# US 2022/0032596 A1 · Bonding Method to Attach Ethylene-Based Polymer Foam with Vulcanized Rubber

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0032596 A1
- Document ID: US20220032596A1
- Status: Published application
- Kind: A1
- Application number: 17/277,565
- Filed: 2018-09-20
- Published: 2022-02-03
- Earliest claimed: 2018-09-20
- Assignees: Dow Global Technologies LLC
- Applicants: Dow Global Technologies LLC
- Inventors: Haiyang Yu; Wanfu Ma; Xin Liu
- Web page: https://patentgrep.com/patent/US20220032596A1

## CPC

- B32B 37/12: characterised by using adhesives
- A43B 13/04: Plastics, rubber or vulcanised fibre
- A43B 13/12: Soles with several layers of different materials
- A43B 13/187: {Resiliency achieved by the features of the material, e.g. foam, non liquid materials}
- B32B 5/18: characterised by features of a layer {of} foamed material
- B32B 7/12: using interposed adhesives or interposed materials with bonding properties
- B32B 25/04: comprising rubber as the main or only constituent of a layer, {which is} next to another layer of {the same or of} a {different material (next to a layer of a particular substance B32B9/043; next to a bituminous or tarry layer B32B11/044; next to a water setting substance layer B32B13/042; next to a metal layer B32B15/06; next to a glass layer B32B17/063; next to a layer formed of natural mineral fibres or particles B32B19/043; next to a wood layer B32B21/045; next to a cellulosic plastic layer B32B23/046)}
- B32B 25/045: {of foam}
- B32B 25/08: of synthetic resin
- B32B 25/14: comprising {synthetic rubber copolymers (B32B25/18 and B32B25/20 take precedence)}
- B32B 25/16: comprising polydienes {homopolymers} or poly-halodienes {homopolymers (B32B25/12 takes precedence)}
- B32B 27/065: {of foam}
- B32B 27/32: comprising polyolefins {(comprising vinyl (co)polymers or acrylic (co)polymers B32B27/30)}
- B32B 27/327: {comprising polyolefins obtained by a metallocene or single-site catalyst}
- B32B 37/10: characterised by the pressing technique, e.g. using action of vacuum or fluid pressure
- B32B 37/14: characterised by the properties of the layers
- B32B 37/182: {one or more of the layers being plastic}
- B29D 35/142: {Soles}
- B29L 2031/504: {Soles}
- B32B 37/02: characterised by a sequence of laminating steps, e.g. by adding new layers at consecutive laminating stations
- B32B 2250/03: 3 layers
- B32B 2250/24: All layers being polymeric
- B32B 2266/025: Polyolefin
- B32B 2307/30: having particular thermal properties
- B32B 2307/54: Yield strength; Tensile strength
- B32B 2307/72: Density
- B32B 2307/732: Dimensional properties
- B32B 2307/748: Releasability
- B32B 2437/02: Gloves, shoes
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- A43B: CHARACTERISTIC FEATURES OF FOOTWEAR; PARTS OF FOOTWEAR
- B29D: PRODUCING PARTICULAR ARTICLES FROM PLASTICS OR FROM SUBSTANCES IN A PLASTIC STATE (making granules B29B9/00; making preforms B29B11/00)
- B29L: INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULAR ARTICLES

## Abstract

A process of adhering a foam structure to a rubber substrate is provided. The foam structure is composed of a first composition comprising a first ethylene-based polymer having a peak melting temperature TE1. A film composed of a second composition comprising a second ethylene-based polymer having a melt index≤10 g/10 min and a peak melting temperature TE2 is applied to the surface of the rubber substrate to form a rubber substrate/film configuration. A compression force is applied at a temperature Tv (38° C.≤TE2<Tv) to form a vulcanized rubber/film laminate. The foam structure is applied to a surface of the film of the vulcanized rubber/film laminate to form a vulcanized rubber-film laminate/foam configuration. A compression force is applied at a temperature TL, wherein TE2<TL<TE1, 15° C.≤(TE1−TL)≤40° C., and 10° C.≤(TL−TE2)≤70° C., to form a vulcanized rubber-film/foam laminate.

## Claims

### Claim 1

A process of adhering a foam structure to a rubber substrate, wherein the foam structure is formed from a first composition comprising a first ethylene-based polymer having a peak melting temperature TE1, the process comprising the following steps:
a) applying a film formed from a second composition comprising a second ethylene-based polymer to a surface of the rubber substrate to form a rubber substrate/film configuration, wherein the second ethylene-based polymer has a melt index of less than or equal to 10 g/10 min and a peak melting temperature TE2;
b) applying a compression force to the rubber substrate/film configuration at a temperature Tv, wherein 38° C.≤TE2<Tv to form a vulcanized rubber/film laminate having an exposed surface of the film;
c) applying the foam structure to the exposed surface of the film to form a vulcanized rubber-film laminate/foam configuration; and
d) applying a compression force to the vulcanized rubber-film laminate/foam configuration at a temperature TL, wherein TE2<TL<TE1, 15° C.≤(TE1−TL)≤40° C., and 10° C.≤(TL−TE2)≤70° C. to form a vulcanized rubber-film/foam laminate.

### Claim 2 (depends on 1)

The process of claim 1, wherein the second ethylene-based polymer has a tensile strength of greater than or equal to 3 MPa.

### Claim 3 (depends on 2)

The process of claim 2, wherein the second ethylene-based polymer is an ethylene/alpha-olefin interpolymer.

### Claim 4 (depends on 3)

The process of claim 3, wherein the second ethylene-based polymer has a density from 0.860 g/cm3 to 0.885 g/cm3 and a melt index from 1.0 g/10 min to 5.0 g/10 min.

### Claim 5 (depends on 4)

The process of claim 4, wherein the first ethylene-based polymer is an ethylene/alpha-olefin multi-block copolymer.

### Claim 6 (depends on 5)

The process of claim 5, wherein the first ethylene-based polymer has a melt index 0.5 g/10 min to 5.0 g/10 min.

### Claim 7 (depends on 6)

The process of claim 6, wherein the first composition comprises from 85 wt % to 95 wt % of the first ethylene-based polymer, based on the total weight of the first composition.

### Claim 8 (depends on 7)

The process of claim 7, wherein the second composition comprises 95 wt % to 100 wt % of the second ethylene-based polymer, based on the total weight of the second composition.

### Claim 9 (depends on 8)

The process of claim 8, wherein the second composition comprises the second ethylene-based polymer to the exclusion of all other polymers.

### Claim 10 (depends on 9)

The process of claim 9, wherein the vulcanized rubber-film/foam laminate has a bond strength greater than or equal to 3 N/mm.

### Claim 11 (depends on 10)

The process of claim 10, wherein the TL≤100° C.