Sealant glass composition and solid oxide fuel cell using same
AssigneeLG Electronics Inc.
InventorsNamjin KIM, Young Seok KIM, Sanghyeok IM
Life of this patent
Estimating the term…
Abstract
The present invention relates to a glass composition capable of being used as a sealant, and a solid oxide fuel cell using same. The sealant glass composition according to the present invention comprises 10-45 wt % of SiO2, 0.1-20 wt % of B2O3, 40-65 wt % of BaO, 0.1-20 wt % of CaO, and 0.1-15 wt % of at least one of Al2O3 and ZrO2, and unlike existing sealant glass compositions, can be suitably used in solid oxide fuel cells operating at intermediate temperatures, and exhibits an advantageous effect in keeping a decrease in sealing adhesion strength to a minimum, even after prolonged use.
Claims17
A sealing glass composition, comprising:
- 10 to 45% by weight of SiO2,
- 0.1 to 20% by weight of B2O3,
- 40 to 65% by weight of BaO,
- 0.1 to 20% by weight of CaO, and
- 0.1 to 15% by weight of at least one of SrO, Al2O3, or ZrO2.
(canceled)
Dependencies are inferred from the claim text.