# US 2022/0033546 A1 · Tetra-functional long-chain branched ethylene-based polymers

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0033546 A1
- Document ID: US20220033546A1
- Status: Published application
- Kind: A1
- Application number: 17/280,293
- Filed: 2019-09-27
- Published: 2022-02-03
- Earliest claimed: 2018-09-28
- Assignees: Dow Global Technologies LLC
- Applicants: Dow Global Technologies LLC
- Inventors: Daniel J. Arriola; Robert D.J. Froese; Teresita Kashyap
- Web page: https://patentgrep.com/patent/US20220033546A1

## CPC

- C08F 210/16: Copolymers of ethene with alpha-alkenes, e.g. EP rubbers
- C08F 210/18: with non-conjugated dienes, e.g. EPT rubbers
- C08F 210/02: Ethene
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

Ethylene-based polymers of this disclosure include an average g′ less than 0.86, where the average g′ is an intrinsic viscosity ratio determined by gel permeation chromatography using a triple detector; and a molecular weight tail quantified by an MWD area metric, ATAIL, and ATAIL is less than or equal to 0.04 as determined by gel permeation chromatography using a triple detector.

## Claims

### Claim 1

An ethylene-based polymer comprising:
an average g′ less than 0.86, where the average g′ is an intrinsic viscosity ratio determined by gel permeation chromatography using a triple detector; and
a high molecular weight tail quantified by an MWD area metric, ATAIL, and ATAIL is less than or equal to 0.04 as determined by gel permeation chromatography using a triple detector.

### Claim 2

An ethylene-based polymer comprising:
a melt strength of greater than 6 cN (Rheotens device, 190° C., 2.4 mm/s2, 120 mm from the die exit to the center of the wheels, extrusion rate of 38.2 s−1, capillary die of 30 mm length, 2 mm diameter and 180° entrance angle); and
a high molecular weight tail quantified by an MWD area metric, ATAIL, and ATAIL is less than or equal to 0.04 as determined by gel permeation chromatography using a triple detector.

### Claim 3 (depends on 2)

The ethylene-based polymer of claim 2, wherein the average g′ is less than 0.86, where the average g′ is an intrinsic viscosity ratio determined by gel permeation chromatography using a triple detector.

### Claim 4 (depends on 1)

The ethylene-based polymer of claim 1, wherein the average g′ is from 0.64 to 0.86, where the average g′ is an intrinsic viscosity ratio determined by gel permeation chromatography using a triple detector.

### Claim 5 (depends on 1)

The ethylene-based polymer of claim 1, wherein the polymer Mw is less than or equal to 800,000 Daltons, as determined by gel permeation chromatography using a triple detector.

### Claim 6 (depends on 1)

The ethylene-based polymer of claim 1, wherein the polymer Mw is less than or equal to 400,000 Daltons, as determined by gel permeation chromatography using a triple detector.

### Claim 7 (depends on 1)

The ethylene-based polymer of claim 1, wherein the melt strength is greater than 10 cN (Rheotens device, 190° C., 2.4 mm/s2, 120 mm from the die exit to the center of the wheels, extrusion rate of 38.2 s−1, capillary die of 30 mm length, 2 mm diameter and 180° entrance angle).

### Claim 8 (depends on 1)

The ethylene-based polymer of claim 1, wherein the ethylene-based polymer has a G(79/29) value of less than or equal to 0.04 as determined from a gel permeation chromatography curve using a triple detector having a peak height, a slope M79 at 79% of the peak height, and a slope M29 at 29% of the peak height, wherein the G(79/29) value equals (M79−M29)/M79.

### Claim 9 (depends on 1)

The ethylene-based polymer of claim 1, wherein the high molecular weight tail quantified by an MWD area metric, ATAIL, and ATAIL is less than or equal to 0.03 as determined by gel permeation chromatography using a triple detector.

### Claim 10 (depends on 1)

The ethylene-based polymer of claim 1, wherein the ethylene-based polymer has a melt viscosity ratio (V0.1/V100) at 190° C. of at least 10, where V0.1 is the viscosity of the ethylene-based polymer at 190° C. at a shear rate of 0.1 radians/second, and V100 is the viscosity of the ethylene-based polymer at 190° C. at a shear rate of 100 radians/second.

### Claim 11 (depends on 1)

The ethylene-based polymer of claim 1, wherein the average g′ is less than 0.80, where the average g′ is an intrinsic viscosity ratio determined by gel permeation chromatography using a triple detector.

### Claim 12 (depends on 1)

The ethylene-based polymer of claim 1, wherein the ethylene-based polymer comprises units derived from ethylene, diene, and one or more C3-C12 α-olefin.

### Claim 13 (depends on 12)

The ethylene-based polymer of claim 12, wherein the diene is linear.

### Claim 14 (depends on 12)

The ethylene-based polymer of claim 12, wherein the diene is selected from 2-methyl-1,4-pentadiene, 3-methyl-1,4-pentadiene, 1,3-divinylcyclopentane, 2-methyl-1,5-hexadiene, 1,4-pentadiene, 1,5-hexadiene, 1,7-octadiene, 1,8-nonadiene, 1,9-decadiene, 1,11-dodecadiene, and 1,15-hexadecadiene.

### Claim 15 (depends on 2)

The ethylene-based polymer of claim 2, wherein the polymer Mw is less than or equal to 800,000 Daltons, as determined by gel permeation chromatography using a triple detector.

### Claim 16 (depends on 2)

The ethylene-based polymer of claim 2, wherein the melt strength is greater than 10 cN (Rheotens device, 190° C., 2.4 mm/s2, 120 mm from the die exit to the center of the wheels, extrusion rate of 38.2 s−1, capillary die of 30 mm length, 2 mm diameter and 180° entrance angle).

### Claim 17 (depends on 2)

The ethylene-based polymer of claim 2, wherein the ethylene-based polymer has a G(79/29) value of less than or equal to 0.04 as determined from a gel permeation chromatography curve using a triple detector having a peak height, a slope M79 at 79% of the peak height, and a slope M29 at 29% of the peak height, wherein the G(79/29) value equals (M79−M29)/M79.

### Claim 18 (depends on 2)

The ethylene-based polymer of claim 2, wherein the high molecular weight tail quantified by an MWD area metric, ATAIL, and ATAIL is less than or equal to 0.03 as determined by gel permeation chromatography using a triple detector.

### Claim 19 (depends on 2)

The ethylene-based polymer of claim 2, wherein the ethylene-based polymer has a melt viscosity ratio (V0.1/V100) at 190° C. of at least 10, where V0.1 is the viscosity of the ethylene-based polymer at 190° C. at a shear rate of 0.1 radians/second, and V100 is the viscosity of the ethylene-based polymer at 190° C. at a shear rate of 100 radians/second.