# US 2022/0032374 A1 · Method of manufacturing aluminum alloy articles

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0032374 A1
- Document ID: US20220032374A1
- Status: Published application
- Kind: A1
- Application number: 17/501,054
- Filed: 2021-10-14
- Published: 2022-02-03
- Earliest claimed: 2017-05-26
- Assignees: Hamilton Sundstrand Corporation
- Applicants: Hamilton Sundstrand Corporation
- Inventors: Eric Karlen; William Louis Wentland; Sergey Mironets; Robert Bianco
- Web page: https://patentgrep.com/patent/US20220032374A1

## CPC

- B22F 10/28: Powder bed fusion, e.g. selective laser melting [SLM] or electron beam melting [EBM]
- B22F 9/04: starting from solid material, e.g. by crushing, grinding or milling ({C22C1/1084 takes precedence}; crushing, grinding or milling, in general, see the relevant subclasses, e.g. B02C)
- B22F 10/20: Direct sintering or melting
- B33Y 70/00: Materials specially adapted for additive manufacturing
- C22C 21/00: Alloys based on aluminium
- C22C 28/00: Alloys based on a metal not provided for in groups C22C5/00 - C22C27/00
- B22F 12/50: Means for feeding of material, e.g. heads
- B33Y 10/00: Processes of additive manufacturing
- Y02P 10/25: Process efficiency
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- B33Y: ADDITIVE MANUFACTURING, i.e. MANUFACTURING OF THREE-DIMENSIONAL [3D] OBJECTS BY ADDITIVE DEPOSITION, ADDITIVE AGGLOMERATION OR ADDITIVE LAYERING, e.g. BY 3D PRINTING, STEREOLITHOGRAPHY OR SELECTIVE LASER SINTERING
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method for making an article is disclosed. The method involves inputting a digital model of an article into an additive manufacturing apparatus comprising an energy source. The additive manufacturing apparatus applies energy from the energy source to successively applied incremental quantities of a powder to fuse the powder to form the article corresponding to the digital model. The powder includes an aluminum alloy having 2.00-10.00 wt. % cerium, 0.50-2.50 wt. % titanium, 0-3.00 wt. % nickel, 0-0.75 wt. % nitrogen, 0-0.05 wt. % other alloying elements, and the balance of aluminum, based on the total weight of the aluminum alloy.

## Claims

### Claim 1

An aluminum alloy comprising greater than 2.00 and less than 4.00 wt. % cerium, 0.50-2.50 wt. % titanium, 0-3.00 wt. % nickel, 0-0.75 wt. % nitrogen, 0-0.05 wt. % other alloying elements, and the balance of aluminum, based on the total weight of the aluminum alloy aluminum alloy.

### Claim 2 (depends on 1)

The aluminum alloy of claim 1, wherein the aluminum alloy comprises 0.50-1.50 wt. % titanium, based on the total weight of the aluminum alloy.

### Claim 3 (depends on 1)

The aluminum alloy of claim 1, wherein the aluminum alloy comprises 1.50-2.50 wt. % titanium, based on the total weight of the aluminum alloy.

### Claim 4 (depends on 1)

The aluminum alloy of claim 1, wherein the aluminum alloy comprises nickel in an amount up to 3.00 wt. %, based on the total weight of the aluminum alloy.

### Claim 5 (depends on 1)

The aluminum alloy of claim 1, wherein the aluminum alloy comprises 1.00-3.00 wt. % nickel, based on the total weight of the aluminum alloy.