# US 2022/0016579 A1 · Polymer electrolyte membrane and method for manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0016579 A1
- Document ID: US20220016579A1
- Status: Published application
- Kind: A1
- Application number: 17/067,628
- Filed: 2020-10-09
- Published: 2022-01-20
- Earliest claimed: 2020-07-15
- Assignees: Korea Petrochemical Ind. Co., Ltd
- Applicants: Korea Petrochemical Ind. Co., Ltd.
- Inventors: Sung Kuk JEONG; Yoon Hyun PARK; Ho Jin SON; Gil Soon KANG; Young Tae JEONG
- Web page: https://patentgrep.com/patent/US20220016579A1

## CPC

- B01D 71/24: Rubbers
- H01M 8/1023: having only carbon, e.g. polyarylenes, polystyrenes or polybutadiene-styrenes
- B01D 67/0002: {Organic membrane manufacture}
- B01D 67/00931: {by introduction of specific groups after membrane formation, e.g. by grafting}
- B01D 69/02: characterised by their properties
- B01D 71/261: {Polyethylene}
- B01D 71/281: {Polystyrene}
- H01M 8/1044: Mixtures of polymers, of which at least one is ionically conductive
- H01M 8/1083: {Starting from polymer melts other than monomer melts}
- H01M 8/1088: Chemical modification, e.g. sulfonation
- H01M 8/18: Regenerative fuel cells, e.g. redox flow batteries or secondary fuel cells
- H01M 8/227: {Dialytic cells or batteries; Reverse electrodialysis cells or batteries}
- B01D 2325/04: Characteristic thickness
- B01D 2325/26: Electrical properties
- B01D 2325/42: Ion-exchange membranes
- H01M 2008/1095: {Fuel cells with polymeric electrolytes}
- H01M 2300/0082: Organic polymers
- H01M 2300/0091: in the form of mixtures
- Y02E 60/50: Fuel cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

According to an embodiment, there is provided a polymer electrolyte membrane, comprising a polymer film including a styrene-based resin, a polyolefin-based resin, and an olefin-based elastomer resin. The polymer film is bonded with a sulfonic acid group (—SO3H) capable of cation exchange through a sulfonation reaction.

## Claims

### Claim 1

A polymer electrolyte membrane, comprising a polymer film including a styrene-based resin, a polyolefin-based resin, and an olefin-based elastomer resin, wherein the polymer film is bonded with a sulfonic acid group (—SO3H) capable of cation exchange through a sulfonation reaction.

### Claim 2 (depends on 1)

The polymer electrolyte membrane of claim 1, wherein the styrene-based resin, the polyolefin-based resin, and the olefin-based elastomer resin are mixed in a weight ratio of 20 to 50:50 to 75:0 to 10, respectively.

### Claim 3 (depends on 1)

The polymer electrolyte membrane of claim 1, wherein the styrene-based resin is one or more selected from the group consisting of polystyrene (PS), acrylonitrile-butadiene-styrene (ABS), styrene-ethylene-butylene-styrene (SEBS), styrene-butadiene-styrene (SBS), and styrene-butadiene-rubber (SBR).

### Claim 4 (depends on 1)

The polymer electrolyte membrane of claim 1, wherein the polyolefin-based resin is one or more selected from the group consisting of polypropylene (PP), linear low density polyethylene (LLDPE), low density polyethylene (LDPE), high density polyethylene (HDPE), ultra-high molecular weight polyethylene (UHMWPE), polymethylpentene (PMP), and cyclic olefin copolymer (COC).

### Claim 5 (depends on 1)

The polymer electrolyte membrane of claim 1, wherein the olefin-based elastomer resin is one or more selected from the group consisting of ethylene-propylene rubber (EPR) and ethylene-propylene-non-conjugated diene rubber (EPDM).

### Claim 6 (depends on 1)

The polymer electrolyte membrane of claim 1, wherein the polymer electrolyte membrane has an ion conductivity (IC) of 60 mS/cm or more at 80° C. and an ion exchange capacity (IEC) of 0.9 meq/g or more.

### Claim 7

A method for manufacturing a polymer electrolyte membrane, the method comprising:
a first step of preparing a mixture by blending a styrene-based resin, a polyolefin-based resin, and an olefin-based elastomer resin in a weight ratio of 20 to 50:50 to 75:0 to 10, respectively;
a second step of putting the mixture into an extruder and preparing pellets;
a third step of preparing a polymer film by performing inflation, casting, biaxial stretching, lamination, and bottom-up inflation extrusion processing on the pellets; and
a fourth step of bonding the polymer film with a sulfonic acid group (—SO3H) via a sulfonation reaction using a sulfone solution and a solvent.

### Claim 8 (depends on 7)

The method of claim 7, wherein the polymer film has a thickness ranging from 5 μm to 200 μm.

### Claim 9 (depends on 7)

The method of claim 7, wherein the sulfone solution is one selected from the group consisting of sulfuric acid, fuming sulfuric acid, chlorosulfonic acid, and acetylsulfate, and wherein the solvent is one or more selected from the group consisting of methylene chloride (MC), ethylene dichloride (EDC), dimethyl sulfoxide (DMSO), and dimethylacetamide (DMAC).

### Claim 10 (depends on 7)

The method of claim 7, wherein the sulfonation reaction includes immersing the polymer film in a sulfone solution at 25° C. to 60° C. for 1 to 4 hours to perform the sulfonation reaction and then re-immersing the polymer film in a 0.5M sodium hydroxide (NaOH) aqueous solution for 2 hours to terminate the sulfonation reaction.