# US 2022/0033285 A1 · Copper Integrated Electrode with Convertible Oxidation State and Preparation Method and Application Method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0033285 A1
- Document ID: US20220033285A1
- Status: Published application
- Kind: A1
- Application number: 17/095,746
- Filed: 2020-11-12
- Published: 2022-02-03
- Earliest claimed: 2020-07-31
- Assignees: Tongji University
- Applicants: Tongji University
- Inventors: Ying WANG; Fengting LI; Tao FENG
- Web page: https://patentgrep.com/patent/US20220033285A1

## CPC

- C02F 1/46109: {Electrodes}
- C01B 32/198: Graphene oxide
- C02F 1/4676: {by electroreduction}
- C25B 1/01: Products
- C25B 11/02: characterised by shape or form
- C25B 11/031: Porous electrodes
- C25B 11/054: Electrodes comprising electrocatalysts supported on a carrier
- C25B 11/061: Metal or alloy
- C25B 11/069: consisting of at least one single element and at least one compound; consisting of two or more compounds
- C25B 11/077: the compound being a non-noble metal oxide
- B82Y 30/00: Nanotechnology for materials or surface science, e.g. nanocomposites
- C02F 2001/46133: {characterised by the material}
- C02F 2001/46138: {Electrodes comprising a substrate and a coating}
- C02F 2001/46142: {Catalytic coating}
- C02F 2101/163: {Nitrates}
- C02F: TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE (separation in general B01D; special arrangements on waterborne vessels of installations for treating water, waste water or sewage, e.g. for producing fresh water, B63J; adding materials to water to prevent corrosion C23F; treating radioactively-contaminated liquids G21F9/04; regeneration of reactants for recirculation into processes, see the relevant places for the processes)
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C25B: ELECTROLYTIC OR ELECTROPHORETIC PROCESSES FOR THE PRODUCTION OF COMPOUNDS OR NON-METALS; APPARATUS THEREFOR (anodic or cathodic protection C23F13/00; single-crystal growth C30B)
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES

## Abstract

A copper integrated electrode with a convertible oxidation state, a preparation method and an application method are provided. The preparation process is based on an electrochemically induced self-growth method. Copper foam is used as a precursor, soaked in a graphene oxide solution, dried, calcined at high temperature and annealed, and then treated with an alkali solution to obtain the copper integrated electrode with the convertible oxidation state. The working electrode prepared by the nano-catalytic material of the present invention has good denitrification performance in the environmental field, which can achieve nearly 100% nitrate removal rate, nearly 100% nitrogen selectivity and long-term stability. These properties are due to the prepared working electrode having an oxidizable copper (I, II/0, I), oxygen vacancy (O) and a one-dimensional nanowire structure. The structure can regulate the adsorption and reduction of intermediate products, resulting in nearly 100% nitrate removal rate and nearly 100% nitrogen selectivity.

## Claims

### Claim 1

A preparation method of a copper integrated electrode with a convertible oxidation state, comprising the following steps:
1) cutting a copper foam into a copper foam strip, and washing the copper foam strip with ethanol and acetone to remove surface impurities of the copper foam strip to obtain a washed copper foam strip;
2) drying the washed copper foam strip obtained in step 1) at room temperature to obtain a dried copper foam strip, and immersing the dried copper foam strip in a graphene oxide solution with a concentration of 0.1 mg/mL-10 mg/mL for 1 min-10 min, covering a surface of the dried copper foam strip with a carbon layer to obtain a carbon coated copper foam strip, transferring the carbon coated copper foam strip to a constant temperature oven, and drying the carbon coated copper foam strip for 1 h-10 h at 50° C.-100° C. to obtain a copper foam carrier;
3) calcining the copper foam carrier obtained in step 2) for 1 h-5 h at 200° C.-500° C. in a tubular furnace with an argon atmosphere to obtain a C—Cu electrode substrate;
4) after cutting the C—Cu electrode substrate obtained in step 3) to a size of 1 cm×1 cm to obtain a trimmed C—Cu electrode substrate, cleaning the trimmed C—Cu electrode substrate 2-3 times with ultrapure water to obtain a first washed C—Cu electrode substrate, placing the first washed C—Cu electrode substrate in an alkali solution with a concentration of 0.1 M-1 M for a CV scanning for 1-400 cycles in a voltage range of −1 V-+1 V by a cyclic voltammetry to obtain a treated C—Cu electrode substrate, then cleaning the treated C—Cu electrode substrate 2-3 times with ultrapure water again to obtain a second washed C—Cu electrode substrate and drying the second washed C—Cu electrode substrate to obtain the copper integrated electrode with the convertible oxidation state.

### Claim 2 (depends on 1)

The preparation method according to claim 1, wherein a concentration of a graphene oxide in the graphene oxide solution is 0.1 mg/mL-5 mg/mL;
a preparation method of the graphene oxide solution comprises the following steps:
M1: adding 2 g of graphite powder with a particle size of 325 mesh into concentrated sulfuric acid containing K2S208 and P2O5 for a uniform mixing to obtain a first mixed solution, heating the first mixed solution to 80° C. and keeping the first mixed solution at 80° C. for a first reaction under reflux and stirring for 5 h to obtain a first mixture, after the first reaction is completed, pouring the first mixture into 500 mL of pure water for stirring, mixing and putting aside to form a first precipitate, and filtering the first precipitate through a 0.2 μm filter membrane to obtain a first filtered precipitate, and then washing the first filtered precipitate with pure water to obtain a first washed precipitate, and drying the first washed precipitate in the air to obtain a pre-oxidized graphite;
M2: adding the pre-oxidized graphite obtained in step M1 into 120 mL of concentrated sulfuric acid in a state of ice bath to obtain a second mixture, slowly adding 25 g of KMnO4 at 4° C.-6° C. into the second mixture under a constant stirring to obtain a third mixture, continuing to stir the third mixture at 35° C. for 4 h, then slowly adding 250 mL of deionized water into the third mixture to obtain a second mixed solution for a second reaction at a temperature below 50° C. to obtain a fourth mixture;
M3: adding 1 L of deionized water to the fourth mixture obtained in step M2 to obtain a third mixed solution, then slowly adding 30 mL of a hydrogen peroxide solution with a mass fraction of 30% dropwise into the third mixed solution to obtain a fourth mixed solution, fully stirring the fourth mixed solution for a third reaction to obtain a second precipitate, washing the second precipitate with 1 L of dilute hydrochloric acid with a volume ratio of 1:10 to remove unreacted KMnO4 on the second precipitate to obtain a second washed precipitate, and then washing the second washed precipitate with 1 L of deionized water to remove residual dilute hydrochloric acid on the second washed precipitate to obtain a fifth mixture;
M4: filtering the fifth mixture obtained in step M3 to obtain a graphene oxide solid, dissolving the graphene oxide solid with deionized water to prepare a graphene oxide solution with a mass fraction of 0.5%;
M5: dialyzing continuously the graphene oxide solution obtained in step M4 for 1 week to remove residual metal ion impurities to obtain a dialyzed graphene oxide solution, performing a suction filtration on the dialyzed graphene oxide solution to obtain graphene oxide solid powder, and preparing the graphene oxide solid powder into a graphene oxide solution with a first predetermined concentration, then stripping a graphene material in the graphene oxide solution with the first predetermined concentration by an ultrasonic method to finally obtain a graphene oxide solution with a second predetermined concentration in a uniform light yellow and clear state.

### Claim 3 (depends on 1)

The preparation method according to claim 1, wherein the alkali solution is a NaOH solution.

### Claim 4 (depends on 1)

The preparation method according to claim 1, wherein the voltage range of the cyclic voltammetry in step 4) is −0.5 V-+0.85 V.

### Claim 5 (depends on 1)

A copper integrated electrode with a convertible oxidation state prepared by the preparation method according to claim 1, wherein the copper integrated electrode is a single metal copper self-supporting Cu2O nanowires electrode.

### Claim 6 (depends on 5)

An application method of the copper integrated electrode with the convertible oxidation state according to claim 5 in a denitrification treatment of a water body containing nitrate, comprising:
forming a three-electrode system using the copper integrated electrode with the convertible oxidation state as a working electrode, a platinum electrode as a counter electrode, and an Ag/AgCl electrode as a reference electrode; and
placing the three-electrode system in the water body containing the nitrate for the denitrification treatment.

### Claim 7 (depends on 6)

The application method according to claim 6, wherein a concentration of the nitrate in the water body containing the nitrate is 10 mgN/L-300 mgN/L.

### Claim 8 (depends on 6)

The application method according to claim 6, wherein a mixed electrolyte of Na2SO4 and NaCl is used in the three-electrode system.

### Claim 9 (depends on 8)

The application method according to claim 8, wherein in the mixed electrolyte of the Na2SO4 and the NaCl, a concentration of the Na2SO4 is 0.06 mol/L-0.2 mol/L, and a concentration of the NaCl is 0.01 mol/L-0.05 mol/L.

### Claim 10 (depends on 6)

The application method according to claim 6, wherein an applied voltage of the denitrification treatment is −1.1 V-−1.5 V, and a denitrification time is 1 h-28 h.

### Claim 11 (depends on 5)

The copper integrated electrode according to claim 5, wherein a concentration of a graphene oxide in the graphene oxide solution is 0.1 mg/mL-5 mg/mL;
a preparation method of the graphene oxide solution comprises the following steps:
M1: adding 2 g of graphite powder with a particle size of 325 mesh into concentrated sulfuric acid containing K2S208 and P2O5 for a uniform mixing to obtain a first mixed solution, heating the first mixed solution to 80° C. and keeping the first mixed solution at 80° C. for a first reaction under reflux and stirring for 5 h to obtain a first mixture, after the first reaction is completed, pouring the first mixture into 500 mL of pure water for stirring, mixing and putting aside to form a first precipitate, and filtering the first precipitate through a 0.2 μm filter membrane to obtain a first filtered precipitate, and then washing the first filtered precipitate with pure water to obtain a first washed precipitate, and drying the first washed precipitate in the air to obtain a pre-oxidized graphite;
M2: adding the pre-oxidized graphite obtained in step M1 into 120 mL of concentrated sulfuric acid in a state of ice bath to obtain a second mixture, slowly adding 25 g of KMnO4 at 4° C.-6° C. into the second mixture under a constant stirring to obtain a third mixture, continuing to stir the third mixture at 35° C. for 4 h, then slowly adding 250 mL of deionized water into the third mixture to obtain a second mixed solution for a second reaction at a temperature below 50° C. to obtain a fourth mixture;
M3: adding 1 L of deionized water to the fourth mixture obtained in step M2 to obtain a third mixed solution, then slowly adding 30 mL of a hydrogen peroxide solution with a mass fraction of 30% dropwise into the third mixed solution to obtain a fourth mixed solution, fully stirring the fourth mixed solution for a third reaction to obtain a second precipitate, washing the second precipitate with 1 L of dilute hydrochloric acid with a volume ratio of 1:10 to remove unreacted KMnO4 on the second precipitate to obtain a second washed precipitate, and then washing the second washed precipitate with 1 L of deionized water to remove residual dilute hydrochloric acid on the second washed precipitate to obtain a fifth mixture;
M4: filtering the fifth mixture obtained in step M3 to obtain a graphene oxide solid, dissolving the graphene oxide solid with deionized water to prepare a graphene oxide solution with a mass fraction of 0.5%;
M5: dialyzing continuously the graphene oxide solution obtained in step M4 for 1 week to remove residual metal ion impurities to obtain a dialyzed graphene oxide solution, performing a suction filtration on the dialyzed graphene oxide solution to obtain graphene oxide solid powder, and preparing the graphene oxide solid powder into a graphene oxide solution with a first predetermined concentration, then stripping a graphene material in the graphene oxide solution with the first predetermined concentration by an ultrasonic method to finally obtain a graphene oxide solution with a second predetermined concentration in a uniform light yellow and clear state.

### Claim 12 (depends on 5)

The copper integrated electrode according to claim 5, wherein the alkali solution is a NaOH solution.

### Claim 13 (depends on 5)

The copper integrated electrode according to claim 5, wherein the voltage range of the cyclic voltammetry in step 4) is −0.5 V-+0.85 V.