# US 2022/0032494 A1 · Formaldehyde-free medium-high-density board capable of meeting deep facing requirements and method for manufacturing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0032494 A1
- Document ID: US20220032494A1
- Status: Published application
- Kind: A1
- Application number: 17/504,215
- Filed: 2021-10-18
- Published: 2022-02-03
- Earliest claimed: 2019-06-28
- Assignees: Beijing Forestry University; Power Dekor Group Co., Ltd.; Hunan Forestech New Materials Co., Ltd.
- Applicants: Beijing Forestry University; Power Dekor Group Co., Ltd.; Hunan Forestech New Materials Co., Ltd.
- Inventors: Runcang Sun; Tongqi Yuan; Xiaolong Chen; Supeng Wang; Yueying Chen; Xianpeng Zhou
- Web page: https://patentgrep.com/patent/US20220032494A1

## CPC

- B27N 3/002: {characterised by the type of binder (compositions of macromolecular compounds C08L)}
- B27N 1/00: Pretreatment of moulding material
- B27N 1/003: {for reducing formaldehyde gas emission}
- B27N 3/04: from fibres
- B27N 3/18: Auxiliary operations, e.g. preheating, humidifying, cutting-off
- B27N 7/00: After-treatment, e.g. reducing swelling or shrinkage, surfacing; Protecting the edges of boards against access of humidity
- C08G 18/302: {Water}
- C08G 18/7671: {containing only one alkylene bisphenyl group}
- C09J 175/04: Polyurethanes
- C09J 197/005: {Lignin}
- C08K 3/22: of metals
- C08K 5/21: Urea; Derivatives thereof, e.g. biuret
- C08K 5/34922: {Melamine; Derivatives thereof}
- B27N: MANUFACTURE BY DRY PROCESSES OF ARTICLES, WITH OR WITHOUT ORGANIC BINDING AGENTS, MADE FROM PARTICLES OR FIBRES CONSISTING OF WOOD OR OTHER LIGNOCELLULOSIC OR LIKE ORGANIC MATERIAL (containing cementitious material B28B; shaping of substances in a plastic state B29C; fibreboards made from fibrous suspensions D21J; drying F26B17/00)
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

The present invention relates to a formaldehyde-free medium-high-density board capable of meeting deep facing requirements, and a method for manufacturing same. The method includes: wood chipping, screening, cooking and softening, fiber separating, gluing, drying and sorting, paving, pre-pressing, hot pressing, cooling, sanding, and inspection and warehousing, where the gluing is two-step gluing, including: first performing gluing once by using a lignin adhesive, and then performing secondary gluing by using an MDI adhesive after waterproof treatment. According to the manufacturing method of the present invention, by using biomass adhesives and formaldehyde-free adhesives without adding additives such as a curing agent and an anti-mildew agent, formaldehyde pollution is eliminated from the source by using a two-step gluing method, so that production is formaldehyde-free, and the product is formaldehyde-free. Through the sequential control of the gluing process and the grasp of the gluing type and ratio, surface hardness of the product is improved, and the final product is capable of deep facing to reach 20 to 80 filaments.

## Claims

### Claim 1

A method for manufacturing a formaldehyde-free medium-high-density board capable of meeting deep facing requirements, comprising: wood chipping, screening, cooking and softening, fiber separating, gluing, drying and sorting, paving, pre-pressing, hot pressing, cooling, sanding, and inspection and warehousing, wherein the gluing is two-step gluing, comprising: first performing gluing once by using a lignin adhesive, and then performing secondary gluing by using an MDI adhesive after waterproof treatment.

### Claim 2 (depends on 1)

The method for manufacturing the formaldehyde-free medium-high-density board capable of meeting deep facing requirements according to claim 1, wherein before the hot pressing, surface spraying is added, and the surface spraying comprises: spraying free water on a surface of a slab after the pre-pressing, so that a water content of fiber of the slab is 8% to 12%.

### Claim 3 (depends on 1)

The method for manufacturing the formaldehyde-free medium-high-density board capable of meeting deep facing requirements according to claim 1, wherein the lignin adhesive comprises components with the following weight percentages:
lignin 20% to 45%;
sodium hydroxide 2.0% to 8.5%;
melamine 2% to 8%;
polyvinyl alcohol 0.2% to 1.0%;
urea 2% to 6%;
water 40% to 70%.

### Claim 4 (depends on 1, 2, 3)

The method for manufacturing the formaldehyde-free medium-high-density board capable of meeting deep facing requirements according to any one of claims 1 to 3, wherein a solid ocntent of the lignin adhesive is 30% to 60%, and an application amount of the lignin adhesive is 50 kg/m3 to 80 kg/m3.

### Claim 5 (depends on 1)

The method for manufacturing the formaldehyde-free medium-high-density board capable of meeting deep facing requirements according to claim 1, wherein waterproof treatment is to apply a waterproof agent on a surface of fiber on which the lignin adhesive is applied, the waterproof agent is paraffin wax, and an application amount of the paraffin wax is 4 kg/m3 to 6 kg/m3.

### Claim 6 (depends on 1)

The method for manufacturing the formaldehyde-free medium-high-density board capable of meeting deep facing requirements according to claim 1, wherein before the secondary gluing, a ratio of the MDI adhesive to water is adjusted to 1:1 to 1:3 based on an initial viscosity of the MDI adhesive, and an application amount of the MDI adhesive is 10 kg/m3 to 40 kg/m3.

### Claim 7 (depends on 1)

The method for manufacturing the formaldehyde-free medium-high-density board capable of meeting deep facing requirements according to claim 1, wherein a raw material of the wood is one or more of eucalyptus wood, cotton wood, pine wood, and mixed hard woods.

### Claim 8 (depends on 1)

The method for manufacturing the formaldehyde-free medium-high-density board capable of meeting deep facing requirements according to claim 1, wherein in the drying and sorting step, fiber is dried to a water content of 5% to 10%.

### Claim 9 (depends on 1, 2, 3, 4, 5, 6, 7, 8)

A formaldehyde-free medium-high-density board capable of meeting deep facing requirements, wherein the medium-high-density board is manufactured by using the method for manufacturing a formaldehyde-free medium-high-density board capable of meeting deep facing requirements according to any one of claims 1 to 8.

### Claim 10 (depends on 9)

The formaldehyde-free medium-high-density board capable of meeting deep facing requirements according to claim 9, wherein the formaldehyde-free medium-high-density board capable of meeting deep facing requirements is capable of implementing 20-80-filament deep facing.