# US 2022/0018400 A1 · Wet friction plate, wet multi-plate clutch device provided with same wet friction plate, and method for manufacturing wet friction plate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0018400 A1
- Document ID: US20220018400A1
- Status: Published application
- Kind: A1
- Application number: 17/294,598
- Filed: 2019-11-01
- Published: 2022-01-20
- Earliest claimed: 2018-11-28
- Assignees: Kabushiki Kaisha F.C.C.
- Applicants: Kabushiki Kaisha F.C.C.
- Inventors: Kenichiro SEKI; Kazuhiro ICHIHARA; Akihiro YAMASHITA; Koji MIYOSHI
- Web page: https://patentgrep.com/patent/US20220018400A1

## CPC

- F16D 13/56: in which the clutching pressure is produced by springs only
- F16D 13/648: {for clutches with multiple lamellae}
- F16D 13/52: Clutches with multiple lamellae {; Clutches in which three or more axially moveable members are fixed alternately to the shafts to be coupled and are pressed from one side towards an axially-located member (F16D13/385 takes precedence)}
- F16D 2200/006: containing fibres or particles
- F16D: COUPLINGS FOR TRANSMITTING ROTATION; CLUTCHES; BRAKES

## Abstract

Provided are a wet friction plate configured so that drag torque can be reduced while a manufacturing burden is reduced with a simple configuration, a wet multiplate clutch device including the wet friction plates, and a wet friction plate manufacturing method. A wet friction plate (200) includes friction members (210) provided on a flat plate annular core metal (201), having oil grooves (203), and made of a paper material. The friction members (210) include higher friction members (211) and lower friction members (212). The higher friction member (211) is formed such that the height thereof from a surface of the core metal (201) is higher than that of the lower friction member (212). In addition, the higher friction member (211) is formed with a less-elastically-deformable structure than that of the lower friction member (212). The lower friction member (212) is formed such that the height thereof from the surface of the core metal (201) is lower than that of the higher friction member (211). In addition, the lower friction member (212) is formed with a more-elastically-deformable structure than that of the higher friction member (211). The higher friction members (211) and the lower friction members (212) are alternately arranged along a circumferential direction on the core metal (201).

## Claims

### Claim 1

A wet friction plate comprising:
multiple friction members arranged on a surface of a core metal, which is formed in a flat plate annular shape, along a circumferential direction through a clearance,
wherein the friction members include two types of higher friction member and lower friction member having elasticity in a thickness direction and having relatively-different heights from the surface of the core metal, and
the higher friction member is formed less elastically deformable in the thickness direction than the lower friction member.

### Claim 2 (depends on 1)

The wet friction plate according to claim 1, wherein
the higher friction member is formed higher by an amount of equal to or higher than 1% and equal to or lower than 25% of a thickness of the lower friction member.

### Claim 3 (depends on 1, 2)

The wet friction plate according to claim 1 or 2, wherein
each friction member includes a paper body containing a papermaking fiber, and
the higher friction member is formed with a higher density than that of the lower friction member, and accordingly, is formed less elastically deformable in the thickness direction than the lower friction member.

### Claim 4 (depends on 1, 2, 3)

The wet friction plate according to any one of claims 1 to 3, wherein
the higher friction member has a. lower area ratio than that of the lower friction member.

### Claim 5 (depends on 1, 2, 3, 4)

The wet friction plate according to any one of claims 1 to 4, wherein
the lower friction member is formed such that an area thereof expands from an inside to an outside in a radial direction of the core metal.

### Claim 6 (depends on 1, 2, 3, 4, 5)

A wet multiplate clutch device comprising:
multiple wet friction plates according to any one of claims 1 to 5;
multiple flat plate annular separator plates to be pressed against the multiple wet friction plates or to be separated from the multiple wet friction plates; and
clutch oil to be supplied to each of clearances among the wet friction plates and the separator plates.

### Claim 7 (depends on 6)

The wet multiplate clutch device according to claim 6, wherein
the multiple wet friction plates are arranged at positions shifted in the circumferential direction of the core metal such that positions of the higher friction members in the circumferential direction do not overlap with each other and positions of the lower friction members in the circumferential direction do not overlap with each other between adjacent ones of the wet friction plates through the separator plate.

### Claim 8

A method for manufacturing a wet friction plate including multiple friction members arranged on a surface of a core metal, which is formed in a flat plate annular shape, along a circumferential direction through a clearance, comprising:
a core metal preparation step of preparing the core metal;
a pre-friction member preparation step of preparing a pre-higher friction member and a pre-lower friction member including two paper bodies made of papermaking fibers and haying different thicknesses and formed as a higher friction member and a lower friction member;
a pre-friction member arrangement step of arranging the pre--higher friction member and the pre-lower friction member on the surface of the core metal; and
a friction member formation step of pressing the pre-higher friction member and the pre-lower friction member arranged on the core metal to compress and deform the pre-higher friction member and the pre-lower friction member to form the higher friction member and the lower friction member having different thicknesses, the higher friction member being less elastically deformable in a thickness direction than the lower friction member.

### Claim 9 (depends on 8)

The wet friction plate manufacturing method according to claim 8, wherein
at the pre-friction member preparation step, the pre-higher friction member and the pre-lower friction member are arranged on each surface of the core metal, and
at the friction member formation step, the pre-higher friction member and the pre-lower friction member arranged on each surface of the core metal are simultaneously pressed from both sides and are compressed and deformed.

### Claim 10 (depends on 9)

The wet friction plate manufacturing method according to claim 9, wherein
at the pre-friction member preparation step, the pre-higher friction members are arranged at an identical position in the circumferential direction on both surfaces of the core metal, and the pre-lower friction members are arranged at an identical position in the circumferential direction on both surfaces of the core metal.