939 A1
- Document ID: US20220033939A1
- Status: Published application
- Kind: A1
- Application number: 17/276,953
- Filed: 2019-08-23
- Published: 2022-02-03
- Earliest claimed: 2018-09-27
- Assignees: Posco
- Applicants: Posco
- Inventors: Kye-Man Lee; Jae-Seok Park
- Web page: https://patentgrep.com/patent/US20220033939A1

## CPC

- C22C 38/28: with titanium or zirconium
- C21D 8/02: during manufacturing of plates or strips (C21D8/12 takes precedence)
- C21D 8/0226: {Hot rolling}
- C21D 8/10: during manufacturing of tubular bodies
- C21D 9/46: for sheet metals
- C22C 38/00: Ferrous alloys, e.g. steel alloys (cast-iron alloys C22C37/00)
- C22C 38/001: {containing N}
- C22C 38/004: {Very low carbon steels, i.e. having a carbon content of less than 0,01%}
- C22C 38/06: containing aluminium
- C22C 38/20: with copper
- C22C 38/22: with molybdenum or tungsten
- C22C 38/26: with niobium or tantalum
- C22C 38/32: with boron
- C22C 38/40: with nickel
- C22C 38/42: with copper
- C22C 38/48: with niobium or tantalum
- C22C 38/50: with titanium or zirconium
- C22C 38/54: with boron
- C21D 2211/005: Ferrite
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)

## Abstract

A ferritic stainless steel with improved mechanical properties of weld zone is disclosed. The ferritic stainless steel includes, in percent (%) by weight of the entire composition, C: 0.005 to 0.02%, N: 0.005 to 0.02%, Cr: 11.0 to 13.0%, Ti: 0.16 to 0.3%, Nb: 0.1 to 0.3%, Al: 0.005 to 0.05%, the remainder of iron (Fe) and other inevitable impurities, and the ferritic stainless steel has a texture maximum strength of 30 or less in the {001} direction after welding.

## Claims

### Claim 1

A ferritic stainless steel with improved mechanical properties of weld zone, the ferritic stainless steel comprising, in percent (%) by weight of the entire composition, C: 0.005 to 0.02%, N: 0.005 to 0.02%, Cr: 11.0 to 13.0%, Ti: 0.16 to 0.3%, Nb: 0.1 to 0.3%, Al: 0.005 to 0.05%, the remainder of iron (Fe) and other inevitable impurities, and
the ferritic stainless steel has a texture maximum strength of 30 or less in the {001} direction after welding.

### Claim 2 (depends on 1)

The ferritic stainless steel according to claim 1, wherein the ferritic stainless steel comprises a secondary phase present in the weld zone of 10 to 100 pieces/mm2 after welding.

### Claim 3 (depends on 2)

The ferritic stainless steel according to claim 2, wherein the secondary phase comprises nitride, oxide and Laves phase precipitates.

### Claim 4 (depends on 1)

The ferritic stainless steel according to claim 1, further comprising: at least one of Mo: 1.0% or less, Ni: 1.0% or less, Cu: 1.0% or less, and B: 0.005% or less.

### Claim 5

A ferritic stainless steel pipe comprising:
a base material comprising, in percent (%) by weight of the entire composition, C: 0.005 to 0.02%, N: 0.005 to 0.02%, Cr: 11.0 to 13.0%, Ti: 0.16 to 0.3%, Nb: 0.1 to 0.3%, Al: 0.005 to 0.05%, the remainder of iron (Fe) and other inevitable impurities, and
a weld zone having a texture maximum strength of 30 or less in the {001} direction.

### Claim 6 (depends on 5)

The ferritic stainless steel pipe according to claim 5, wherein the weld zone comprises a secondary phase of 10 to 100/mm2.

### Claim 7 (depends on 6)

The ferritic stainless steel pipe according to claim 6, wherein the secondary phase comprises nitride, oxide and Laves phase precipitates.

### Claim 8 (depends on 5)

The ferritic stainless steel pipe according to claim 5, wherein the base material further comprises at least one of Mo: 1.0% or less, Ni: 1.0% or less, Cu: 1.0% or less, and B: 0.005% or less.

### Claim 9 (depends on 5)

The ferritic stainless steel pipe according to claim 5, wherein a ductile to brittle transition temperature (DBTT) of the weld zone is −50° C. or less.