# US 2022/0032262 A1 · Preparation method of bacterial cellulose-defective molybdenum disulfide heterojunction material for treating radioactive wastewater

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0032262 A1
- Document ID: US20220032262A1
- Status: Published application
- Kind: A1
- Application number: 17/190,407
- Filed: 2021-03-03
- Published: 2022-02-03
- Earliest claimed: 2020-07-31
- Assignees: Southwest University of Science and Technology
- Applicants: Southwest University of Science and Technology
- Inventors: Wenkun Zhu; Tao Chen; Rong He; Fan Yang; Yun Dong; Qian Wang; Bo Liu; Rong Wang
- Web page: https://patentgrep.com/patent/US20220032262A1

## CPC

- B01J 20/0266: {Compounds of S}
- B01J 20/0218: {Compounds of Cr, Mo, W}
- B01J 20/0285: {Sulfides of compounds other than those provided for in B01J20/045}
- B01J 20/20: comprising free carbon; comprising carbon obtained by carbonising processes
- B01J 20/3021: {Milling, crushing or grinding}
- B01J 20/3078: {Thermal treatment, e.g. calcining or pyrolizing}
- B01J 20/3085: {Chemical treatments not covered by groups B01J20/3007 - B01J20/3078}
- C02F 1/283: {using coal, charred products, or inorganic mixtures containing them}
- C02F 1/70: by reduction {(C02F1/4676 takes precedence)}
- C02F 1/30: by irradiation
- C02F 2101/006: {Radioactive compounds}
- C02F 2305/10: Photocatalysts
- G21F 9/12: by absorption; by adsorption; by ion-exchange
- Y02W 10/37: using solar energy
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C02F: TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE (separation in general B01D; special arrangements on waterborne vessels of installations for treating water, waste water or sewage, e.g. for producing fresh water, B63J; adding materials to water to prevent corrosion C23F; treating radioactively-contaminated liquids G21F9/04; regeneration of reactants for recirculation into processes, see the relevant places for the processes)
- G21F: PROTECTION AGAINST X-RADIATION, GAMMA RADIATION, CORPUSCULAR RADIATION OR PARTICLE BOMBARDMENT; TREATING RADIOACTIVELY CONTAMINATED MATERIAL; DECONTAMINATION ARRANGEMENTS THEREFOR (radiation protection by pharmaceutical means A61K8/00, A61Q17/04; in cosmonautic vehicles B64G1/54; combined with a reactor G21C11/00; combined with X-ray tubes H01J35/16; combined with X-ray apparatus H05G1/02)
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

A preparation method of a bacterial cellulose-defective molybdenum disulfide (BC-MoS2-x) heterojunction material for treating radioactive wastewater is provided, including: preparing bacterial cellulose by the in situ growth technology of Acetobacter xylinum, and freeze-drying to obtain dried bacterial cellulose; carbonizing the dried bacterial cellulose to obtain carbonized bacterial cellulose; dispersing the carbonized bacterial cellulose into deionized water under an ultrasonic treatment; then adding thiourea and Na2MoO4.2H2O, dissolving under an ultrasonic treatment to obtain a reaction mixture, subjecting the reaction mixture to a hydrothermal reaction to obtain a BC-MoS2 heterojunction; and calcining the BC-MoS2 heterojunction in a tube furnace with an Ar/H2 atmosphere to obtain the BC-MoS2-x heterojunction.

## Claims

### Claim 1

A preparation method of a bacterial cellulose-defective molybdenum disulfide (BC-MoS2-x) heterojunction material for treating radioactive wastewater, comprising the following steps:
step 1: preparing a liquid culture medium (per 150 mL) by dissolving and evenly mixing 5 wt % D-glucose, 0.5 wt % yeast extract, 0.2 wt % disodium hydrogen phosphate, 0.5 wt % peptone, 0.1 wt % citric acid, 0.1 wt % potassium dihydrogen phosphate and water, adjusting a pH value to 6.8, and performing a sterilization under a vapor pressure of 103.4 kPa and a temperature of 120-121.3° C. for 15-20 min; inoculating Acetobacter xylinum in the liquid culture medium and placing the liquid culture medium with the Acetobacter xylinum in a constant temperature incubator, incubating the Acetobacter xylinum in the liquid culture medium for 7 days at 293 K with a shaking speed of 120 rpm to obtain an Acetobacter xylinum-inoculated culture medium, and then rinsing the Acetobacter xylinum-inoculated culture medium to neutral with deionized water to obtain neutral Acetobacter xylinum; performing a freeze-drying on the neutral Acetobacter xylinum to obtain dried bacterial cellulose; wherein the Acetobacter xylinum is inoculated in the liquid culture medium according to a volume fraction of 3-8%;
step 2: placing the dried bacterial cellulose in a tube furnace with a nitrogen/argon protective atmosphere, and heating the dried bacterial cellulose to 750-850° C. at a rate of 5° C./min, and keeping the dried bacterial cellulose at 750-850° C. for 2-3 h to obtain carbonized bacterial cellulose;
step 3: dispersing the carbonized bacterial cellulose into deionized water under a first ultrasonic treatment to obtain dispersed carbonized bacterial cellulose; adding thiourea and Na2MoO4.2H2O to the dispersed carbonized bacterial cellulose for a dissolution under the first ultrasonic treatment to obtain a first reaction mixture, transferring the first reaction mixture into a Teflon-lined stainless steel autoclave, and conducting a first heat preservation on the first reaction mixture at 140-230° C. for 12 h; cooling the first reaction mixture naturally to obtain a first cooled reaction mixture, and collecting a bacterial cellulose-MoS2 (BC-MoS2) heterojunction from the first cooled reaction mixture by a first centrifugation;
step 4: placing the BC-MoS2 heterojunction in a tube furnace with an Ar/H2 atmosphere, heating the BC-MoS2 heterojunction to 300° C. at a rate of 5-10° C./min, keeping the BC-MoS2 heterojunction at 300° C. for 0-200 min, and cooling the BC-MoS2 heterojunction naturally to obtain the BC-MoS2-x heterojunction, wherein 0≤X<2.

### Claim 2 (depends on 1)

The preparation method of the BC-MoS2-x heterojunction material for treating the radioactive wastewater according to claim 1, wherein in step 3, a mass ratio of the carbonized bacterial cellulose to the deionized water is 1:600-800, a mass ratio of the carbonized bacterial cellulose to the thiourea is 1:0.3-0.4, and a mass ratio of the thiourea to the Na2MoO4.2H2O is 1:14-17.

### Claim 3 (depends on 1)

The preparation method of the BC-MoS2-x heterojunction material for treating the radioactive wastewater according to claim 1, wherein in step 2, the carbonized bacterial cellulose is subjected to a pretreatment as follows: laying the carbonized bacterial cellulose on a bottom plate of a low-temperature plasma generator, wherein a thickness of the carbonized bacterial cellulose after being laid is 6-12 mm; adjusting a spacing between two plates of the low-temperature plasma generator to 25-65 mm; controlling an internal air pressure of the low-temperature plasma generator to 900-1,200 Pa, then introducing a gas into the low-temperature plasma generator; adjusting a working voltage and a current between the two plates of the low-temperature plasma generator to 50-220 V and 0.5-1.2 A, respectively, and treating the carbonized bacterial cellulose for 30-60 min to obtain pretreated carbonized bacterial cellulose.

### Claim 4 (depends on 3)

The preparation method of the BC-MoS2-x heterojunction material for treating the radioactive wastewater according to claim 3, wherein the gas is one selected from the group consisting of air, oxygen and carbon dioxide.

### Claim 5 (depends on 1)

The preparation method of the BC-MoS2-x heterojunction material for treating the radioactive wastewater according to claim 1, wherein step 3 is replaced by the following step: adding the carbonized bacterial cellulose into a ball mill, and adding the thiourea and the Na2MoO4.2H2O into the ball mill simultaneously to obtain a mixture; introducing liquid nitrogen into the ball mill to immerse the mixture in the liquid nitrogen, and keeping a liquid level of the liquid nitrogen stable; preforming a ball milling on the mixture after keeping a constant temperature for 15-30 min to obtain milled materials, wherein the constant temperature in the ball mill is −155° C. to −180° C.; placing the milled materials at 40-60° C. for 90-120 min; dispersing the milled materials into deionized water under a second ultrasonic treatment to obtain a second reaction mixture, transferring the second reaction mixture into the Teflon-lined stainless steel autoclave, and conducting a second heat preservation on the second reaction mixture at 140-230° C. for 12 h; cooling the second reaction mixture naturally to obtain a second cooled reaction mixture, and collecting the BC-MoS2 heterojunction from the second cooled reaction mixture by a second centrifugation.

### Claim 6 (depends on 5)

The preparation method of the BC-MoS2-x heterojunction material for treating the radioactive wastewater according to claim 5, wherein a time of the ball milling is 60-90 min, and a speed of the ball milling is 500-650 rpm.

### Claim 7 (depends on 5)

The preparation method of the BC-MoS2-x heterojunction material for treating the radioactive wastewater according to claim 5, wherein in step 3, a mass ratio of the carbonized bacterial cellulose to the deionized water is 1:600-800, a mass ratio of the carbonized bacterial cellulose to the thiourea is 1:0.3-0.4, and a mass ratio of the thiourea to the Na2MoO4.2H2O is 1:14-17.