# US 2022/0032697 A1 · Method for Fabricating a Tow Hook Assembly

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0032697 A1
- Document ID: US20220032697A1
- Status: Published application
- Kind: A1
- Application number: 16/943,059
- Filed: 2020-07-30
- Published: 2022-02-03
- Earliest claimed: 2020-07-30
- Assignees: Trenton Forging Company
- Applicants: Trenton Forging Company
- Inventors: David Moxlow; Dane Moxlow; Robert Hopkins
- Web page: https://patentgrep.com/patent/US20220032697A1

## CPC

- C21D 9/0068: {for particular articles not mentioned below}
- B60D 1/04: Hook or hook-and-hasp couplings
- B60D 1/565: {having an eyelet}
- C21D 9/46: for sheet metals
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- B60D: VEHICLE CONNECTIONS

## Abstract

A method for manufacturing a tow hook assembly begins with heating a first steel blank to within a range of 2200° F. and 2300° F. to create a first heated steel blank. A second steel blank is heated to within the range of 2200° F. at 2300° F. to create a second heated steel blank. The first heated steel blank is forged into a tow hook. The second heated steel blank is forged into a flange plate. The tow hook in the flange plate are welded together to form the tow hook assembly. This method reduces waste by minimizing the size of the first and second steel blanks.

## Claims

### Claim 1

A method for manufacturing a tow hook assembly, the method comprising the steps of:
heating a first steel blank to within a range between 2200° F. and 2300° F. to create a first heated steel blank;
heating a second steel blank to within a range between 2200° F. and 2300° F. to create a second heated steel blank;
forging the first heated steel blank into a tow hook main body;
forging the second heated steel blank into a flange plate; and
welding the tow hook in the flange plate together to form a tow hook assembly.

### Claim 2 (depends on 1)

A method as set forth in claim 1 including the step of cooling the tow hook main body and the flange plate prior to the step of welding.

### Claim 3 (depends on 2)

A method as set forth in claim 2 wherein the step of cooling reduces the temperature of the tow hook main body and the flange plate to room temperature.

### Claim 4 (depends on 1)

A method as set forth in claim 1 wherein the step of forging the flange plate includes forming two holes.

### Claim 5 (depends on 3)

A method as set forth in claim 3 including the step of forming an alignment boss in the tow hook main body.

### Claim 6 (depends on 5)

A method as set forth in claim 5 including the step of forming an alignment recess in the flange plate.

### Claim 7 (depends on 6)

A method as set forth in claim 6 including the step of inserting the alignment boss of the tow hook into the alignment recess of the flange prior to the step of welding and after the step of cooling.