# US 2022/0032399 A1 · Metal member and manufacturing method for metal member

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0032399 A1
- Document ID: US20220032399A1
- Status: Published application
- Kind: A1
- Application number: 17/343,924
- Filed: 2021-06-10
- Published: 2022-02-03
- Earliest claimed: 2020-08-03
- Assignees: Toyota Jidosha Kabushiki Kaisha
- Applicants: Toyota Jidosha Kabushiki Kaisha
- Inventors: Masahiro UCHIMURA; Hiromichi NAKATA; Masashi FURUKAWA
- Web page: https://patentgrep.com/patent/US20220032399A1

## CPC

- B23K 26/16: Removal of by-products, e.g. particles or vapours produced during treatment of a workpiece (by a fluid stream B23K26/142)
- B23K 26/3584: {Increasing rugosity, i.e. roughening}
- B23K 26/0622: by shaping pulses
- B23K 26/354: by melting
- H10W 70/042: {Etching}
- H10W 70/457: {of metallic layers on leadframes}
- B23K 2101/35: {Surface treated articles}
- B23K 2103/08: Non-ferrous metals or alloys
- B23K 2103/10: Aluminium or alloys thereof
- B23K 2103/12: Copper or alloys thereof
- B23K 2103/14: Titanium or alloys thereof
- H10W 74/00: Encapsulations, e.g. protective coatings
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A manufacturing method for a metal member includes irradiating a first region of a surface of the base material, the surface having at least any one of Cu, Al, Sn, Ti, and Fe, as a main component, with a laser beam to melt the first region; generating metal particles from a vapor or plasma of a metal released to a predetermined atmosphere by melting the surface of the base material in the first region, and depositing the metal particles in the first region; irradiating a second region adjacent to the first region with a laser beam to melt the second region; and generating metal particles from a vapor or plasma of a metal released to a predetermined atmosphere by melting the surface of the base material in the second region, and depositing the metal particles in each of the first region and the second region.

## Claims

### Claim 1

A manufacturing method for a metal member that includes a base material of which at least a surface is made of a material containing at least any one of Cu, Al, Sn, Ti, and Fe, as a main component, and an uneven portion having an uneven shape, which is formed on the surface of the base material, the manufacturing method comprising forming the uneven portion,
wherein forming the uneven portion includes;
irradiating a first region of the surface of the base material with a pulse-oscillating laser beam to melt the surface of the base material in the first region,
generating metal particles from a vapor or plasma of a metal released to a predetermined atmosphere by melting the surface of the base material in the first region, and depositing the metal particles in the first region,
irradiating a second region of the surface of the base material with the pulse-oscillating laser beam, the second region being adjacent to the first region, to melt the surface of the base material in the second region, and
generating metal particles from a vapor or plasma of a metal released to the predetermined atmosphere by melting the surface of the base material in the second region, and depositing the metal particles in each of the second region and the first region adjacent to the second region.

### Claim 2 (depends on 1)

The manufacturing method according to claim 1, wherein:
the base material has a thin metal film, on the surface, that is made of a material containing at least any one of Cu, Al, Sn, Ti, and Fe, as a main component; and
the uneven portion is formed on a surface of the thin metal film.

### Claim 3 (depends on 1)

The manufacturing method according to claim 1, wherein:
the base material is made of a material containing Al, as a main component; and
irradiation conditions of the laser beam include a peak output of 3 kW or more, a pulse width of 1 ns to 1,000 ns, a laser spot diameter of 200 μm or less, the laser spot diameter being a diameter of each of the first region and the second region, and a spot interval of equal to or smaller than the laser spot diameter, the spot interval being an interval between the first region and the second region.

### Claim 4 (depends on 1)

The manufacturing method according to claim 1, wherein:
the base material is made of a material containing Cu, as a main component; and
irradiation conditions of the laser beam include a peak output of 6 kW or more, a pulse width of 1 ns to 1,000 ns, a laser spot diameter of 200 μm or less, the laser spot diameter being a diameter of each of the first region and the second region, and a spot interval of equal to or smaller than the laser spot diameter, the spot interval being an interval between the first region and the second region.

### Claim 5 (depends on 1)

The manufacturing method according to claim 1, wherein:
the base material is made of a material containing Sn, as a main component; and
irradiation conditions of the laser beam include a peak output of 1 kW or more, a pulse width of 1 ns to 1,000 ns, a laser spot diameter of 250 μm or less, the laser spot diameter being a diameter of each of the first region and the second region, and a spot interval of equal to or smaller than the laser spot diameter, the spot interval being an interval between the first region and the second region.

### Claim 6 (depends on 1)

The manufacturing method according to claim 1, wherein:
the base material is made of a material containing Ti, as a main component; and
irradiation conditions of the laser beam include a peak output of 1 kW or more, a pulse width of 1 ns to 1,000 ns, a laser spot diameter of 250 μm or less, the laser spot diameter being a diameter of each of the first region and the second region, and a spot interval of equal to or smaller than the laser spot diameter, the spot interval being an interval between the first region and the second region.

### Claim 7 (depends on 1)

The manufacturing method according to claim 1, wherein:
the base material is made of a material containing Fe, as a main component; and
irradiation conditions of the laser beam include a peak output of 1 kW or more, a pulse width of 1 ns to 1,000 ns, a laser spot diameter of 250 μm or less, the laser spot diameter being a diameter of each of the first region and the second region, and a spot interval of equal to or smaller than the laser spot diameter, the spot interval being an interval between the first region and the second region.

### Claim 8 (depends on 1)

The manufacturing method according to claim 1, further comprising:
partially densifying the uneven shape of the uneven portion, after forming the uneven portion,
wherein the partial densifying of the uneven shape of the uneven portion includes
irradiating a predetermined region of the uneven portion formed on the surface of the base material with a laser beam weaker than the laser beam that is used in forming the uneven portion, to melt a deposit that forms the uneven shape of the uneven portion in the predetermined region.

### Claim 9

A metal member comprising:
a base material of which at least a surface is made of a material containing at least any one of Cu, Al, Sn, Ti, and Fe, as a main component; and
an uneven portion having an uneven shape, which is formed on the surface of the base material,
wherein the uneven portion is made of deposited metal particles containing the material used in the surface of the base material, as a main component.

### Claim 10 (depends on 9)

The metal member according to claim 9, wherein:
the base material has a thin metal film, on the surface, that is made of a material containing at least any one of Cu, Al, Sn, Ti, and Fe, as a main component; and
the uneven portion is formed on a surface of the thin metal film.