# US 2022/0024810 A1 · Transparent tantalum oxide glass-ceramics and transparent aluminum tantalate glass-ceramics

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0024810 A1
- Document ID: US20220024810A1
- Status: Published application
- Kind: A1
- Application number: 17/494,996
- Filed: 2021-10-06
- Published: 2022-01-27
- Earliest claimed: 2018-02-14
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: Bruce Gardiner Aitken; Randall Eugene Youngman
- Web page: https://patentgrep.com/patent/US20220024810A1

## CPC

- C03C 3/097: containing phosphorus, niobium or tantalum
- C03C 10/0009: {containing silica as main constituent}
- C03C 3/062: with less than 40% silica by weight
- C03C 3/064: containing boron
- C03C 10/0054: {containing PbO, SnO2, B2O3}
- C03C 2204/00: Glasses, glazes or enamels with special properties
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

A transparent glass-ceramic composition including: of the formula Ta2-xAlxO5-x where x is less than 1; of the formula AlTaO4; of the formula AlPO4; a mixture of AlTaO4 and AlPO4; or a mixture of the formula Ta2-xAlxO5-x, AlTaO4, and AlPO4. Also disclosed are transparent glass-ceramic compositions including, for example, a dopant as defined herein, or a supplemental metal oxide or metalloid oxide of MxOy, MxM′xOy, or a mixture thereof such as oxides of Nb, Ti, W, B, or Ga, as defined herein. Also disclosed are methods of making the disclosed transparent glass-ceramic compositions, and optical articles, optical components, and optical apparatus thereof.

## Claims

### Claim 1

A method of making a transparent glass-ceramic composition, comprising:
ceramming a suitable precursor glass composition at a temperature in a range of 900 to 1100° C. for a time in a range of 0.5 to 10 hrs.

### Claim 2 (depends on 1)

The method of making the transparent glass-ceramic composition of claim 1, wherein the suitable precursor glass composition comprises:
5 to 15% Ta2O5,
10 to 25% Al2O3,
3 to 10% P2O5, and
65 to 75% SiO2 based on a 100 mol % total.

### Claim 3 (depends on 1)

The method of making the transparent glass-ceramic composition of claim 1, further comprising:
including a dopant in an amount of 1 mol % or less based on the 100 mol % of the suitable precursor glass composition, and the dopant is selected from the group of a Cr oxide, a Ni oxide, a Co oxide, a rare earth oxide, or a mixture thereof.

### Claim 4 (depends on 1)

The method of making the transparent glass-ceramic composition of claim 1, wherein the dopant is an oxide selected from Cr, Ni, Co, V, Mn, Cu, Er, or a mixture thereof.

### Claim 5 (depends on 1)

The method of making the transparent glass-ceramic composition of claim 1, wherein the ceramming is conducted at a temperature in a range of 900 to 950° C. for a time in a range of 1 to 4 hrs.

### Claim 6 (depends on 1)

The method of making the transparent glass-ceramic composition of claim 1, wherein the transparent glass-ceramic comprises a formula of Ta2-xAlxO5-x, where x is less than 1 and greater than 0.001.

### Claim 7 (depends on 1)

The method of making the transparent glass-ceramic composition of claim 1, wherein the transparent glass-ceramic comprises a formula of a mixture of AlTaO4 and AlPO4.

### Claim 8 (depends on 1)

The method of making the transparent glass-ceramic composition of claim 1, further comprising including a dopant in an amount of 1 mol % or less based on the 100 mol % total of the suitable precursor glass composition, and the dopant is selected from the group of a Cr oxide, a Ni oxide, a Co oxide, a rare earth oxide, a V oxide, a Mn oxide, a Cu oxide, an Er oxide, or mixtures thereof.