# US 2022/0024808 A1 · Lead-free glass paste, chip resistor and method for producing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0024808 A1
- Document ID: US20220024808A1
- Status: Published application
- Kind: A1
- Application number: 17/487,666
- Filed: 2021-09-28
- Published: 2022-01-27
- Earliest claimed: 2020-07-22
- Assignees: Changxin Memory Technologies, Inc.
- Applicants: Changxin Memory Technologies, Inc.
- Inventors: Hongkun SHEN
- Web page: https://patentgrep.com/patent/US20220024808A1

## CPC

- C03C 8/16: with vehicle or suspending agents, e.g. slip
- C03C 8/02: Frit compositions, i.e. in a powdered or comminuted form
- C03C 14/004: {the non-glass component being in the form of particles or flakes}
- C09D 7/61: inorganic
- C09D 185/04: containing boron
- H01C 1/01: Mounting; Supporting
- H01C 1/02: Housing; Enclosing; Embedding; Filling the housing or enclosure
- H01C 1/028: the resistive element being embedded in insulation with outer enclosing sheath
- H01C 1/14: Terminals or tapping points specially adapted for resistors; Arrangements of terminals or tapping points on resistors
- H01C 7/003: {Thick film resistors}
- H01C 17/006: {adapted for manufacturing resistor chips}
- H01C 17/02: adapted for manufacturing resistors with envelope or housing (apparatus or processes for filling or compressing insulating material in heating element tubes H05B3/52)
- H01C 17/065: by thick film techniques, e.g. serigraphy
- H01C 17/28: adapted for applying terminals
- H01C 17/283: {Precursor compositions therefor, e.g. pastes, inks, glass frits}
- C03C 2204/00: Glasses, glazes or enamels with special properties
- C03C 2205/00: Compositions applicable for the manufacture of vitreous enamels or glazes
- C03C 2214/04: Particles; Flakes
- H01C 17/281: {by thick film techniques}
- Y02E 10/50: Photovoltaic [PV] energy
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- H01C: RESISTORS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A lead-free glass paste, a chip resistor and a method for producing the same are provided. The lead-free glass paste includes 6-7 parts by mass of borosilicate oil, 12-21 parts by mass of aluminum oxide powder, 2-3 parts by mass of glass fiber powder, and 0.1-0.5 parts by mass of a curing agent.

## Claims

### Claim 1

A lead-free glass paste, comprising 6-7 parts by mass of borosilicate oil, 12-21 parts by mass of aluminum oxide powder, 2-3 parts by mass of glass fiber powder, and 0.1-0.5 parts by mass of a curing agent.

### Claim 2 (depends on 1)

The lead-free glass paste of claim 1, wherein the borosilicate oil comprises 100-115 parts by mass of a phenyl-containing silicon substance, 13-28 parts by mass of a boron-containing monomer, 50-75 parts by mass of silane, and 60-80 parts by mass of dihydroxypyridine.

### Claim 3 (depends on 2)

The lead-free glass paste of claim 2, wherein the phenyl-containing silicon substance comprises at least one of ethoxydiphenylsilane, diphenyldimethoxysilane or diphenylsilanediol; the silane comprises at least one of dichlorodimethylsilane, dichlorodiethylsilane or dichlorodiphenylsilane; the dihydroxypyridine comprises at least one of 2,4-dihydroxypyridine, 2,6-dihydroxypyridine or 3,5-dihydroxypyridine; the boron-containing monomer comprises at least one of boric acid, phenylboronic acid, tri-isopropyl borate or dichlorophenylborane.

### Claim 4 (depends on 1)

The lead-free glass paste of claim 1, wherein the aluminum oxide powder comprises at least one of nanoscale aluminum oxide powder, gas-phase aluminum oxide powder or α-type nanoscale aluminum oxide powder.

### Claim 5 (depends on 1)

The lead-free glass paste of claim 1, wherein the glass fiber powder comprises at least one of alkali-free glass fiber powder, alkali-resistant glass fiber powder, high-alkali glass fiber powder or medium-alkali glass fiber powder.

### Claim 6 (depends on 1)

The lead-free glass paste of claim 1, wherein the curing agent comprises at least one of tetramethoxysilane (TMO), 2,5-dimethyl-2,5-di(tert-butylperoxy)hexane (DBPH), dibutyltin dilaurate, dibutyltin diacetate, or dicumyl peroxide (DCP).

### Claim 7 (depends on 1)

The lead-free glass paste of claim 1, wherein the lead-free glass paste is represented by the chemical structural formula below:
wherein x:y=1.1-1.9:0.3-0.7; R1 is phenyl, hydroxyl, or ethanol; R2 is methyl, ethyl, or phenyl; and R3 is dihydroxypyridine.

### Claim 8 (depends on 1)

A method for producing the lead-free glass paste of claim 1, comprising:
preparing the borosilicate oil;
uniformly mixing the borosilicate oil with the aluminum oxide powder and the glass fiber powder to obtain a mixture; and
adding the curing agent to the mixture to undergo a curing reaction, and then crushing to obtain the lead-free glass paste.

### Claim 9 (depends on 8)

The method for producing a lead-free glass paste of claim 8, wherein preparing the borosilicate oil comprises:
weighing a phenyl-containing silicon substance and a boron-containing monomer, adding the weighed phenyl-containing silicon substance and boron-containing monomer to a first solvent, stirring for uniformity to undergo a reaction, and then removing the first solvent to obtain a first product;
weighing silane and dihydroxypyridine, adding the weighed silane and dihydroxypyridine to a second solvent, stirring for uniformity to undergo a reaction, and then removing the second solvent to obtain a second product; and
weighing the first product and the second product, adding the weighed first product and second product to a third solvent, and stirring for uniformity to undergo a reaction to obtain the borosilicate oil.

### Claim 10 (depends on 9)

The method for producing a lead-free glass paste of claim 9, wherein a mass of the weighed phenyl-containing silicon substance is 100 g to 115 g, a mass of the weighed boron-containing monomer is 13 g to 28 g, a volume of the first solvent is 150 ml to 250 ml, and the first solvent comprises a dichloroethane solvent; a mass of the weighed silane is 50 g to 75 g, a mass of the weighed dihydroxypyridine is 60 g to 80 g, a volume of the second solvent is 350 ml to 450 ml, and the second solvent comprises propyl acetate; and the weighed first product is 1 to 1.1 parts by mass, the weighed second product is 0.95 to 1 parts by mass, a volume of the third solvent is 95 ml to 150 ml, and the third solvent comprises acetone.

### Claim 11 (depends on 9)

The method for producing a lead-free glass paste of claim 9, wherein in a process of obtaining the first product, a reaction temperature is 50° C. to 75° C., and a reaction time is 2.5 h to 3.5 h; in a process of obtaining the second product, a reaction temperature is 60° C. to 90° C., and a reaction time is 1.5 h to 2.5 h; and in a process of obtaining the borosilicate oil, a reaction temperature is 35° C. to 45° C. and a reaction time is 5.5 h to 6.5 h.

### Claim 12 (depends on 8)

The method for producing a lead-free glass paste of claim 8, wherein a temperature of the curing reaction is 26° C. to 45° C. and a time for the curing reaction is 5 h to 7 h.

### Claim 13 (depends on 1)

A chip resistor, comprising:
a substrate;
a backside electrode, located on a lower surface of the substrate;
a topside electrode, having one end in contact with the backside electrode, another end extending from a side wall of the substrate to an upper surface of the substrate;
a barrier layer, located on a surface of the topside electrode away from the substrate;
an external electrode, located on a surface of the barrier layer away from the topside electrode;
a resistive layer, located on the upper surface of the substrate and located on a side of the topside electrode;
a first protective layer, located on an upper surface of the resistive layer, wherein the first protective layer is prepared by the lead-free glass paste of claim 1; and
a second protective layer, located on an upper surface of the first protective layer.

### Claim 14 (depends on 2, 13)

The chip resistor of claim 13, wherein the first protective layer is prepared by the lead-free glass paste of claim 2.

### Claim 15 (depends on 7, 13)

The chip resistor of claim 13, wherein the first protective layer is prepared by the lead-free glass paste of claim 7.

### Claim 16 (depends on 8)

A method for producing a chip resistor, comprising:
providing a substrate;
forming a backside electrode on a lower surface of the substrate;
forming a topside electrode, a barrier layer and an external electrode, wherein one end of the topside electrode is in contact with the backside electrode, and another end extends from a side wall of the substrate to an upper surface of the substrate; the barrier layer is located on a surface of the topside electrode away from the substrate; and the external electrode is located on a surface of the barrier layer away from the topside electrode;
forming a resistive layer on the upper surface of the substrate, wherein the resistive layer is located on a side of the topside electrode;
preparing a lead-free glass paste by the method for producing a lead-free glass paste of claim 8;
coating an upper surface of the resistive layer with the lead-free glass paste to form a first protective layer; and
forming a second protective layer on an upper surface of the first protective layer.

### Claim 17 (depends on 9, 16)

The method for producing a chip resistor of claim 16, wherein the lead-free glass paste is prepared by the method for producing a lead-free glass paste of claim 9.

### Claim 18 (depends on 11, 17)

The method for producing a chip resistor of claim 17, wherein the lead-free glass paste is prepared by the method for producing a lead-free glass paste of claim 11.