# US 2022/0033535 A1 · On-Line Adjustment of Mixed Catalyst Ratio and Olefin Polymerization

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0033535 A1
- Document ID: US20220033535A1
- Status: Published application
- Kind: A1
- Application number: 17/279,715
- Filed: 2019-10-30
- Published: 2022-02-03
- Earliest claimed: 2018-11-01
- Applicants: ExxonMobil Chemical Patents Inc.
- Inventors: Kevin A. Stevens; David F. Sanders; Matthew W. Holtcamp; Charles J. Harlan; Xuan Ye; Adriana S. Silva; Matthew S. Bedoya; Joshua P. Olson
- Web page: https://patentgrep.com/patent/US20220033535A1

## CPC

- C08F 2/34: Polymerisation in gaseous state
- C08F 2/01: characterised by special features of the polymerisation apparatus used
- C08F 4/65904: {in combination with another component of C08F4/64}
- C08F 4/65912: {in combination with an organoaluminium compound}
- C08F 4/65916: {supported on a carrier, e.g. silica, MgCl2, polymer}
- C08F 4/65925: {two cyclopentadienyl rings being mutually non-bridged}
- C08F 210/16: Copolymers of ethene with alpha-alkenes, e.g. EP rubbers
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

The present disclosure provides processes for polymerizing olefin(s). In at least one embodiment, a method for producing a polyolefin is provided. The method includes contacting a first composition and a second composition in a line to form a third composition. The first composition includes a contact product of a first catalyst, a second catalyst, a support, a first activator, and a diluent, and the mol ratio of first catalyst to second catalyst is from 90:10 to 40:60. The second composition includes a contact product of the second catalyst, a second activator, and a second diluent. The third composition includes a mol ratio of first catalyst to second catalyst of from 89:11 to 10:90. The method includes introducing the third composition from the line into a gas-phase fluidized bed reactor, exposing the third composition to polymerization conditions, and obtaining a polyolefin.

## Claims

### Claim 1

A method for producing a polyolefin comprising:
contacting a first composition and a second composition in a line to form a third composition, wherein:
the first composition comprises a contact product of a first catalyst, a second catalyst, a support, a first activator, a wax, and a diluent, wherein the mol ratio of first catalyst to second catalyst is from 90:10 to 40:60,
the second composition comprises a contact product of the second catalyst, a second activator, and a second diluent, and
the third composition comprises a mol ratio of first catalyst to second catalyst of from 89:11 to 10:90;
introducing the third composition from the line into a gas-phase fluidized bed reactor;
exposing the third composition to polymerization conditions; and
obtaining a polyolefin.

### Claim 2 (depends on 1)

The method of claim 1, wherein the wax is a paraffin wax and the first composition comprises 10 wt % or greater of the paraffin wax.

### Claim 3 (depends on 1)

The method of claim 1, wherein the polyolefin has a density of from 0.913 g/cm3 to 0.940 g/cm3.

### Claim 4 (depends on 1)

The method of claim 1, wherein the first compositions comprises a mol ratio of first catalyst to second catalyst from 90:10 to 75:25, and the third composition comprises a mol ratio of first catalyst to second catalyst of from 60:40 to 40:60.

### Claim 5 (depends on 1)

The method of claim 1, wherein the polyolefin has a high load melt index (HLMI, as determined by ASTM D1238 at 190° C. and 21.6 kg load) of from 20 to 45 g/10 min.

### Claim 6

(canceled)

### Claim 7

(canceled)

### Claim 8 (depends on 1)

The method of claim 1, wherein the first catalyst is bis(n-propylcyclopentadienyl) hafnium (IV) dimethyl.

### Claim 9 (depends on 8)

The method of claim 8, wherein the second catalyst is di(1-ethylindenyl) zirconium dimethyl.

### Claim 10 (depends on 1)

The method of claim 1, wherein the diluent comprises a mineral oil, and further wherein the mineral oil of the first composition and the second composition has a density of from 0.85 g/cm3 to 0.9 g/cm3 at 25° C. according to ASTM D4052, a kinematic viscosity at 25° C. of from 150 cSt to 200 cSt according to ASTM D341, and an average molecular weight of from 400 g/mol to 600 g/mol according to ASTM D2502.

### Claim 11

(canceled)

### Claim 12 (depends on 2)

The method of claim 2, wherein the first composition comprises 40 wt % or greater of the paraffin wax.

### Claim 13 (depends on 1)

The method of claim 1, wherein the second composition is free of a support.

### Claim 14 (depends on 1)

The method of claim 1, further comprising mixing the third composition in a static mixer before introducing the third composition to the reactor.

### Claim 15 (depends on 1)

The method of claim 1, wherein introducing the third composition into the gas-phase fluidized bed reactor comprises passing the third composition through a nozzle, the nozzle comprising:
a first annulus defined by an inner surface of a first conduit and an outer surface of a second conduit;
a second annulus within the second conduit; and
a third annulus defined by an inner surface of a support member and an outer surface of the first conduit.

### Claim 16 (depends on 15)

The method of claim 15, wherein the support member has a tapered outer diameter.

### Claim 17 (depends on 15)

The method of claim 15, further comprising one or more of the following:
(a) providing ethylene to the nozzle at a flow rate of from 100 to 300 kg/hr;
(b) providing a carrier gas to the nozzle at a flow rate of from 2 to 20 kg/hr; and
(c) providing a carrier fluid to the nozzle at a flow rate of from 10 to 25 kg/hr.

### Claim 18

(canceled)

### Claim 19

(canceled)

### Claim 20 (depends on 1)

The method of claim 1, wherein the support is a silica support.

### Claim 21 (depends on 1)

The method of claim 1, wherein the activator of the first composition and the second composition is an aluminoxane.

### Claim 22 (depends on 1)

The method of claim 1, wherein the method has a trim efficiency value of 50% or greater.

### Claim 23 (depends on 22)

The method of claim 22, wherein the method has a trim efficiency value of 80% or greater.

### Claim 24 (depends on 1)

The method of claim 1, wherein the wax has one or more of the following properties:
a density of from about 0.75 g/cm3 (at 100° C.) to about 0.87 g/cm3 (at 100° C.);
a kinematic viscosity of from 5 mm2/s (at 100° C.) to about 30 mm2/s (at 100° C.);
a boiling point of about 200° C. or greater; and
a melting point of from about 35° C. to about 80° C.

### Claim 25 (depends on 24)

The method of claim 24, wherein the wax has each of the following properties:
a density of from about 0.75 g/cm3 (at 100° C.) to about 0.87 g/cm3 (at 100° C.);
a kinematic viscosity of from 5 mm2/s (at 100° C.) to about 30 mm2/s (at 100° C.);
a boiling point of about 200° C. or greater; and
a melting point of from about 35° C. to about 80° C.