# US 2022/0017411 A1 · Method for manufacturing window

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0017411 A1
- Document ID: US20220017411A1
- Status: Published application
- Kind: A1
- Application number: 17/298,505
- Filed: 2019-04-23
- Published: 2022-01-20
- Earliest claimed: 2019-04-23
- Assignees: Samsung Display Co., Ltd.
- Applicants: Samsung Display Co., Ltd.
- Inventors: HOIKWAN LEE; MINKI KIM; BYEONG-BEOM KIM; SEUNGHO KIM; YURI KIM; JONGHOON YEUM
- Web page: https://patentgrep.com/patent/US20220017411A1

## CPC

- C03C 21/002: {to perform ion-exchange between alkali ions (C03C21/005 takes precedence)}
- C03C 3/083: containing aluminium oxide or an iron compound
- C03C 3/097: containing phosphorus, niobium or tantalum
- C03C 17/002: {for flat glass, e.g. float glass}
- C03C 2218/119: by printing
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

A method for manufacturing a window includes providing a base glass, and strengthening the base glass by exposing the base glass to a strengthening molten salt and an additive. The additive contains at least one of Al2(SO4)3, Al(NO3)3, K2SiO3, Na2SiO3, KCl, Ca(NO3)2, and Mg(NO3)2, and a window having good surface compressive stress and excellent surface chemical resistance may thus Ire provided.

## Claims

### Claim 1

A method for manufacturing a window, the method comprising the steps of:
providing a base glass; and
exposing the base glass to a mixed melt comprising a strengthening molten salt and an additive,
wherein the additive comprises Al2(SO4)3, Al(NO3)3, K2SiO3, Na2SiO3, KCl, Ca(NO3)2, and/or Mg(NO3)2.

### Claim 2 (depends on 1)

The method of claim 1, wherein the additive is included in the mixed melt an amount of 0 wt % to 10 wt % with respect to a total weight of the mixed melt.

### Claim 3 (depends on 1)

The method of claim 1, wherein the additive is Al2(SO4)3 or Al(NO3)3.

### Claim 4 (depends on 1)

The method of claim 1, wherein the base glass comprises SiO2, Al2O3, and Li2O3.

### Claim 5 (depends on 4)

The method of claim 4, wherein the base glass further comprises P2O5.

### Claim 6 (depends on 4)

The method of claim 4, wherein the base glass comprises:
SiO2 in an amount of 50 wt % to 80 wt %;
Al2O3 in an amount of 10 wt % to 30 wt %; and
Li2O3 in an amount of 3 wt % to 20 wt %.

### Claim 7 (depends on 1)

The method of claim 1, wherein the base glass comprises SiO2, Al2O3, and P2O5.

### Claim 8 (depends on 1)

The method of claim 1, wherein the strengthening molten salt is a mixed salt comprising two or more ions selected from the group consisting of Li+, Na+, K+, Rb+ and Cs+, or a single salt containing any one ion selected from the group consisting of Li+, Na+, K+, Rb+ and Cs+.

### Claim 9 (depends on 1)

The method of claim 1, wherein the step of exposing the base glass to the mixed melt comprises:
exposing the base glass to a first strengthening molten salt and the additive to strengthen the base glass; and
exposing the base glass to a second strengthening molten salt, without exposing the base glass to the additive, to further strengthen the base glass.

### Claim 10 (depends on 9)

The method of claim 9, wherein:
exposing the base glass to the first strengthening molten salt and the additive is performed at a first temperature; and
exposing the base glass to the second strengthening molten salt, without exposing the base glass to the additive, is performed at a second temperature that is lower than the first temperature.

### Claim 11 (depends on 9)

The method of claim 9, wherein:
exposing the base glass to the first strengthening molten salt and the additive is performed at a temperature within a range of 380° C. to 440° C.; and
exposing the base glass to the second strengthening molten salt, without exposing the base glass to the additive, is performed at a temperature within a range of 380° C. to 410° C.

### Claim 12 (depends on 9)

The method of claim 9, wherein:
the first strengthening molten salt comprises KNO3 and NaNO3; and
the second strengthening molten salt comprises KNO3.

### Claim 13 (depends on 1)

The method of claim 1, further comprising a step of forming a printing layer on an upper surface of the base glass and/or a lower surface of the base glass after having exposed the base glass to the mixed melt.

### Claim 14

A method for manufacturing a window, the method comprising:
providing a base glass comprising SiO2, Al2O3, and Li2O3; and
exposing the base glass to a mixed melt comprising a strengthening molten salt and an additive,
wherein the strengthening molten salt is a mixed salt containing two or more ions selected from the group consisting of Li+, Na+, K+, Rb+ and Cs+ or a single salt containing any one ion selected from the group consisting of Li+, Na+, K+, Rb+ and Cs+, and
wherein the additive includes Al2(SO4)3, Al(NO3)3, K2SiO3, Na2SiO3, KCl, Ca(NO3)2, and/or Mg(NO3)2.

### Claim 15 (depends on 14)

The method of claim 14, wherein:
the strengthening molten salt comprises KNO3 and/or NaNO3; and
the additive comprises Al2(SO4)3 or Al(NO3)3.

### Claim 16 (depends on 14)

The method of claim 14, wherein the additive is included in the mixed melt an amount of 0 wt % to 10 wt % with respect to a total weight of the mixed melt.

### Claim 17

A method for manufacturing a window, the method comprising:
providing a base glass;
exposing the base glass to a mixed melt comprising a first strengthening molten salt and an additive; and
exposing the base glass, that has been exposed to the mixed melt, to a melt comprising a second strengthening molten salt.
wherein the additive comprises Al2(SO4)3, Al(NO3)3, K2SiO3, Na2SiO3, KCl, Ca(NO3)2, and/or Mg(NCO3).

### Claim 18 (depends on 17)

The method of claim 17, wherein the base glass comprises SiO3, Al2O3, and Li2O3.

### Claim 19 (depends on 17)

The method of claim 17, wherein
the mixed melt comprises Al2(SO4)3 and Al(NO3)3, and/or NaNO3; and
the melt comprises KNO3.

### Claim 20 (depends on 17)

The method of claim 17, further comprising forming a printing layer on an upper surface of the base glass and/or a lower surface of the base glass after the base glass has been exposed to the melt,
wherein, the base glass is not polished after having exposed the base glass to the melt and before forming the printing layer.