# US 2022/0017994 A1 · Hot-forged tial-based alloy, method for producing same, and uses for same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0017994 A1
- Document ID: US20220017994A1
- Status: Published application
- Kind: A1
- Application number: 17/311,866
- Filed: 2019-12-13
- Published: 2022-01-20
- Earliest claimed: 2018-12-21
- Assignees: National Institute for Materials Science
- Applicants: National Institute for Materials Science
- Inventors: Toshimitsu TETSUI
- Web page: https://patentgrep.com/patent/US20220017994A1

## CPC

- C22C 14/00: Alloys based on titanium
- B23P 15/02: turbine or like blades from one piece
- C22F 1/183: {of titanium or alloys based thereon}
- F01D 5/28: Selecting particular materials; {Particular measures relating thereto;} Measures against erosion or corrosion
- F02B 39/00: Component parts, details, or accessories relating to, driven charging or scavenging pumps, not provided for in groups F02B33/00 - F02B37/00
- F05D 2300/174: Titanium alloys, e.g. TiAl
- F05D 2300/608: Microstructure
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B23P: METAL-WORKING NOT OTHERWISE PROVIDED FOR; COMBINED OPERATIONS; UNIVERSAL MACHINE TOOLS (arrangements for copying or controlling B23Q)
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- F01D: NON-POSITIVE DISPLACEMENT MACHINES OR ENGINES, e.g. STEAM TURBINES (machines or engines for liquids F03; non-positive displacement pumps F04D)
- F02B: INTERNAL-COMBUSTION PISTON ENGINES; COMBUSTION ENGINES IN GENERAL (gas-turbine plants F02C; hot-gas or combustion-product positive-displacement engine plants F02G)
- F05D: INDEXING SCHEME FOR ASPECTS RELATING TO NON-POSITIVE-DISPLACEMENT MACHINES OR ENGINES, GAS-TURBINES OR JET-PROPULSION PLANTS

## Abstract

The present invention provides a TiAl-based alloy, including: Al: 41 to 43 at %; Fe: 0 to 2.5 at %; Ni: 0 to 2.5 at %; Mo: 0 to 2.0 at %; W: 0 to 2.0 at %; Cr: 0 to 4.5 at %; Mn: 0 to 5.5 at %; V: 0 to 10 at %; Nb: 0 to 10 at %; C: 0.3 to 0.7 at %; and a remainder consisting of Ti and inevitable impurities, in which an alloy element parameter “P=(41.5−Al)/3+Fe+Ni+Mo+W+0.5 Cr+0.4 Mn+0.2 V+0.2 Nb—C” is in a composition range of 1.1 to 1.9, and the TiAl-based alloy has a microstructure consisting of a γ phase of 5 to 30 area %, a β phase of 0.5 to 5 area %, and a lamellar structure occupying a remaining part.

## Claims

### Claim 1

A TiAl-based alloy, comprising:
Al: 41 to 43 at %;
Fe: 0 to 2.5 at %;
Ni: 0 to 2.5 at %;
Mo: 0 to 2.0 at %;
W: 0 to 2.0 at %;
Cr: 0 to 4.5 at %;
Mn: 0 to 5.5 at %;
V: 0 to 10 at %;
Nb: 0 to 10 at %;
C: 0.3 to 0.7 at %; and
a remainder consisting of Ti and inevitable impurities,
wherein an alloy element parameter P obtained by Equation (1) below is in a composition range of 1.1 to 1.9, and
the TiAl-based alloy has a microstructure consisting of a γ phase of 5 to 30 area %, a β phase of 0.5 to 5 area %, and a lamellar structure occupying a remaining part,
P=(41.5−Al)/3+Fe+Ni+Mo+W+0.5 Cr+0.4 Mn+0.2 V+0.2 Nb—C (1).

### Claim 2 (depends on 1)

The TiAl-based alloy according to claim 1, comprising:
Al: 41.2 to 42.8 at %;
Fe: 0 to 2.0 at %;
Ni: 0 to 2.0 at %;
Mo: 0 to 1.7 at %;
W: 0 to 1.7 at %;
Cr: 0 to 4.0 at %;
Mn: 0 to 5.0 at %;
V: 0 to 8 at %;
Nb: 0 to 8 at %;
C: 0.35 to 0.65 at %; and
a remainder consisting of Ti and inevitable impurities,
wherein the alloy element parameter P is in a composition range of 1.2 to 1.8, and
the TiAl-based alloy has a microstructure consisting of a γ phase of 7 to 25 area %, a β phase of 0.5 to 4.5 area %, and a lamellar structure occupying a remaining part.

### Claim 3 (depends on 1)

The TiAl-based alloy according to claim 1, comprising:
Al: 41.4 to 42.6 at %,
Fe: 0 to 1.5 at %;
Ni: 0 to 1.5 at %;
Mo: 0 to 1.5 at %;
W: 0 to 1.5 at %;
Cr: 0 to 3.5 at %;
Mn: 0 to 4.5 at %;
V: 0 to 6 at %;
Nb: 0 to 6 at %;
C: 0.4 to 0.6 at %; and
a remainder consisting of Ti and inevitable impurities,
wherein the alloy element parameter P is in a composition range of 1.3 to 1.7, and the TiAl-based alloy has a microstructure consisting of a γ phase of 10 to 20 area %, a β phase of 0.5 to 4 area %, and a lamellar structure occupying a remaining part.

### Claim 4 (depends on 1)

A method for producing a TiAl-based alloy, comprising:
a step of hot-forging a TiAl-based alloy base material that has the composition and the microstructure according to claim 1 as the temperature of the TiAl-based alloy base material is held in a coexistence temperature range of an α phase and a β phase; and
a step of holding a TiAl-based alloy material obtained by hot-forging in a temperature range of 1200 to 1250° C. for 0.5 to 5 hours and then heat treating the TiAl-based alloy material at a cooling rate of 1 to 10° C./min.

### Claim 5 (depends on 4)

The method for producing a TiAl-based alloy according to claim 4,
wherein in a cooling process in the step of heat treating the TiAl-based alloy material, a γ phase is precipitated from the β phase and an amount of the β phase is reduced.

### Claim 6 (depends on 1)

A blade for a turbine using a TiAl-based alloy material that has the composition and the microstructure according to claim 1.

### Claim 7 (depends on 6)

A gas turbine for power generation, a jet engine for an aircraft, a supercharger for a ship, or a gas turbine or a steam turbine for various industrial machines, which uses the blade for a turbine according to claim 6.