# US 2022/0033577 A1 · Method for preparing biogenic guanidine complex, method for preparing polyethylene terephthalate (pet), and method for preparing poly (ethylene isophthalate-co-terephthalate) (peit)

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0033577 A1
- Document ID: US20220033577A1
- Status: Published application
- Kind: A1
- Application number: 17/033,787
- Filed: 2020-09-26
- Published: 2022-02-03
- Earliest claimed: 2020-08-02
- Assignees: Polytex Chemical Engineering Co., Ltd.
- Applicants: Polytex Chemical Engineering Co., Ltd.
- Inventors: Hong Li; Dubin Wang
- Web page: https://patentgrep.com/patent/US20220033577A1

## CPC

- C07F 3/003: {without C-Metal linkages}
- C08G 63/81: using solvents (C08G63/79 takes precedence)
- C07F 15/025: {without a metal-carbon linkage}
- C08G 63/183: Terephthalic acids
- C08G 63/785: {characterised by the apparatus used}
- C08G 63/826: {Metals not provided for in groups C08G63/83 - C08G63/86 (C08G63/823 takes precedence)}
- C08G 63/83: Alkali metals, alkaline earth metals, beryllium, magnesium, copper, silver, gold, zinc, cadmium, mercury, manganese, or compounds thereof {(C08G63/823 takes precedence)}
- C08G 63/90: Purification; Drying
- C08L 67/03: the dicarboxylic acids and dihydroxy compounds having the carboxyl- and the hydroxy groups directly linked to aromatic rings
- C08J 2367/03: the dicarboxylic acids and dihydroxy compounds having the hydroxy and the carboxyl groups directly linked to aromatic rings
- C07F: ACYCLIC, CARBOCYCLIC OR HETEROCYCLIC COMPOUNDS CONTAINING ELEMENTS OTHER THAN CARBON, HYDROGEN, HALOGEN, OXYGEN, NITROGEN, SULFUR, SELENIUM OR TELLURIUM (metal-containing porphyrins C07D487/22)
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)

## Abstract

A method for preparing a biogenic guanidine complex, the method including: mixing dimethyl sulfoxide (DMSO) with water in a volume ratio thereof of 1:1 to yield a solvent DMSO-H2O; adding organic guanidine (G) and a compound MX2 in a molar ratio G/MX2=1:1 or 2:1 to the solvent DMSO-H2O, where the organic guanidine (G) is selected from arginine (Arg), guanidinoacetic acid (Gaa), creatine (Cra), creatinine (Cran), guanine (Gua), and agmatine (Agm); M represents Fe2+, Mg2+, or Zn2+; and X represents Cl−, CH3COO−, or CH3CH(OH)COO−; stirring the solvent DMSO-H2O containing the organic guanidine and the compound MX2; recycling the solvent DMSO-H2O through vacuum distillation and obtaining a solid; transferring the solid to a Buchner funnel, and washing the solid with deionized water and ethanol consecutively; and removing the deionized water and ethanol through vacuum filtration, and drying the solid.

## Claims

### Claim 1

A method, comprising:
mixing dimethyl sulfoxide (DMSO) with water in a volume ratio thereof of 1:1 to yield a solvent DMSO-H2O;
adding a biogenic organic guanidine (G) and a compound MX2 in a molar ratio G/MX2=1:1 or 2:1 to the solvent DMSO-H2O, wherein the organic guanidine (G) is selected from arginine (Arg), guanidinoacetic acid (Gaa), creatine (Cra), creatinine (Cran), guanine (Gua), and agmatine (Agm); M represents Fe2+, Mg2+, or Zn2+; and X represents Cl−, CH3COO−, or CH3CH(OH)COO−;
under nitrogen protection, stirring the solvent DMSO-H2O containing the organic guanidine (G) and the compound MX2 at a temperature of 25-95° C. for 8-12 hours;
recycling the solvent DMSO-H2O through vacuum distillation and obtaining a solid; transferring the solid to a Buchner funnel, and washing the solid with deionized water and ethanol consecutively; and
removing the deionized water and ethanol through vacuum filtration, and drying the solid at 60° C. for 12-14 hours, to yield a guanidine complex GMX2/G2MX2, with a yield of ≥98%;
a process chart of the method being as follows:

### Claim 2

A method, comprising:
adding to a reactor, terephthalic acid (TA), ethylene glycol (EG), and guanidine complex GMX2/G2X2 in a molar ratio TA:EG:GMX2/G2MX2=1.0:1.3:(2.0-3.0)×10−5, wherein G represents arginine (Arg), guanidinoacetic acid (Gaa), creatine (Cra), creatinine (Cran), guanine (Gua), or agmatine (Agm); M represents Fe2+, Mg2+, or Zn2+; and X represents Cl−, CH3COO−, or CH3CH(OH)COO−;
purging the reactor with nitrogen until a pressure of the reactor is 150 kPa; holding the pressure at 220-244° C. for 2.0-2.5 hours; reducing the pressure to 10 kPa, and holding the pressure at 245-257° C. for 40-45 min; further reducing the pressure to 1 kPa, and holding the pressure at 258-264° C. for 30-35 min; reducing the pressure to 5 Pa, and holding the pressure at 265-268° C. for 40-45 min; and
collecting a product in the reactor, pelleting the product, and drying to yield polyethylene terephthalate (PET);
a process chart of the method being as follows:

### Claim 3 (depends on 2)

The method of claim 2, wherein the PET has the following characteristic parameters: intrinsic viscosity ≥0.675 DL/g, melting point ≥257° C., carboxyl end group content 24±4 mole/T, L value of chromaticity ≥80, b value of chromaticity is 1.5±1.5.

### Claim 4

A method, comprising:
adding to a reactor terephthalic acid (TA), isophthalic acid (IPA), ethylene glycol (EG), and guanidine complex GMX2/G2MX2 in a molar ratio of 0.98:0.02:1.30:(2.0-3.0)×10−5, wherein G represents arginine (Arg), guanidinoacetic acid (Gaa), creatine (Cra), creatinine (Cran), guanine (Gua), or agmatine (Agm); M represents Fe2+, Mg2+, or Zn2+; and X represents Cl−, CH3COO−, or CH3CH(OH)COO−;
purging the reactor with nitrogen until a pressure of the reactor is 150 kPa; holding the pressure at 220-244° C. for 2.0-2.5 hours; reducing the pressure to 10 kPa, and holding the pressure at 245-257° C. for 40-45 min; further reducing the pressure to 1 kPa, and holding the pressure at 258-264° C. for 30-35 min; reducing the pressure to 5 Pa, and holding the pressure at 265-268° C. for 40-45 min; and
collecting a product in the reactor, pelleting the product, and drying to yield poly(ethylene isophthalate-co-terephthalate) (PEIT);
a process chart of the method being as follows, wherein Ph represents 1,4-phenylene, and mPh represent 1,3-phenylene:

### Claim 5 (depends on 4)

The method of claim 4, wherein the PEIT has the following characteristic parameters: intrinsic viscosity ≥0.675 DL/g, melting point ≥257° C., carboxyl end group content 24±4 mole/T, L value of chromaticity ≥80, b value of chromaticity is 1.5±1.5.