# US 2022/0033926 A1 · High-strength cold rolled steel sheet having high hole expansion ratio, highstrength hot-dip galvanized steel sheet, and manufacturing methods therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0033926 A1
- Document ID: US20220033926A1
- Status: Published application
- Kind: A1
- Application number: 17/280,524
- Filed: 2019-09-27
- Published: 2022-02-03
- Earliest claimed: 2018-09-28
- Assignees: Posco
- Applicants: Posco
- Inventors: Young-Roc IM; Jong-Chan PARK; Jai-Hyun KWAK; Min-Seo KOO
- Web page: https://patentgrep.com/patent/US20220033926A1

## CPC

- C21D 9/46: for sheet metals
- B32B 15/013: {one layer being formed of an iron alloy or steel, another layer being formed of a metal other than iron or aluminium}
- C21D 1/19: by interrupted quenching
- C21D 1/25: Hardening, combined with annealing between 300 degrees Celsius and 600 degrees Celsius, i.e. heat refining ("Vergüten")
- C21D 6/002: {containing Cr (C21D6/004 takes precedence)}
- C21D 6/004: {containing Cr and Ni}
- C21D 6/005: {containing Mn}
- C21D 6/008: {containing Si}
- C21D 8/02: during manufacturing of plates or strips (C21D8/12 takes precedence)
- C21D 8/0226: {Hot rolling}
- C21D 8/0236: {Cold rolling}
- C21D 8/0247: characterised by the heat treatment
- C21D 8/0263: {following hot rolling}
- C21D 8/0426: {Hot rolling}
- C21D 8/0442: {Flattening; Dressing; Flexing}
- C21D 8/0463: {following hot rolling}
- C21D 9/48: deep-drawing sheets
- C22C 38/00: Ferrous alloys, e.g. steel alloys (cast-iron alloys C22C37/00)
- C22C 38/001: {containing N}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/02: containing silicon
- C22C 38/06: containing aluminium
- C22C 38/20: with copper
- C22C 38/22: with molybdenum or tungsten
- C22C 38/24: with vanadium
- C22C 38/26: with niobium or tantalum
- C22C 38/28: with titanium or zirconium
- C22C 38/32: with boron
- C22C 38/38: with more than 1.5% by weight of manganese
- C22C 38/40: with nickel
- C22C 38/42: with copper
- C22C 38/44: with molybdenum or tungsten
- C22C 38/46: with vanadium
- C22C 38/48: with niobium or tantalum
- C22C 38/50: with titanium or zirconium
- C22C 38/54: with boron
- C22C 38/58: with more than 1.5% by weight of manganese
- C23C 2/02: Pretreatment of the material to be coated, e.g. for coating on selected surface areas (C23C2/30 takes precedence)
- C23C 2/0224: {Two or more thermal pretreatments}
- C23C 2/06: Zinc or cadmium or alloys based thereon
- C23C 2/28: Thermal after-treatment, e.g. treatment in oil bath
- C23C 2/29: {Cooling or quenching}
- C23C 2/40: Plates; Strips
- C21D 2211/001: Austenite
- C21D 2211/002: Bainite
- C21D 2211/003: Cementite
- C21D 2211/005: Ferrite
- C21D 2211/008: Martensite
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

Provided is a high-strength cold rolled steel sheet, a high-strength hot-dip galvanized steel sheet manufactured using the cold rolled steel sheet, and manufacturing methods therefor, the high-strength cold rolled steel sheet comprising, by wt %, 0.17-0.21% of carbon (C), 0.3-0.8% of silicon (Si), 2.7-3.3% of manganese (Mn), 0.3-0.7% of chromium (Cr), 0.01-0.3% of aluminum (Al), 0.01-0.03% of titanium (Ti), 0.001-0.003% of boron (B), 0.04% or less of phosphorus (P), 0.02% or less of sulfur (S), 0.01% or less of nitrogen (N) and the balance of iron (Fe) and other inevitable impurities, wherein the amounts of carbon (C), silicon (Si) and aluminum (Al) satisfy the following mathematical relation (1). [Mathematical relation (1)] [C]+([Si]+[Al])/5≤0.35% (wherein [C], [Si] and [Al] respectively mean the wt % of C, Si and Al.)

## Claims

### Claim 1

A high-strength cold rolled steel sheet comprising:
by weight percent (wt %), 0.17 to 0.21% of carbon (C), 0.3 to 0.8% of silicon (Si), 2.7 to 3.3% of manganese (Mn), 0.3 to 0.7% of chromium (Cr, 0.01 to 0.3% of aluminum (Al), 0.01 to 0.03% of titanium (Ti), 0.001 to 0.003% of boron (B), 0.04% or less of phosphorus (P), 0.02% or less of sulfur (S), 0.01% or less of nitrogen (N), the balance of iron (Fe), and other inevitable impurities, wherein the contents of carbon (C), silicon (Si), and aluminum (Al) satisfy Equation 1 below, a microstructure thereof includes, by area fraction, 3 to 7% of retained austenite, 5 to 15% of fresh martensite, 5% or less (including 0%) of ferrite, and the balance of bainite or tempered martensite, and, by volume fraction, 1 to 3% of a cementite phase, as a second phase, is precipitated and distributed between bainite laths or in the laths or grain boundary of a tempered martensite phase,
[C]+([Si]+[Al])/5≤0.35% [Equation (1)]
wherein [C], [Si], [Al] refer to weight percents of C, Si, and Al, respectively.

### Claim 2 (depends on 1)

The high-strength cold rolled steel sheet of claim 1, wherein the cold rolled steel sheet further includes 0.1% or less of copper (Cu), 0.1% or less of nickel (Ni), and 0.1% or less of molybdenum (Mo).

### Claim 3 (depends on 1)

The high-strength cold rolled steel sheet of claim 1, wherein the cold rolled steel sheet further includes 0.03% or less of niobium (Nb) and 0.01% of less of vanadium (V).

### Claim 4 (depends on 1)

The high-strength cold rolled steel sheet of claim 1, wherein the cold rolled steel sheet has a tensile strength of 1180 MPa or more, a yield ratio of 0.65 to 0.85, a hole expansion ratio of 25% or more (HER), and an elongation of 5 to 13%.

### Claim 5 (depends on 1)

A high strength hot-dip galvanized steel sheet comprising a hot-dip zinc plating layer on a surface of the high-strength cold rolled steel sheet of claim 1.

### Claim 6

(canceled)

### Claim 7

A method of manufacturing a high-strength cold rolled steel sheet, the method comprising:
preparing a slab including, by weight percent (wt %), 0.17 to 0.21% of carbon (C), 0.3 to 0.8% of silicon (Si), 2.7 to 3.3% of manganese (Mn), 0.3 to 0.7% of chromium (Cr, 0.01 to 0.3% of aluminum (Al), 0.01 to 0.03% of titanium (Ti), 0.001 to 0.003% of boron (B), 0.04% or less of phosphorus (P), 0.02% or less of sulfur (S), 0.01% or less of nitrogen (N), the balance of iron (Fe), and other inevitable impurities, wherein the contents of carbon (C), silicon (Si), and aluminum (Al) satisfy Equation 1 below;
heating the slab to a temperature in a range of 1,150° C. to 1,250° C.;
finish hot rolling the heated slab within a finish delivery temperature (FDT) range of 900° C. to 980° C.;
cooling the slab at an average cooling rate of 10° C./sec to 100° C./sec after the finish hot rolling;
winding the slab in a temperature in a range of 500° C. to 700° C.;
cold rolling the slab at a cold-rolling reduction ratio of 30% to 60% to obtain a cold rolled steel sheet;
continuously annealing the cold rolled steel sheet at a temperature in a range of (Ae3+30° C. to Ae3+80° C.);
primarily cooling the continuously annealed steel sheet at an average cooling rate of 10° C./s or less to a temperature in a range of 560° C. to 700° C. and secondarily cooling the steel sheet at an average cooling rate of 10° C./s or more to a temperature in a range of 270° C. to 330° C.; and
reheating the cooled steel sheet at a temperature increase rate of 5° C./s or lower to a temperature in a range of 380° C. to 460° C.,
[C]+([Si]+[Al])/5≤0.35% [Equation (1)]
wherein [C], [Si], and [Al] refer to weight percent of C, Si, and Al, respectively.

### Claim 8 (depends on 7)

The method of claim 7, wherein the slab further includes 0.1% or less of copper (Cu), 0.1% or less of nickel (Ni), and 0.1% or less of molybdenum (Mo).

### Claim 9 (depends on 7)

The method of claim 7, wherein the slab further includes 0.03% or less of niobium (Nb) and 0.01% or less of vanadium (V).

### Claim 10 (depends on 7)

The method of claim 7, wherein the continuous annealing is performed at a temperature in a range of 830° C. to 880° C.

### Claim at position 11

-13. (canceled)