# US 2022/0024802 A1 · Crystallized glass substrate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0024802 A1
- Document ID: US20220024802A1
- Status: Published application
- Kind: A1
- Application number: 17/296,983
- Filed: 2018-12-21
- Published: 2022-01-27
- Earliest claimed: 2018-12-21
- Assignees: Ohara Inc.
- Applicants: Ohara Inc.
- Inventors: TOSHITAKA YAGI; KOHEI OGASAWARA
- Web page: https://patentgrep.com/patent/US20220024802A1

## CPC

- C03C 3/087: containing calcium oxide, e.g. common sheet or container glass
- C03C 10/0018: {containing SiO2, Al2O3 and monovalent metal oxide as main constituents}
- C03C 21/002: {to perform ion-exchange between alkali ions (C03C21/005 takes precedence)}
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

Provided is a crystallized glass substrate including a surface with a compressive stress layer, in which a gradient A of a surface compressive stress from an outermost surface to a depth of 6 μm in the compressive stress layer is 50.0 to 110.0 MPa/μm, a gradient B of a surface compressive stress from a depth of (a stress depth DOLzero—10 μm) to the stress depth DOLzero is 2.5 to 15.0 MPa/μm, where the stress depth DOLzero is a depth of the compressive stress layer at a surface compressive stress of 0 MPa, and a hardness of the outermost surface at an indentation depth of 20 nm is 7.50 to 9.50 GPa.

## Claims

### Claim 1

A crystallized glass substrate including a surface with a compressive stress layer, wherein a gradient A of a surface compressive stress from an outermost surface to a depth of 6 μm in the compressive stress layer is 50.0 to 110.0 MPa/μm,
a gradient B of a surface compressive stress from a depth of (a stress depth DOLzero—10 μm) to the stress depth DOLzero is 2.5 to 15.0 MPa/μm,
where the stress depth DOLzero is a depth of the compressive stress layer at a surface compressive stress of 0 MPa, and
a hardness of the outermost surface at an indentation depth of 20 nm is 7.50 to 9.50 GPa.

### Claim 2

A crystallized glass substrate including a surface with a compressive stress layer,
wherein a gradient A of a surface compressive stress from an outermost surface to a depth of 6 μm in the compressive stress layer is 50.0 to 110.0 MPa/μm,
a gradient B of a surface compressive stress from a depth of (a stress depth DOLzero—10 μm) to the stress depth DOLzero is 2.5 to 15.0 MPa/μm,
where the stress depth DOLzero is a depth of the compressive stress layer at a surface compressive stress of 0 MPa, and
a hardness of the outermost surface at an indentation depth of 100 nm is 8.00 to 9.50 GPa.

### Claim 3

A crystallized glass substrate including a surface with a compressive stress layer,
wherein a gradient A of a surface compressive stress from an outermost surface to a depth of 6 μm in the compressive stress layer is 50.0 to 110.0 MPa/μm,
a gradient B of a surface compressive stress from a depth of (a stress depth DOLzero—10 μm) to the stress depth DOLzero is 2.5 to 15.0 MPa/μm,
where the stress depth DOLzero is a depth of the compressive stress layer at a surface compressive stress of 0 MPa, and
a surface compressive stress CS on the outermost surface of the compressive stress layer is 900.0 to 1200.0 MPa.

### Claim 4 (depends on 1)

The crystallized glass substrate according to claim 1, wherein the stress depth DOLzero is 30.0 to 70.0 μm,
a surface compressive stress CS on an outermost surface of the compressive stress layer is 870.0 to 1150.0 MPa, and
a central compressive stress CT is 35.0 to 70.0 MPa.

### Claim 5 (depends on 1)

The crystallized glass substrate according to claim 1, comprising:
by wt % in terms of oxide,
40.0% to 70.0% of a SiO2 component;
11.0% to 25.0% of an Al2O3 component;
5.0% to 19.0% of a Na2O component;
0% to 9.0% of a K2O component;
1.0% to 18.0% of one or more selected from a MgO component and a ZnO component;
0% to 3.0% of a CaO component; and
0.5% to 12.0% of a TiO2 component.

### Claim 6 (depends on 1)

The crystallized glass substrate according to claim 1, wherein a thickness of the crystallized glass substrate is 0.1 to 1.0 mm.

### Claim 7 (depends on 2)

The crystallized glass substrate according to claim 2, wherein the stress depth DOLzero is 30.0 to 70.0 μm,
a surface compressive stress CS on an outermost surface of the compressive stress layer is 870.0 to 1150.0 MPa, and
a central compressive stress CT is 35.0 to 70.0 MPa.

### Claim 8 (depends on 2)

The crystallized glass substrate according to claim 2, comprising:
by wt % in terms of oxide,
40.0% to 70.0% of a SiO2 component;
11.0% to 25.0% of an Al2O3 component;
5.0% to 19.0% of a Na2O component;
0% to 9.0% of a K2O component;
1.0% to 18.0% of one or more selected from a MgO component and a ZnO component;
0% to 3.0% of a CaO component; and
0.5% to 12.0% of a TiO2 component.

### Claim 9 (depends on 3)

The crystallized glass substrate according to claim 3, comprising:
by wt % in terms of oxide,
40.0% to 70.0% of a SiO2 component;
11.0% to 25.0% of an Al2O3 component;
5.0% to 19.0% of a Na2O component;
0% to 9.0% of a K2O component;
1.0% to 18.0% of one or more selected from a MgO component and a ZnO component;
0% to 3.0% of a CaO component; and
0.5% to 12.0% of a TiO2 component.

### Claim 10 (depends on 4)

The crystallized glass substrate according to claim 4, comprising:
by wt % in terms of oxide,
40.0% to 70.0% of a SiO2 component;
11.0% to 25.0% of an Al2O3 component;
5.0% to 19.0% of a Na2O component;
0% to 9.0% of a K2O component;
1.0% to 18.0% of one or more selected from a MgO component and a ZnO component;
0% to 3.0% of a CaO component; and
0.5% to 12.0% of a TiO2 component.

### Claim 11 (depends on 2)

The crystallized glass substrate according to claim 2, wherein a thickness of the crystallized glass substrate is 0.1 to 1.0 mm.

### Claim 12 (depends on 3)

The crystallized glass substrate according to claim 3, wherein a thickness of the crystallized glass substrate is 0.1 to 1.0 mm.

### Claim 13 (depends on 4)

The crystallized glass substrate according to claim 4, wherein a thickness of the crystallized glass substrate is 0.1 to 1.0 mm.

### Claim 14 (depends on 5)

The crystallized glass substrate according to claim 5, wherein a thickness of the crystallized glass substrate is 0.1 to 1.0 mm.