# US 2022/0033309 A1 · Antioxidants in green ceramic bodies containing various oils for improved firing

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0033309 A1
- Document ID: US20220033309A1
- Status: Published application
- Kind: A1
- Application number: 17/502,091
- Filed: 2021-10-15
- Published: 2022-02-03
- Earliest claimed: 2017-07-24
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: Robert Joseph Castilone; Cecilia Sarah Flynn; Mark Alan Lewis; William Joseph Murray; Manivannan Ravichandran; Rachel Marie Shaver; Molly Kyser Walton
- Web page: https://patentgrep.com/patent/US20220033309A1

## CPC

- C04B 35/195: Alkaline earth aluminosilicates, e.g. cordierite {or anorthite}
- C04B 35/10: based on aluminium oxide
- C04B 35/185: Mullite {3Al2O3-2SiO2}
- C04B 35/478: based on aluminium titanates
- C04B 35/565: based on silicon carbide
- C04B 35/63: using additives specially adapted for forming the products {, e.g.. binder binders}
- C04B 35/632: Organic additives
- C04B 35/64: Burning or sintering processes (C04B33/32 takes precedence {; powder metallurgy B22F})
- C04B 38/0006: {Honeycomb structures (from one or more corrugated sheets by winding or stacking C04B38/0083)}
- C10M 101/02: Petroleum fractions
- C04B 2235/3206: Magnesium oxides or oxide-forming salts thereof
- C04B 2235/3217: Aluminum oxide or oxide forming salts thereof, e.g. bauxite, alpha-alumina
- C04B 2235/3232: Titanium oxides or titanates, e.g. rutile or anatase
- C04B 2235/3286: Gallium oxides, gallates, indium oxides, indates, thallium oxides, thallates or oxide forming salts thereof, e.g. zinc gallate
- C04B 2235/3418: Silicon oxide, silicic acids or oxide forming salts thereof, e.g. silica sol, fused silica, silica fume, cristobalite, quartz or flint
- C04B 2235/3463: Alumino-silicates other than clay, e.g. mullite
- C04B 2235/3481: Alkaline earth metal alumino-silicates other than clay, e.g. cordierite, beryl, micas such as margarite, plagioclase feldspars such as anorthite, zeolites such as chabazite
- C04B 2235/5436: micrometer sized, i.e. from 1 to 100 micron
- C04B 2235/6021: Extrusion moulding
- C04B 2235/6567: Treatment time
- C04B 2235/77: Density
- C04B 2235/9684: Oxidation resistance
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- C10M: LUBRICATING COMPOSITIONS (well drilling compositions C09K8/02); USE OF CHEMICAL SUBSTANCES EITHER ALONE OR AS LUBRICATING INGREDIENTS IN A LUBRICATING COMPOSITION (mould release, i.e. separating, agents for metals B22C3/00, for plastics or substances in a plastic state, in general B29C33/56, for glass C03B40/02; textile lubricating compositions D06M11/00, D06M13/00, D06M15/00; immersion oils for microscopy G02B21/33)

## Abstract

Green ceramic mixture for extruding into an extruded green body includes one or more inorganic components selected from the group consisting of ceramic ingredients, inorganic ceramic-forming ingredients, and combinations thereof, at least one mineral oil, and from about 0.01 wt % to about 0.45 wt % of an antioxidant based on a total weight of the inorganic component(s), by super addition. The mineral oil has a kinematic viscosity of ≥about 1.9 cSt at 100° C. The at least one antioxidant may have a degradation-rate peak temperature that is greater than the degradation-rate peak temperature of the at least one mineral oil. In some embodiments, the at least one mineral oil includes greater than about 20 wt % alkanes with greater than 20 carbons, based on a total weight of the at least one mineral oil. Methods of making an unfired extruded body using the batch mixture are also disclosed.

## Claims

### Claim 1

A method of making porous ceramic bodies, the method comprising:
mixing at least one mineral oil, at least one antioxidant, and one or more ceramic ingredients or inorganic ceramic-forming ingredients to form a first batch mixture;
extruding the first batch mixture to form a first green body;
mixing at least one mineral oil, at least one antioxidant, and one or more ceramic ingredients or inorganic ceramic-forming ingredients to form a second batch mixture;
extruding the second batch mixture to form a second green body;
firing the first green honeycomb body in a kiln according to a first firing cycle for a first total firing time sufficient to produce a first porous ceramic body;
firing the second green body in a kiln according to a second firing cycle for a second total firing time sufficient to produce a second porous ceramic body;
wherein the first and second green bodies differ in composition, size, and/or geometry of the respective green body;
wherein the amount of antioxidant included in each respective batch mixture is selected such that the first total firing time is the same as the second total firing time.

### Claim 2 (depends on 1)

The method of claim 1 wherein the at least one mineral oil includes greater than about 20 wt % alkanes with greater than 20 carbons based on a total weight of the at least one mineral oil.

### Claim 3 (depends on 1)

The method of claim 1 wherein the at least one antioxidant is present at about 0.01 wt % to about 0.45 wt %, by super addition, to the one or more ceramic ingredients or inorganic ceramic-forming ingredients.

### Claim 4 (depends on 1)

The method of claim 1 wherein the at least one mineral oil has a kinematic viscosity of equal to or greater than about 1.9 cSt at 100° C.

### Claim 5 (depends on 1)

The method of claim 1 wherein the at least one antioxidant has a thermal degradation-rate peak temperature that is greater than a thermal degradation-rate peak temperature of the at least one mineral oil.

### Claim 6

A method of making porous ceramic bodies, the method comprising:
mixing at least one mineral oil, at least one antioxidant, and one or more ceramic ingredients or inorganic ceramic-forming ingredients to form a first batch mixture;
extruding the first batch mixture to form a first green body;
mixing at least one mineral oil, at least one antioxidant, and one or more ceramic ingredients or inorganic ceramic-forming ingredients to form a second batch mixture;
extruding the second batch mixture to form a second green body;
firing the first green honeycomb body in a kiln according to a first firing cycle for a first total firing time sufficient to produce a first porous ceramic body;
firing the second green honeycomb body in a kiln according to a second firing cycle for a second total firing time sufficient to produce a second porous ceramic body;
wherein the first and second green honeycomb bodies differ in composition, size, and/or geometry of the respective green body;
wherein the amount of antioxidant included in each respective batch mixture is selected such that the thermal peak responses of the respective batch mixtures are aligned with each other.

### Claim 7 (depends on 6)

The method of claim 6 wherein the at least one mineral oil includes greater than about 20 wt % alkanes with greater than 20 carbons based on a total weight of the at least one mineral oil.

### Claim 8 (depends on 6)

The method of claim 6 wherein the at least one antioxidant is present at about 0.01 wt % to about 0.45 wt %, by super addition, to the one or more ceramic ingredients or inorganic ceramic-forming ingredients.

### Claim 9 (depends on 6)

The method of claim 6 wherein the at least one mineral oil has a kinematic viscosity of equal to or greater than about 1.9 cSt at 100° C.

### Claim 10 (depends on 6)

The method of claim 6 wherein the at least one antioxidant has a thermal degradation-rate peak temperature that is greater than a thermal degradation-rate peak temperature of the at least one mineral oil.

### Claim 11

A method of making porous ceramic bodies, the method comprising:
mixing at least one mineral oil, at least one antioxidant, and one or more ceramic ingredients or inorganic ceramic-forming ingredients to form a first batch mixture;
extruding the first batch mixture to form a first green body;
mixing at least one mineral oil, at least one antioxidant, and one or more ceramic ingredients or inorganic ceramic-forming ingredients to form a second batch mixture;
extruding the second batch mixture to form a second green body;
firing the first green honeycomb body in a kiln according to a first firing cycle for a first total firing time sufficient to produce a first porous ceramic body;
firing the second green honeycomb body in a kiln according to a second firing cycle for a second total firing time sufficient to produce a second porous ceramic body;
wherein the first and second green honeycomb bodies differ in composition, size, and/or geometry of the respective green body;
wherein the amount of antioxidant included in each respective batch mixture is selected such that a timing of a first thermal event of the respective batch mixtures occurring in the respective firing cycles are adjusted.

### Claim 12 (depends on 11)

The method of claim 11 wherein the at least one mineral oil includes greater than about 20 wt % alkanes with greater than 20 carbons based on a total weight of the at least one mineral oil.

### Claim 13 (depends on 11)

The method of claim 11 wherein the at least one antioxidant is present at about 0.01 wt % to about 0.45 wt %, by super addition, to the one or more ceramic ingredients or inorganic ceramic-forming ingredients.

### Claim 14 (depends on 11)

The method of claim 11 wherein the at least one mineral oil has a kinematic viscosity of equal to or greater than about 1.9 cSt at 100° C.

### Claim 15 (depends on 11)

The method of claim 11 wherein the at least one antioxidant has a thermal degradation-rate peak temperature that is greater than a thermal degradation-rate peak temperature of the at least one mineral oil.