# US 2022/0017398 A1 · Method for decreasing bubble lifetime on a glass melt surface

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0017398 A1
- Document ID: US20220017398A1
- Status: Published application
- Kind: A1
- Application number: 17/294,833
- Filed: 2019-11-14
- Published: 2022-01-20
- Earliest claimed: 2018-11-21
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: Laura Rose Van Cott Adkins; William Gurney Dorfeld
- Web page: https://patentgrep.com/patent/US20220017398A1

## CPC

- C03B 5/235: Heating the glass (C03B5/02, C03B5/18, C03B5/225 take precedence)
- C03B 7/07: Electric means
- C03B 5/16: Special features of the melting process; Auxiliary means specially adapted for glass-melting furnaces
- C03B 5/20: Bridges, shoes, throats, or other devices for withholding dirt, foam, or batch
- C03B 5/225: Refining (C03B5/18 takes precedence {; Refining agents C03C1/004})
- C03B 7/096: for heating
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES

## Abstract

A method of reducing bubble lifetime on the free surface of a volume of molten glass contained within or flowing through a vessel including a free volume above the free surface, thereby minimizing re-entrainment of the bubbles back into the volume of molten glass and reducing the occurrence of blisters in finished glass products. The method includes vaporizing a volatile material, entraining the vapor in a carrier gas to form an enrichment gas, and flowing the enrichment gas into the free volume to increase a concentration of the volatile material at the surface of the molten glass in the vessel.

## Claims

### Claim 1

A method of reducing bubble lifetime in a glass making process, comprising:
forming molten glass in a melting vessel;
directing the molten glass through a conditioning vessel downstream of the melting vessel, the conditioning vessel comprising a free volume above a free surface of the molten glass in the conditioning vessel; and
flowing an enrichment gas comprising a volatile material into the free volume, the volatile material reducing a surface tension of the molten glass in the conditioning vessel.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the flowing an enrichment gas comprises flowing a carrier gas over a source of the volatile material and heating the source of volatile material.

### Claim 3 (depends on 2)

The method according to claim 2, further comprising controlling a concentration of the volatile material in the enrichment gas by controlling a temperature of the source of volatile material.

### Claim 4 (depends on 1)

The method according to claim 1, wherein an atmosphere in the free volume is saturated with the volatilized material.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the conditioning vessel comprises a fining vessel or a stirring vessel.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the volatile material comprises B2O3.

### Claim 7

A method of reducing bubble lifetime in a glass making process, comprising:
forming a molten glass in a melting vessel;
flowing the molten glass through a conditioning vessel downstream of the melting vessel, the conditioning vessel comprising a free volume above a free surface of the molten glass;
flowing a carrier gas through a surfactant distribution vessel comprising a source of B2O3;
heating the surfactant distribution vessel to melt the source of B2O3 and form a boron-comprising vapor;
entraining the boron-comprising vapor in the carrier gas to form an enrichment gas; and
flowing the enrichment gas into the free volume of the conditioning vessel.

### Claim 8 (depends on 7)

The method according to claim 7, wherein the free volume comprises an atmosphere, and a concentration of B2O3 in the atmosphere is maintained in saturation.

### Claim 9 (depends on 7)

The method according to claim 7, wherein a partial pressure of B2O3 in the free volume is equal to or greater than a partial pressure of B2O3 within a bubble in the molten glass.

### Claim 10 (depends on 7)

The method according to claim 7, wherein a partial pressure of B2O3 in the free volume is controlled by controlling a temperature of the source of B2O3 in the surfactant distribution vessel.

### Claim 11 (depends on 7)

The method according to claim 7, wherein the source of B2O3 is pure B2O3.

### Claim 12 (depends on 7)

The method according to claim 7, wherein the molten glass in the conditioning vessel is a first molten glass and the source of B2O3 is a second molten glass.

### Claim 13 (depends on 7)

The method according to claim 7, wherein the conditioning vessel comprises a fining vessel.

### Claim 14 (depends on 7)

The method according to claim 7, wherein the conditioning vessel comprises a stirring vessel.

### Claim 15 (depends on 7)

The method according to claim 7, further comprising directing the first molten glass from the conditioning vessel to a forming body and drawing the first molten glass from the forming body.

### Claim 16

An apparatus for processing molten glass, comprising:
a melting vessel configured to form molten glass;
a conditioning vessel downstream of the melting vessel and configured to receive the molten glass from the melting vessel, the conditioning vessel containing a free volume above a free surface of the molten glass in the conditioning vessel; and
a surfactant distribution vessel in fluid communication with the conditioning vessel, the surfactant distribution vessel containing a source of volatile material; and
a carrier gas source in fluid communication with the surfactant distribution vessel.

### Claim 17 (depends on 16)

The apparatus according to claim 16, wherein the source of volatile material comprises B2O3.

### Claim 18 (depends on 16)

The apparatus according to claim 16, wherein a heating element is arranged to heat the surfactant distribution vessel.