# US 2022/0033266 A1 · Copper ion-doped carbon dots, preparation method and application thereof as photosensitizer for photodynamic therapy

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0033266 A1
- Document ID: US20220033266A1
- Status: Published application
- Kind: A1
- Application number: 17/277,298
- Filed: 2019-03-15
- Published: 2022-02-03
- Earliest claimed: 2019-02-28
- Assignees: Anhui University
- Applicants: Anhui University
- Inventors: Hong BI; Mingsheng XU; Jingmin WANG; Antonio Claudio TEDESCO
- Web page: https://patentgrep.com/patent/US20220033266A1

## CPC

- C01B 32/914: Carbides of single elements
- A61K 33/34: Copper; Compounds thereof
- A61K 41/0057: {Photodynamic therapy with a photosensitizer, i.e. agent able to produce reactive oxygen species upon exposure to light or radiation, e.g. UV or visible light; photocleavage of nucleic acids with an agent}
- A61P 17/00: Drugs for dermatological disorders
- A61P 27/02: Ophthalmic agents
- A61P 35/00: Antineoplastic agents
- C01B 32/15: Nano-sized carbon materials
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- A61K: PREPARATIONS FOR MEDICAL, DENTAL OR TOILETRY PURPOSES (devices or methods specially adapted for bringing pharmaceutical products into particular physical or administering forms A61J3/00; chemical aspects of, or use of materials for deodorisation of air, for disinfection or sterilisation, or for bandages, dressings, absorbent pads or surgical articles A61L; soap compositions C11D)
- A61P: SPECIFIC THERAPEUTIC ACTIVITY OF CHEMICAL COMPOUNDS OR MEDICINAL PREPARATIONS

## Abstract

Copper ion-doped carbon dots (Cu-CDs) and a preparation method thereof are disclosed. The preparation method includes the following steps: using copper nitrate as a dopant to generate a complex of polyacrylic acid and copper ions as a precursor by an in situ polymerization; standing overnight, and performing repeated suction filtration to collect filter residues; then, performing pyrolysis and carbonization to generate carbonized products, dispersing in ultrapure water, taking a supernatant, and then performing extraction and purification to obtain the CDs. When the Cu-CDs prepared by the present invention are used in photodynamic therapy, photothermal/photodynamic synergistic therapy is not required, and the Cu-CDs are suitable for the therapeutic process of skin cancer, lung cancer, pancreatic cancer, esophageal cancer, brain glioma, as well as some skin diseases and ophthalmological diseases.

## Claims

### Claim 1

A preparation method of copper ion-doped carbon dots (Cu-CDs), comprising: using copper nitrate as a dopant to generate a complex of polyacrylic acid and copper ions by an in situ polymerization, wherein the complex of polyacrylic acid and copper ions is used as a precursor, standing the precursor overnight, and performing a repeated suction filtration on the precursor to collect filter residues; then performing a pyrolysis and a carbonization on the filter residues to generate a carbonized product, dispersing the carbonized product in ultrapure water to obtain a mixture, taking a supernatant from the mixture, and then performing an extraction and a purification on the supernatant to obtain the Cu-CDs.

### Claim 2 (depends on 1)

The preparation method of the Cu-CDs according to claim 1, specifically comprising the following steps:
1) weighing and adding 0.3 mol·L−1 acrylic acid, a 0.2 mol·L−1 copper nitrate solution, ammonium persulfate and hydrazine hydrate to a beaker for a reaction for a predetermined time to obtain a solution, and standing the solution overnight;
2) subjecting the solution to a first suction filtration, collecting and dispersing a first filter residue in a predetermined amount of the ultrapure water, then performing a second suction filtration, collecting a second filter residue for a vacuum drying at a predetermined temperature, and collecting a powder;
3) spreading the powder of step 2) in a crucible, putting the crucible in a muffle furnace for the pyrolysis in an air atmosphere to obtain a carbonized powder, taking out the carbonized powder in the crucible, grinding the carbonized powder in a mortar to obtain a ground carbonized powder, then performing an ultrasonic treatment on the ground carbonized powder for a plurality of times to disperse the ground carbonized powder in a predetermined amount of the ultrapure water to obtain the mixture, and then standing the mixture for subsequently use; then, performing a third suction filtration on the mixture, pouring out the supernatant from the mixture, and then putting the supernatant into a dialysis bag with a predetermined molecular weight cut-off for the dialysis in the ultrapure water to obtain a resulting product, and performing a freeze-drying on the resulting product to obtain the Cu-CDs with a yellow-brown color.

### Claim 3 (depends on 2)

The preparation method of the Cu-CDs according to claim 2, wherein in the step 1), 10-20 mL of the acrylic acid, 2-10 mL of the copper nitrate solution, 10-30 mL of the ammonium persulfate and 5-10 mL of the hydrazine hydrate are added, and the predetermined time for the reaction is 25-40 min.

### Claim 4 (depends on 2)

The preparation method of the Cu-CDs according to claim 2, wherein the predetermined temperature of the vacuum drying in the step 2) is 30° C.-45° C.

### Claim 5 (depends on 2)

The preparation method of the Cu-CDs according to claim 2, wherein in the step 3), a heating rate of the pyrolysis is 2-10° C./min, a temperature for the pyrolysis is 300° C.-500° C., and a time for the pyrolysis is 1.5-2 h.

### Claim 6 (depends on 2)

The preparation method of the Cu-CDs according to claim 2, wherein an organic aqueous microporous filter membrane with a pore diameter of 0.22 μm is used for the first suction filtration, the second suction filtration and the third suction filtration in the step 2) and step 3).

### Claim 7 (depends on 2)

The preparation method of the Cu-CDs according to claim 2, wherein in the step 3), the predetermined molecular weight cut-off of the dialysis bag is 500-1000, a time for the dialysis is 48-72 h and a time for the freeze-drying is 56-72 h.

### Claim 8 (depends on 1)

Cu-CDs, wherein the Cu-CDs are obtained by the preparation method according to claim 1.

### Claim 9 (depends on 1)

A method of a photodynamic therapy, comprising the step of using the Cu-CDs prepared by the preparation method according to claim 1 as a photosensitizer for the photodynamic therapy.

### Claim 10 (depends on 8)

The Cu-CDs according to claim 8, wherein the preparation method specifically comprises the following steps:
1) weighing and adding 0.3 mol·L−1 acrylic acid, a 0.2 mol·−1 copper nitrate solution, ammonium persulfate and hydrazine hydrate to a beaker for a reaction for a predetermined time to obtain a solution, and standing the solution overnight;
2) subjecting the solution to a first suction filtration, collecting and dispersing a first filter residue in a predetermined amount of the ultrapure water, then performing a second suction filtration, collecting a second filter residue for a vacuum drying at a predetermined temperature, and collecting a powder;
3) spreading the powder of step 2) in a crucible, putting the crucible in a muffle furnace for the pyrolysis in an air atmosphere to obtain a carbonized powder, taking out the carbonized powder in the crucible, grinding the carbonized powder in a mortar to obtain a ground carbonized powder, then performing an ultrasonic treatment on the ground carbonized powder for a plurality of times to disperse the ground carbonized powder in a predetermined amount of the ultrapure water to obtain the mixture, and then standing the mixture for subsequently use; then, performing a third suction filtration on the mixture, pouring out the supernatant from the mixture, and then putting the supernatant into a dialysis bag with a predetermined molecular weight cut-off for the dialysis in the ultrapure water to obtain a resulting product, and performing a freeze-drying on the resulting product to obtain the Cu-CDs with a yellow-brown color.

### Claim 11 (depends on 10)

The Cu-CDs according to claim 10, wherein in the step 1), 10-20 mL of the acrylic acid, 2-10 mL of the copper nitrate solution, 10-30 mL of the ammonium persulfate and 5-10 mL of the hydrazine hydrate are added, and the predetermined time for the reaction is 25-40 min.

### Claim 12 (depends on 10)

The Cu-CDs according to claim 10, wherein the predetermined temperature of the vacuum drying in the step 2) is 30° C.-45° C.

### Claim 13 (depends on 10)

The Cu-CDs according to claim 10, wherein in the step 3), a heating rate of the pyrolysis is 2-10° C./min, a temperature for the pyrolysis is 300° C.-500° C., and a time for the pyrolysis is 1.5-2 h.

### Claim 14 (depends on 10)

The Cu-CDs according to claim 10, wherein an organic aqueous microporous filter membrane with a pore diameter of 0.22 μm is used for the first suction filtration, the second suction filtration and the third suction filtration in the step 2) and step 3).

### Claim 15 (depends on 10)

The Cu-CDs according to claim 10, wherein in the step 3), the predetermined molecular weight cut-off of the dialysis bag is 500-1000, a time for the dialysis is 48-72 h and a time for the freeze-drying is 56-72 h.

### Claim 16 (depends on 9)

The method according to claim 9, wherein the preparation method specifically comprises the following steps:
1) weighing and adding 0.3 mol·L−1 acrylic acid, a 0.2 mol·L−1 copper nitrate solution, ammonium persulfate and hydrazine hydrate to a beaker for a reaction for a predetermined time to obtain a solution, and standing the solution overnight;
2) subjecting the solution to a first suction filtration, collecting and dispersing a first filter residue in a predetermined amount of the ultrapure water, then performing a second suction filtration, collecting a second filter residue for a vacuum drying at a predetermined temperature, and collecting a powder;
3) spreading the powder of step 2) in a crucible, putting the crucible in a muffle furnace for the pyrolysis in an air atmosphere to obtain a carbonized powder, taking out the carbonized powder in the crucible, grinding the carbonized powder in a mortar to obtain a ground carbonized powder, then performing an ultrasonic treatment on the ground carbonized powder for a plurality of times to disperse the ground carbonized powder in a predetermined amount of the ultrapure water to obtain the mixture, and then standing the mixture for subsequently use; then, performing a third suction filtration on the mixture, pouring out the supernatant from the mixture, and then putting the supernatant into a dialysis bag with a predetermined molecular weight cut-off for the dialysis in the ultrapure water to obtain a resulting product, and performing a freeze-drying on the resulting product to obtain the Cu-CDs with a yellow-brown color.

### Claim 17 (depends on 16)

The method according to claim 16, wherein in the step 1), 10-20 mL of the acrylic acid, 2-10 mL of the copper nitrate solution, 10-30 mL of the ammonium persulfate and 5-10 mL of the hydrazine hydrate are added, and the predetermined time for the reaction is 25-40 min.

### Claim 18 (depends on 16)

The method according to claim 16, wherein the predetermined temperature of the vacuum drying in the step 2) is 30° C.-45° C.

### Claim 19 (depends on 16)

The method according to claim 16, wherein in the step 3), a heating rate of the pyrolysis is 2-10° C./min, a temperature for the pyrolysis is 300° C.-500° C., and a time for the pyrolysis is 1.5-2 h.

### Claim 20 (depends on 16)

The method according to claim 16, wherein an organic aqueous microporous filter membrane with a pore diameter of 0.22 μm is used for the first suction filtration, the second suction filtration and the third suction filtration in the step 2) and step 3).