# US 2022/0033547 A1 · Tetra-functional long-chain branched ethylene-based polymers

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0033547 A1
- Document ID: US20220033547A1
- Status: Published application
- Kind: A1
- Application number: 17/280,300
- Filed: 2019-09-27
- Published: 2022-02-03
- Earliest claimed: 2018-09-28
- Assignees: Dow Global Technologies LLC
- Applicants: Dow Global Technologies LLC
- Inventors: Teresita Kashyap; Robert D.J. Froese; Daniel J. Arriola
- Web page: https://patentgrep.com/patent/US20220033547A1

## CPC

- C08F 210/16: Copolymers of ethene with alpha-alkenes, e.g. EP rubbers
- C08F 210/18: with non-conjugated dienes, e.g. EPT rubbers
- C08F 210/02: Ethene
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

Ethylene-based polymers of this disclosure include a melt viscosity ratio (V0.1/V100) at 190° C. of at least 10, where V0.1 is the viscosity of the ethylene-based polymer at 190° C. at a shear rate of 0.1 radians/second, and V100 is the viscosity of the ethylene-based polymer at 190° C. at a shear rate of 100 radians/second; and a molecular weight tail quantified by an MWD area metric, ATAIL, and ATAIL is less than or equal to 0.04 as determined by gel permeation chromatography using a triple detector.

## Claims

### Claim 1

An ethylene-based polymer comprising:
a melt viscosity ratio (V0.1/V100) at 190° C. of at least 10, where V0.1 is the viscosity of the ethylene-based polymer at 190° C. at a shear rate of 0.1 radians/second, and V100 is the viscosity of the ethylene-based polymer at 190° C. at a shear rate of 100 radians/second; and
a high molecular weight tail quantified by an MWD area metric, ATAIL, and ATAIL is less than or equal to 0.04 as determined by gel permeation chromatography using a triple detector.

### Claim 2

An ethylene-based polymer comprising:
a melt viscosity ratio (V0.1/V100) at 190° C. of greater than 50, where V0.1 is the viscosity of the ethylene-based polymer at 190° C. at a shear rate of 0.1 radians/second, and V100 is the viscosity of the ethylene-based polymer at 190° C. at a shear rate of 100 radians/second; and
an average g′ is from 0.64 to 0.86, where the average g′ is an intrinsic viscosity ratio determined by gel permeation chromatography using a triple detector.

### Claim 3 (depends on 2)

The ethylene-based polymer of claim 2, wherein the ethylene-based polymer has a high molecular weight tail quantified by an MWD area metric, ATAIL, and ATAIL is less than or equal to 0.04 as determined by gel permeation chromatography using a triple detector.

### Claim 4 (depends on 1)

The ethylene-based polymer of claim 1, wherein the average g′ is from 0.64 to 0.86, where the average g′ is an intrinsic viscosity ratio determined by gel permeation chromatography using a triple detector.

### Claim 5

(canceled)

### Claim 6 (depends on 1)

The ethylene-based polymer of claim 1, wherein the melt viscosity ratio (V0.1/V100) at 190° C. is at least 60, where V0.1 is the viscosity of the ethylene-based polymer at 190° C. at a shear rate of 0.1 radians/second, and V100 is the viscosity of the ethylene-based polymer at 190° C. at a shear rate of 100 radians/second.

### Claim 7 (depends on 1)

The ethylene-based polymer of claim 1, wherein the ethylene-based polymer has a G(79/29) value of less than or equal to 0.04 as determined from a gel permeation chromatography curve using a triple detector having a peak height, a slope M79 at 79% of the peak height, and a slope M29 at 29% of the peak height, wherein the G(79/29) value equals (M79−M29)/M79.

### Claim 8 (depends on 1)

The ethylene-based polymer of claim 1, wherein the ethylene-based polymer has a molecular weight tail quantified by an MWD area metric, ATAIL, and ATAIL is less than or equal to 0.03 as determined by gel permeation chromatography using a triple detector.

### Claim 9 (depends on 1)

The ethylene-based polymer of claim 1, wherein the melt strength is greater than 6 cN (Rheotens device, 190° C., 2.4 mm/s2, 120 mm from the die exit to the center of the wheels, extrusion rate of 38.2 s−1, capillary die of 30 mm length, 2 mm diameter and 180° entrance angle).

### Claim 10 (depends on 1)

The ethylene-based polymer of claim 1, wherein the polymer Mw is less than or equal to 800,000 Daltons, as determined by gel permeation chromatography using a triple detector.

### Claim 11 (depends on 1)

The ethylene-based polymer of claim 1, wherein the polymer Mw is less than or equal to 400,000 Daltons, as determined by gel permeation chromatography using a triple detector.

### Claim 12 (depends on 1)

The ethylene-based polymer of claim 1, wherein the ethylene-based polymer comprises units derived from ethylene, diene, and one or more C3-C12 α-olefin.

### Claim 13 (depends on 12)

The ethylene-based polymer of claim 12, wherein the diene is linear.

### Claim 14 (depends on 12)

The ethylene-based polymer of claim 12, wherein the diene is selected from 2-methyl-1,4-pentadiene, 3-methyl-1,4-pentadiene, 1,3-divinylcyclopentane, 2-methyl-1,5-hexadiene, 1,4-pentadiene, 1,5-hexadiene, 1,7-octadiene, 1,8-nonadiene, 1,9-decadiene, 1,11-dodecadiene, and 1,15-hexadecadiene.

### Claim 15 (depends on 2)

The ethylene-based polymer of claim 2, wherein the melt viscosity ratio (V0.1/V100) at 190° C. is at least 60, where V0.1 is the viscosity of the ethylene-based polymer at 190° C. at a shear rate of 0.1 radians/second, and V100 is the viscosity of the ethylene-based polymer at 190° C. at a shear rate of 100 radians/second.

### Claim 16 (depends on 2)

The ethylene-based polymer of claim 2, wherein the ethylene-based polymer has a G(79/29) value of less than or equal to 0.04 as determined from a gel permeation chromatography curve using a triple detector having a peak height, a slope M79 at 79% of the peak height, and a slope M29 at 29% of the peak height, wherein the G(79/29) value equals (M79−M29)/M79.

### Claim 17 (depends on 2)

The ethylene-based polymer of claim 2, wherein the ethylene-based polymer has a molecular weight tail quantified by an MWD area metric, ATAIL, and ATAIL is less than or equal to 0.03 as determined by gel permeation chromatography using a triple detector.

### Claim 18 (depends on 2)

The ethylene-based polymer of claim 2, wherein the melt strength is greater than 6 cN (Rheotens device, 190° C., 2.4 mm/s2, 120 mm from the die exit to the center of the wheels, extrusion rate of 38.2 s−1, capillary die of 30 mm length, 2 mm diameter and 180° entrance angle).