# US 2022/0033316 A1 · Process for Forming Sintered Ceramic Bodies Having Improved Properties

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0033316 A1
- Document ID: US20220033316A1
- Status: Published application
- Kind: A1
- Application number: 17/503,459
- Filed: 2021-10-18
- Published: 2022-02-03
- Earliest claimed: 2017-10-31
- Assignees: James R. Glidewell Dental Ceramics, Inc.
- Applicants: James R. Glidewell Dental Ceramics, Inc.
- Inventors: Sreeram Balasubramanian; Yan Yang; Akash
- Web page: https://patentgrep.com/patent/US20220033316A1

## CPC

- C04B 35/64: Burning or sintering processes (C04B33/32 takes precedence {; powder metallurgy B22F})
- A61C 13/0006: {Production methods}
- A61C 13/0022: {Blanks or green, unfinished dental restoration parts}
- B28B 11/243: {Setting, e.g. drying, dehydrating or firing ceramic articles (B28B11/242 takes precedence)}
- C04B 35/48: based on zirconium or hafnium oxides, zirconates, {zircon} or hafnates
- C04B 35/486: Fine ceramics
- A61C 5/77: Methods or devices for making crowns
- C04B 2235/3246: Stabilised zirconias, e.g. YSZ or cerium stabilised zirconia
- C04B 2235/6027: Slip casting
- C04B 2235/608: Green bodies or pre-forms with well-defined density
- C04B 2235/6562: Heating rate
- C04B 2235/6567: Treatment time
- C04B 2235/661: Multi-step sintering
- C04B 2235/785: Submicron sized grains, i.e. from 0,1 to 1 micron
- C04B 2235/96: Properties of ceramic products, e.g. mechanical properties such as strength, toughness, wear resistance
- C04B 2235/9653: Translucent or transparent ceramics other than alumina
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- A61C: DENTISTRY; APPARATUS OR METHODS FOR ORAL OR DENTAL HYGIENE (non-driven toothbrushes A46B; {tongue scrapers A61B17/24;} preparations for dentistry A61K6/00; preparations for cleaning the teeth or mouth A61K8/00, A61Q11/00)
- B28B: SHAPING CLAY OR OTHER CERAMIC COMPOSITIONS; SHAPING SLAG; SHAPING MIXTURES CONTAINING CEMENTITIOUS MATERIAL, e.g. PLASTER (foundry moulding B22C; working stone or stone-like material B28D; shaping of substances in a plastic state, in general B29C; making layered products not composed wholly of these substances B32B)

## Abstract

A method is provided for making ceramic bodies having improved properties, such as optical and/or strength properties in which the ceramic bodies are densified by new sintering processes. The sintering profiles may have shorter run times than conventional sintering processes. Ceramic bodies made by these methods are suitable for use in dental applications, for example, as crowns.

## Claims

### Claim 1

A method for forming a sintered ceramic body comprising
heating a bisque stage ceramic body in a heating chamber of a sintering oven, comprising
i. in a first heating stage, heating the sintering oven to a first temperature that is from 1200° C. to 1500° C. for an optional first dwell time that is from 0 minutes to 180 minutes, and raising the first temperature from 50° C. to 500° C. to a second temperature between 1400° C. and 1700° C.; and
ii. in a second heating stage, holding the second temperature for a second dwell time of between 0 minutes and 20 minutes.

### Claim 2 (depends on 1)

The method of claim 1, wherein the first heating stage has a ramp rate of 0.5° C./minute to 60° C./minutes from the first heating temperature to the second temperature.

### Claim 3 (depends on 1)

The method of claim 1, wherein the first temperature is from 1350° C. to 1500° C.

### Claim 4 (depends on 1)

The method of claim 1, wherein the first dwell time is from 15 minutes to 180 minutes.

### Claim 5 (depends on 1)

The method of claim 1, wherein the first temperature is from 50° C. to 200° C. lower than the second temperature.

### Claim 6 (depends on 1)

The method of claim 1, wherein the first temperature is from 300° C. to 500° C. lower than the second temperature.

### Claim 7 (depends on 1)

The method of claim 1, wherein the second temperature is from 1530° C. to 1600° C.

### Claim 8 (depends on 1)

The method of claim 1, wherein
i. the first temperature is from 1350° C. to 1500° C. and the first dwell time is from 15 minutes to 180 minutes, and
ii. the second temperature is from 1530° C. to 1600° C. and the second dwell time is from 0 minutes to 20 minutes.

### Claim 9 (depends on 1)

The method of claim 1, wherein the sintering oven is heated to the first temperature from a preliminary heating temperature that is lower than the first temperature, and the preliminary heating temperature is from 1000° C. to 1450° C.

### Claim 10 (depends on 1)

The method of claim 1, further comprising a third heating stage wherein the second temperature is decreased between 50° C. and 200° C. to a third temperature for a dwell time of about 0 minutes to 120 minutes.

### Claim 11 (depends on 10)

The method of claim 10, wherein the third temperature is 1200° C.

### Claim 12 (depends on 10)

The method of claim 10, further comprising a fourth heating stage wherein the third temperature is increased between 100° C. and 800° C. to a fourth temperature for a dwell time of about 0 minutes to about 5 minutes.

### Claim 13 (depends on 12)

The method of claim 12, wherein the fourth temperature is between 1600° C. and 1800° C.

### Claim 14 (depends on 1)

The method of claim 1, wherein the ceramic body comprises yttria-stabilized zirconia stabilized comprising from 2 mol % to 8 mol % yttria.

### Claim 15 (depends on 11)

The method of claim 11, wherein the ceramic body comprises yttria-stabilized zirconia stabilized comprising from 2 mol % to 8 mol % yttria.

### Claim 16 (depends on 13)

The method of claim 13, wherein the ceramic body comprises yttria-stabilized zirconia stabilized comprising from 2 mol % to 8 mol % yttria.