# US 2022/0033276 A1 · Method for producing positive electrode active substance for non-aqueous electrolyte secondary battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0033276 A1
- Document ID: US20220033276A1
- Status: Published application
- Kind: A1
- Application number: 17/430,881
- Filed: 2020-01-21
- Published: 2022-02-03
- Earliest claimed: 2019-02-27
- Assignees: Panasonic Intellectual Property Management Co., Ltd.
- Applicants: Panasonic Intellectual Property Management Co., Ltd.
- Inventors: Akihiro Kawakita; Takeshi Ogasawara; Yuji Goshima
- Web page: https://patentgrep.com/patent/US20220033276A1

## CPC

- C01G 53/42: containing alkali metals, e.g. LiNiO2
- H01M 4/366: {as layered products}
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 4/62: Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- C01P 2002/52: containing elements as dopants
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2004/84: one phase coated with the other
- C01P 2006/82: water content
- H01M 10/052: Li-accumulators
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method for producing a positive electrode active substance for a non-aqueous electrolyte secondary battery is characterized by including: a washing step for washing a lithium-containing transition metal oxide with water and then dehydrating the same so as to obtain a cake-like composition; a tungsten addition step for adding at least a tungsten compound or a tungsten-containing solution to the cake-like composition so as to obtain a tungsten-added product; a first heat treatment step for heat treating the tungsten-added product at a temperature of 180° C. or lower; and a second heat treatment step for heat treating the tungsten-added product in an atmosphere other than a reducing atmosphere at a temperature of higher than 180° C. to 330° C. This method is further characterized by including a boron addition step for adding a boron compound or a boron-containing solution to the cake-like composition.

## Claims

### Claim 1

A method for producing a positive electrode active material for a non-aqueous electrolyte secondary battery, the method comprising:
washing with water and dehydrating a lithium-containing transition metal oxide to obtain a cake-like composition;
adding tungsten by adding at least one of a tungsten compound or a tungsten-containing solution to the cake-like composition to obtain a tungsten additive;
first heat treating that heat treats the tungsten additive at a temperature of 180° C. or lower; and
second heat treating that heat treats the tungsten additive at a temperature in a range from over 180° C. to 330° C. in an atmosphere other than a reducing atmosphere,
wherein the method further comprises adding boron by adding a boron compound or a boron-containing solution to the cake-like composition before the adding of tungsten, to the tungsten additive before the first heat treating, to the tungsten additive before the second heat treating after the first heat treating or to the tungsten additive during the second heat treating after the first heat treating.

### Claim 2 (depends on 1)

The method for producing the positive electrode active material for the non-aqueous electrolyte secondary battery according to claim 1, wherein the lithium-containing transition metal oxide is expressed by a general formula: LizNi1-x-yCoxMyO2, where 0≤x≤0.2, 0≤y≤0.1, 0.97≤z≤1.20, and M is at least one element selected from the group consisting of Mn, W, Mg, Mo, Nb, Ti, Si, and Al.

### Claim 3 (depends on 1)

The method for producing the positive electrode active material for the non-aqueous electrolyte secondary battery according to claim 1, wherein the adding boron is performed after the first heat treating.

### Claim 4 (depends on 1)

The method for producing the positive electrode active material for the non-aqueous electrolyte secondary battery according to claim 1, wherein
the water content of the cake-like composition after the washing is 10 wt % or lower, and the water content of the cake-like composition or the tungsten additive before the adding boron is 2 wt % or lower.

### Claim 5 (depends on 1)

The method for producing the positive electrode active material for the non-aqueous electrolyte secondary battery according to claim 1, wherein in the adding boron, the boron compound is boron acid.

### Claim 6 (depends on 1)

The method for producing the positive electrode active material for the non-aqueous electrolyte secondary battery according to claim 1, wherein
the method further comprises cooling the tungsten additive after the second heat treating such that the temperature of the tungsten additive drops to 100° C. or lower within one hour after the second heat treating.