Ammoxidation catalyst for propylene, manufacturing method of the same catalyst, ammoxidation method using the same catalyst
AssigneeLG Chem, Ltd.
InventorsKyungyeon Kang, Ji Yeon Kim, Jun Seon Choi
Life of this patent
Estimating the term…
Abstract
There are provided an ammoxidation catalyst for propylene, a manufacturing method of the same, and an ammoxidation method of propylene using the same. Specifically, according to one embodiment of the invention, a catalyst is realized with a structure in which metal oxide is supported on a silica carrier, and thus, using mesopores useful for adsorption and desorption of gas, a high reaction surface area can be provided, and ultimately, ammoxidation of propylene can be increased.
Claims20
An ammoxidation catalyst for propylene in which metal oxide represented by Chemical Formula 1 is supported on a silica carrier,
- wherein the catalyst comprises pores having a diameter of 5 to 200 nm and a volume of 0.1 to 3.0 cm3/g, and
- has BET specific surface area of 50 m2/g to 1000 m2/g:
- Mo12BiaFebAcBdCeOx [Chemical Formula 1]
- in Chemical Formula 1,
- A is one or more elements of Ni, Mn, Co, Zn, Mg, Ca, and Ba,
- B is one or more elements of Li, Na, K, Rb, and Cs,
- C is one or more elements of Cr, W, B, Al, Ca, and V, and
- a to e, and x are respectively fractions of each atom or atomic group, wherein a is 0.1 to 5, b is 0.1 to 5, c is 0.01 to 10, d is 0.01 to 2, e is 0 to 10, and x is 24 to 48.
A method for preparing an ammoxidation catalyst for propylene comprising:
- preparing a first precursor solution comprising a Mo precursor,
- preparing a second precursor solution comprising a Bi precursor, a Fe precursor, an A precursor, wherein A is one or more elements of Ni, Mn, Co, Zn, Mg, Ca, and Ba, and a B precursor, wherein B is one or more elements of Li, Na, K, Rb, and Cs, or a second precursor solution comprising a Bi precursor, a Fe precursor, an A precursor, wherein A is one or more elements of Ni, Mn, Co, Zn, Mg, Ca, and Ba, a B precursor, wherein B is one or more elements of Li, Na, K, Rb, and Cs, and a C precursor, wherein C is one or more elements of Cr, W, B, Al, Ca, and V,
- mixing the first and second precursor solutions such that a molar ratio of metals satisfies stoichiometric molar ratio of Chemical Formula 1,
- supporting the mixture of the first and second precursor solutions on a silica carrier,
- drying the silica carrier in which the mixture of the first and second precursor solutions is supported, and
- calcining the dried material:
- Mo12BiaFebAcBdCeOx [Chemical Formula 1]
- in the Chemical Formula 1,
- A is one or more elements of Ni, Mn, Co, Zn, Mg, Ca, and Ba,
- B is one or more elements of Li, Na, K, Rb, and Cs,
- C is one or more elements of Cr, W, B, Al, Ca, and V, and
- a to e, and x are respectively fractions of each atom or atomic group, wherein a is 0.1 to 5, b is 0.1 to 5, c is 0.01 to 10, d is 0.01 to 2, e is 0 to 10, and x is 24 to 48.
Dependencies are inferred from the claim text.