# US 2022/0033560 A1 · Method for preparing heat-moisture-resistant polyurethane elastomer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0033560 A1
- Document ID: US20220033560A1
- Status: Published application
- Kind: A1
- Application number: 16/944,190
- Filed: 2020-07-31
- Published: 2022-02-03
- Earliest claimed: 2020-07-31
- Assignees: National Chung Shan Institute of Science
- Applicants: National Chung Shan Institute of Science
- Inventors: CHANG-LUN LEE; BEI-HUW SHEN; CHENG-EN LEE; BIING-SHANN YU; MING-HUANG LIN; CHIN-LUNG CHIANG
- Web page: https://patentgrep.com/patent/US20220033560A1

## CPC

- C08G 8/12: with monohydric phenols having only one hydrocarbon substituent ortho on para to the OH group, e.g. p-tert.-butyl phenol
- C08G 18/10: Prepolymer processes involving reaction of isocyanates or isothiocyanates with compounds having active hydrogen in a first reaction step
- C08G 18/246: {containing also tin-carbon bonds}
- C08G 18/3206: {aliphatic}
- C08G 18/48: Polyethers
- C08G 18/4825: {Polyethers containing two hydroxy groups (C08G18/4833 - C08G18/5096 take precedence)}
- C08G 18/755: {and at least one isocyanate or isothiocyanate group linked to a secondary carbon atom of the cycloaliphatic ring, e.g. isophorone diisocyanate}
- C08L 75/08: from polyethers
- C08L 2201/08: Stabilised against heat, light or radiation or oxydation
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

A method for preparing a heat-moisture-resistant polyurethane elastomer includes (A) providing a polyol and an aliphatic diisocyanate to react in the presence of a suitable catalyst under a heating environment, thereby forming a urethane prepolymer with an reactive isocyanate terminal group; (B) providing a hydrophobic diol with a hydroxyl group and/or a castor oil-based triol as a chain extender; and (C) performing an addition reaction of the urethane prepolymer and the chain extender under an appropriate heating environment to generate the heat-moisture-resistant polyurethane elastomer that can be used for a long time in a warm and humid environment.

## Claims

### Claim 1

A method for preparing a heat-moisture-resistant polyurethane elastomer, comprising:
(A) providing a polyol and an aliphatic diisocyanate to react in the presence of a suitable catalyst under a heating environment, thereby forming a urethane prepolymer with a reactive isocyanate terminal group;
(B) providing a diol with a hydroxyl group and/or a castor oil-based triol as a chain extender; and
(C) performing an addition reaction of the urethane prepolymer and the chain extender under an appropriate heating environment to generate a polyurethane elastomer material.

### Claim 2 (depends on 1)

The method for preparing a heat-moisture-resistant polyurethane elastomer of claim 1, wherein a molecular weight of the urethane prepolymer ranges from 1,500 to 5,000.

### Claim 3 (depends on 1)

The method for preparing a heat-moisture-resistant polyurethane elastomer of claim 1, wherein the aliphatic diisocyanate is isophorone diisocyanate.

### Claim 4 (depends on 1)

The method for preparing a heat-moisture-resistant polyurethane elastomer of claim 1, wherein the polyol is selected from aliphatic polyether polyols with a molecular weight from 750 to 2,300.

### Claim 5 (depends on 1)

The method for preparing a heat-moisture-resistant polyurethane elastomer of claim 1, wherein the diol is selected from diols with a branched hydrocarbon configuration and has a molecular weight of 50 to 500.

### Claim 6 (depends on 1)

The method for preparing a heat-moisture-resistant polyurethane elastomer of claim 1, wherein a weight of the castor oil-based triol is not more than 9% of a total weight of the polyurethane elastomer.

### Claim 7 (depends on 1)

The method for preparing a heat-moisture-resistant polyurethane elastomer of claim 1, wherein the heating environment refers to a temperature range of 80-90° C.