# US 2022/0033630 A1 · Polyolefin resin blends for high stress cracking resistance and good processability

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0033630 A1
- Document ID: US20220033630A1
- Status: Published application
- Kind: A1
- Application number: 17/278,840
- Filed: 2019-09-16
- Published: 2022-02-03
- Earliest claimed: 2018-09-24
- Assignees: Thai Polyethylene Co., Ltd.; SCG Chemicals Co., Ltd.
- Applicants: Thai Polyethylene Co., Ltd.; SCG Chemicals Co., Ltd.
- Inventors: Saranya TRAISILANUN; Wiroj NANTASETPHONG; Watcharee CHEEVASRIRUNGRUANG
- Web page: https://patentgrep.com/patent/US20220033630A1

## CPC

- C08L 23/06: Polyethylene
- C08L 23/0815: {with aliphatic 1-olefins containing one carbon-to-carbon double bond}
- C08L 2203/16: used for films
- C08L 2203/18: used for pipes
- C08L 2203/202: use in electrical wires or wirecoating
- C08L 2205/025: containing two or more polymers of the same hierarchy C08L, and differing only in parameters such as density, comonomer content, molecular weight, structure
- C08L 2205/03: containing three or more polymers in a blend
- C08L 2205/035: containing four or more polymers in a blend
- C08L 2314/02: Ziegler natta catalyst
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

Polyethylene composition comprising a melt blend, the melt blend comprising: a) a first multimodal polyethylene, the first multimodal polyethylene having a medium weight average molecular weight of a high weight average molecular weight, a density of more than 0.950 to 0.965 g/cm3 according to ISO 1183 and a MFR2 of 0.3 to 2.0 g/10 min according to ISO 1133; and b) a second multimodal polyethylene, the second multimodal polyethylene having a high weight average molecular weight, a density of 0.940 to 0.950 g/cm3 according to ISO 1183 and a MFR2 of 0.03 to 0.15 g/10 min according to ISO 1133; wherein the polymer composition has a Full Notch Creep Test (FNCT) according to ISO 16770 of at least 58 hours and a Charpy impact strength at a temperature of 23° C. of at least 4 kJ/m2 according to ISO 179.

## Claims

### Claim 1

A polyethylene composition comprising a melt blend, the melt blend comprising:
a) a first multimodal polyethylene, the first multimodal polyethylene having a medium weight average molecular weight from 90,000 to 200,000 g/mol or a high weight average molecular weight from 200,000 to 1,000,000 g/mol, a density of more than 0.950 to 0.965 g/cm3 according to ISO 1183 and a MFR2 of 0.3 to 2.0 g/10 min according to ISO 1133; and
b) a second multimodal polyethylene, the second multimodal polyethylene having a high weight average molecular weight from 200,000 to 1,000,000 g/mol, a density of 0.940 to 0.950 g/cm3 according to ISO 1183 and a MFR2 of 0.03 to 0.15 g/10 min according to ISO 1133;
wherein the polymer composition has a Full Notch Creep Test (FNCT) according to ISO 16770 of at least 58 hours and a Charpy impact strength at a temperature of 23° C. of at least 4 kJ/m2 according to ISO 179.

### Claim 2 (depends on 1)

The polyethylene composition according to claim 1, wherein the polymer composition has a FNCT from 58 to 100 hours.

### Claim 3 (depends on 1)

The polyethylene composition according to claim 1, wherein the polyethylene composition has a Charpy impact strength at a temperature of 23° C. from 4 to 10 kJ/m2.

### Claim 4 (depends on 1)

The polyethylene composition according to claim 1, wherein the first multimodal polyethylene is a bimodal polyethylene or a trimodal polyethylene and the second multimodal polyethylene is a bimodal polyethylene or a trimodal polyethylene.

### Claim 5 (depends on 4)

The polyethylene composition according to claim 4, wherein the bimodal polyethylene comprises 40 to 60% by weight of an ethylene homopolymer and 40 to 60% by weight of an ethylene copolymer, based on the total weight of the bimodal polyethylene respectively, wherein the ethylene copolymer comprises a co-monomer in an amount of at least 0.30 mol % with respect to the total amount of monomer in the ethylene copolymer.

### Claim 6 (depends on 5)

The polyethylene composition according to claim 5, wherein the co-monomer is selected from the group consisting of 1-butene, 1-hexene, 1-octene, and mixtures thereof.

### Claim 7 (depends on 4)

The polyethylene composition according to claim 4, wherein the bimodal polyethylene has a MFR2 of 0.02 to 1.0 g/10 min according to ISO 1133 and/or a density of 0.945 to 0.960 g/cm3, according to ISO 1138.

### Claim 8 (depends on 4)

The polyethylene composition according to claim 4, wherein the bimodal polyethylene has a weight average molecular weight of 100,000 to 400,000 g/mol, measured by gel permeation chromatography.

### Claim 9 (depends on 4)

The polyethylene composition according to claim 4, wherein the trimodal polyethylene comprises:
(A) 30 to 65% by weight, based on the total weight of the trimodal polyethylene, of a low molecular weight polyethylene, wherein the low molecular weight polyethylene has a MFR2 of 500 to 1,000 g/10 min according to ISO 1133 and a weight average molecular weight (Mw) of 20,000 to 90,000 g/mol, measured by gel permeation chromatography;
(B) 5 to 40% by weight, based on the total weight of the trimodal polyethylene, of an ultrahigh molecular weight polyethylene having a weight average molecular weight from 1,000,000 to 5,000,000 g/mol; and
(C) 20 to 60% by weight, based on the total weight of the trimodal polyethylene, of a high molecular weight polyethylene having a weight average molecular weight from 200,000 to 1,000,000 g/mol.

### Claim 10 (depends on 4)

The polyethylene composition according to claim 4, wherein the trimodal polyethylene has a weight average molecular weight from 80,000 to 500,000 g/mol, measured by gel permeation chromatography.

### Claim 11 (depends on 1)

The polyethylene composition according to claim 1, wherein the melt blend comprises 70 to 97% by weight of the first multimodal polyethylene; and 3 to 30% by weight of the second multimodal polyethylene, based on the total weight of the melt blend respectively.

### Claim 12 (depends on 1)

The polyethylene composition according to claim 1, wherein the polyethylene composition has a MFR2 of 0.05 to 2.0 g/10 min, according to ISO 1133.

### Claim 13 (depends on 1)

The polyethylene composition according to claim 1, wherein the polyethylene composition has a density from 0.945 to 0.960 g/cm3, according to ISO 1183.

### Claim 14 (depends on 1)

The polyethylene composition according to claim 1, wherein the polyethylene composition has a weight average molecular weight of 80,000 to 500,000 g/mol, measured by gel permeation chromatography; and/or a polydispersity index from 10 to 25.

### Claim 15 (depends on 1)

An article comprising the polyethylene composition according to claim 1.

### Claim 16 (depends on 2)

The polyethylene composition of claim 2, wherein the FNCT is from 58 to 100 hours.

### Claim 17 (depends on 4)

The polyethylene composition of claim 4, wherein one of the first multimodal polyethylene and the second multimodal polyethylene is a bimodal polyethylene and the other one of the first multimodal polyethylene and the second multimodal polyethylene is a trimodal polyethylene.

### Claim 18 (depends on 17)

The polyethylene composition of claim 17, wherein the first multimodal polyethylene is a bimodal polyethylene and the second multimodal polyethylene is trimodal polyethylene.

### Claim 19 (depends on 6)

The polyethylene composition of claim 6, wherein the co-monomer is 1-butene.

### Claim 20 (depends on 15)

The article of claim 15, wherein the article is a molding, a pipe, a film, a cap, a closure, a wire, a cable, or a sheet.