# US 2022/0017730 A1 · Polyolefin Compositions Suitable for Films

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0017730 A1
- Document ID: US20220017730A1
- Status: Published application
- Kind: A1
- Application number: 17/309,237
- Filed: 2019-11-11
- Published: 2022-01-20
- Earliest claimed: 2018-11-16
- Assignees: ExxonMobil Chemical Patents Inc.
- Applicants: ExxonMobil Chemical Patents Inc.
- Inventors: Sushanta DHAR ROY; Bradley A. KRAMER; Ying ZOU; Jasper HOLSBEEK; Stefan B. OHLSSON; Maciej M. PASNIEWSKI; Mosha H. ZHAO
- Web page: https://patentgrep.com/patent/US20220017730A1

## CPC

- B32B 27/18: characterised by the use of special additives
- C08L 23/06: Polyethylene
- B32B 27/08: of synthetic resin
- B32B 27/32: comprising polyolefins {(comprising vinyl (co)polymers or acrylic (co)polymers B32B27/30)}
- B32B 27/327: {comprising polyolefins obtained by a metallocene or single-site catalyst}
- C08J 5/18: Manufacture of films or sheets
- C08L 23/0815: {with aliphatic 1-olefins containing one carbon-to-carbon double bond}
- C08L 23/12: Polypropene
- B32B 2250/02: 2 layers
- B32B 2250/03: 3 layers
- B32B 2250/04: 4 layers
- B32B 2250/05: 5 or more layers
- B32B 2250/242: All polymers belonging to those covered by group B32B27/32
- B32B 2307/54: Yield strength; Tensile strength
- B32B 2307/546: Flexural strength; Flexion stiffness
- B32B 2307/558: Impact strength, toughness
- B32B 2307/5825: Tear resistant
- B32B 2307/72: Density
- B32B 2307/734: Dimensional stability
- B32B 2439/46: Bags
- B32B 2439/70: Food packaging
- C08L 2205/025: containing two or more polymers of the same hierarchy C08L, and differing only in parameters such as density, comonomer content, molecular weight, structure
- C08L 2205/03: containing three or more polymers in a blend
- C08L 2207/066: LDPE (radical process)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)

## Abstract

The present disclosure provides polyolefin compositions and films and method for producing such films. The polyolefin composition contains about 40 wt % to about 95 wt % of a BOCD polyethylene and about 10 wt % to about 60 wt % of a polypropylene, by weight of the polyolefin composition. The polyolefin composition has a 1% secant flexural modulus MID of greater than 250 MPa and a 1% secant flexural modulus TD of greater than 300 MPa, as determined for a layer of the polyolefin composition having a thickness of about 50 μm and a Dart Impact (Method A) of greater than 15 g/μm and an Elmendorf tear MI) of greater than 7 g/μm, as determined for a film containing the polyolefin composition and having a thickness of about 90 μm.

## Claims

### Claim 1

A polyolefin composition, comprising:
a) a broad orthogonal composition distribution (BOCD) polyethylene comprising about 70 mol % to about 100 mol % of ethylene and having:
i. a density of about 0.91 g/cm3 to about 0.925 g/cm3, in accordance with ASTM D-4703 and ASTM D-1505/ISO 1183; and
ii. a branching index (g′vis) of 0.98 or greater; and
b) a trimmed polypropylene (tPP) produced from a high melt strength polypropylene (HMS PP).

### Claim 2 (depends on 1)

The polyolefin composition of claim 1, wherein the polyolefin composition comprises about 40 wt % to about 95 wt %, by weight of the polyolefin composition, of the BOCD polyethylene; and about 5 wt % to about 60 wt %, by weight of the polyolefin composition of the polypropylene.

### Claim 3 (depends on 1)

The polyolefin composition of claim 1, comprising a 1% secant flexural modulus MD of about 300 MPa to about 1,200 MPa, as determined for a layer of the polyolefin composition having a thickness of about 50 μm.

### Claim 4

(canceled)

### Claim 5 (depends on 1)

The polyolefin composition according to claim 1, comprising a 1% secant flexural modulus TD of about 340 MPa to about 1,200 MPa, as determined for a layer of the polyolefin composition having a thickness of about 50 μm.

### Claim 6

(canceled)

### Claim 7 (depends on 1)

The polyolefin composition according to claim 1, having one or both of the following properties, as determined for a film comprising the polyolefin composition and having a thickness of about 90 μm: (i) Dart Impact (Method A) of about 16 g/μm to about 20 g/μm; and (ii) Elmendorf tear MD of greater than 13 g/μm.

### Claim at position 8

-9. (canceled)

### Claim 10 (depends on 1)

The polyolefin composition according to claim 1, wherein the BOCD polyethylene has an Mw1/Mw2 of about 1.5 to about 8 and a Tw1-Tw2 of about −5° C. to about −40° C.

### Claim at position 10

-14. (canceled)

### Claim 15 (depends on 1)

The polyolefin composition according to claim 1, wherein the polypropylene has one or more of the following properties:
(a) a molecular weight distribution (Mw/Mn) of about 7 to about 22;
(b) a z-average molecular weight of less than 2,500,000 g/mol;
(c) a branching index (g′vis) of 0.95 or greater; and
(d) a melt strength of less than 20 cN determined using an extensional rheometer at 190° C.

### Claim at position 12

-18. (canceled)

### Claim 19 (depends on 10)

The polyolefin composition according to claim 10, wherein the BOCD polyethylene has a density of about 0.912 g/cm3 to about 0.918 g/cm3, in accordance with ASTM D-4703 and ASTM D-1505/ISO 1183.

### Claim 20 (depends on 10)

The polyolefin composition according to claim 10, wherein the BOCD polyethylene has a density of about 0.915 g/cm3 to about 0.921 g/cm3, in accordance with ASTM D-4703 and ASTM D-1505/ISO 1183.

### Claim 21 (depends on 10)

The polyolefin composition according to claim 10, wherein the BOCD polyethylene has a branching index (g′vis) of about 0.985 to 1.0.

### Claim 22 (depends on 1)

The polyolefin composition of claim 1, further comprising a linear low-density polyethylene (LLDPE).

### Claim 23 (depends on 22)

The polyolefin composition of claim 22, wherein the LLDPE is in a concentration of about 10 wt % to about 40 wt %, by weight of the polyolefin composition.

### Claim 24 (depends on 22)

The polyolefin composition of claim 22, wherein the LLDPE comprises ethylene derived units and comonomers selected from C3 to C10 alpha-olefin derived units.

### Claim 25 (depends on 1)

A film comprising the polyolefin composition according to claim 1, having a thickness of about 10 μm to about 300 μm.

### Claim 26 (depends on 25)

The film of claim 25, wherein the film is a monolayer having a thickness of about 10 μm to about 100 μm.

### Claim 27 (depends on 26)

The film of claim 26, wherein the film comprises about 75 wt % to about 95 wt % of the BOCD polyethylene and about 5 wt % to about 25 wt % of the polypropylene, by weight of the polyolefin composition.

### Claim 28 (depends on 26)

The film of claim 26, wherein the film has an Elmendorf Tear MD of about 8 g/μm to about 10 g/μm and an Elmendorf Tear TD of about 13.5 g/μm to about 16 g/μm.

### Claim 29 (depends on 25)

The film of claim 25, wherein the film comprises a core layer disposed between two skin layers, and wherein the core layer comprises the polyolefin composition.

### Claim 30

(canceled)

### Claim 31 (depends on 29)

The film of claim 29, wherein one or two of the skin layers also comprise the polyolefin composition.

### Claim 32 (depends on 29)

The film of claim 29, further comprising a linear low-density polyethylene (LLDPE).

### Claim at position 27

-45. (canceled)