# US 2022/0033920 A1 · Wire rod of which softening heat treatment can be omitted, and manufacturing method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0033920 A1
- Document ID: US20220033920A1
- Status: Published application
- Kind: A1
- Application number: 17/414,063
- Filed: 2019-12-13
- Published: 2022-02-03
- Earliest claimed: 2018-12-18
- Assignees: Posco
- Applicants: Posco
- Inventors: Jae-Seung LEE; Byoung-Gab LEE; Sang-Yoon LEE; Se-Hong MIN; Woo-Seok CHOI
- Web page: https://patentgrep.com/patent/US20220033920A1

## CPC

- C21D 8/06: during manufacturing of rods or wires
- B21B 1/16: for rolling {wire rods, bars, merchant bars, rounds} wire or material of like small cross-section
- C21D 1/32: Soft annealing, e.g. spheroidising
- C21D 9/52: for wires; for strips {; for rods of unlimited length}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/22: with molybdenum or tungsten
- C21D 2211/001: Austenite
- C21D 2211/002: Bainite
- C21D 2211/005: Ferrite
- C21D 2211/008: Martensite
- C21D 2211/009: Pearlite
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- B21B: ROLLING OF METAL (auxiliary operations used in connection with metal-working operations covered in B21, see B21C; bending by rolling B21D; manufacture of particular objects, e.g. screws, wheels, rings, barrels, balls, by rolling B21H; pressure welding by means of a rolling mill B23K20/04)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

The present invention relates to a wire rod of which softening heat treatment can be omitted, and a manufacturing method therefor. One embodiment of the present invention provides a wire rod of which softening heat treatment can be omitted, and a manufacturing method therefor, the wire rod comprising, by wt %, 0.2-0.45% of C, 0.02-0.4% of Si, 0.3-1.5% of Mn, 0.3-1.5% of Cr, 0.02-0.05% of Al, 0.01-0.5% of Mo, 0.01% or less of N, and the balance of Fe and other inevitable impurities, and having a microstructure consisting of, by area %, 40% or more of proeutectoid ferrite based on an equilibrium phase, 40% or more of regenerated pearlite and bainite, and 20% or less of martensite, and wherein the colony average size of the pearlite in the region amounting to ⅖ to ⅗ of the diameter is 5 μm or less.

## Claims

### Claim 1

A wire rod allowing a softening heat treatment to be omitted, the wire rod comprising, by weight %, 0.2 to 0.45% of carbon (C), 0.02 to 0.4% of silicon (Si), 0.3 to 1.5% of manganese (Mn), 0.3 to 1.5% of chromium (Cr), 0.02 to 0.05% of aluminum (Al), 0.01 to 0.5% of molybdenum (Mo), 0.01% or less of nitrogen (N), and a balance of iron (Fe) and inevitable impurities,
wherein the wire rod has a microstructure consisting of, by area %, 40% or more of proeutectoid ferrite based on an equilibrium phase, 40% or more of regenerated pearlite and bainite, and 20% or less of martensite, and
wherein an average colony size of the pearlite in a region from a ⅖ point to a ⅗ point of a diameter, from a surface of the wire rod, is 5 μm or less.

### Claim 2 (depends on 1)

The wire rod of claim 1, wherein an average grain size of the proeutectoid ferrite in the region of the ⅖ point to ⅗ point of the diameter, from the surface of the wire rod, is 7 μm or less.

### Claim 3 (depends on 1)

The wire rod of claim 1, wherein an average major-axis size of cementite in the pearlite colony is 5 μm or less.

### Claim 4 (depends on 1)

The wire rod of claim 1, wherein a deviation between an average grain size of the proeutectoid ferrite in a region from a surface of the wire rod to a ⅕ point of the diameter and an average grain size of the proeutectoid ferrite in the region from the ⅖ point to the ⅗ point of the diameter is 6 μm or less.

### Claim 5 (depends on 1)

The wire rod of claim 1, wherein tensile strength is 579+864×([C]+[Si]/8+[Mn]/18) MPa or more.

### Claim 6 (depends on 1)

The wire rod of claim 1, wherein an average aspect ratio of cementite after a spheroidizing annealing heat treatment performed once is 2.5 or less.

### Claim 7 (depends on 1)

The wire rod of claim 1, wherein tensile strength after a spheroidization heat treatment performed once is 540 MPa or less.

### Claim 8

A method of manufacturing a wire rod allowing a softening heat treatment to be omitted, the method comprising:
heating a billet at a temperature within a range of 950 to 1050° C., the billet comprising, by weight %, 0.2 to 0.45% of carbon (C), 0.02 to 0.4% of silicon (Si), 0.3 to 1.5% of manganese (Mn), 0.3 to 1.5% of chromium (Cr), 0.02 to 0.05% of aluminum (Al), 0.01 to 0.5% of molybdenum (Mo), 0.01% or less of nitrogen (N), and a balance of iron (Fe) and inevitable impurities;
performing two step hot rolling on the heated billet to obtain a rod wire;
coiling the rod wire; and
cooling the coiled rod wire to 600° C. at a cooling rate of 2° C./sec, and then cooling the cooled rod wire at a cooling rate of 3° C./sec,
wherein the performing of the two step hot rolling comprises:
performing intermediate finish rolling on the heated billet; and
performing finish rolling at a temperature of 730° C. to Ae3 with a critical deformation amount or more expressed by the following Relational Expression 1.
Critical Deformation Amount=−2.46Ceq2+3.11Ceq−0.39 [Relational Expression 1]
(Ceq=C+Mn/6+Cr/5, and C, Mn, and Cr are weight %)

### Claim 9 (depends on 8)

The method of claim 8, wherein a heating time during the heating is 90 minutes or less.

### Claim 10 (depends on 8)

The method of claim 8, wherein after the intermediate finish rolling, an average grain size of austenite of the rod wire is 5 to 20 μm.

### Claim 11 (depends on 8)

The method of claim 8, wherein an average surface temperature Tpf of the rod wire before the finish rolling and an average surface temperature Tf of the rod wire after the finish finishing rolling satisfy the following Relational Expression 1.
Tpf−Tf≤50° C. [Relational Expression 1]

### Claim 12 (depends on 8)

The method of claim 8, wherein an average surface temperature Tf of the rod wire after the finish rolling and a coiling temperature T1 of the rod wire satisfy the following Relational Expression 2.
Tf−Tl≤30° C. [Relational Expression 2]

### Claim 13 (depends on 8)

The method of claim 8, after the cooling at a cooling rate of 3° C./sec, further comprising:
performing a spheroidizing heat treatment in which the wire rod is heated to Ae1 to Ae1+40° C. and maintained for 10 to 15 hours, and then cooled to 660° C. at 20° C./hr or less.