# US 2022/0013815 A1 · Process for Recycling Cobalt and Nickel from Lithium Ion Batteries

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0013815 A1
- Document ID: US20220013815A1
- Status: Published application
- Kind: A1
- Application number: 17/218,863
- Filed: 2021-03-31
- Published: 2022-01-13
- Earliest claimed: 2020-07-08
- Assignees: American Hyperform, Inc.
- Applicants: American Hyperform, Inc.
- Inventors: William Novis Smith; Scott D. Swoffer
- Web page: https://patentgrep.com/patent/US20220013815A1

## CPC

- H01M 10/4242: {Regeneration of electrolyte or reactants}
- C01G 53/84: Hydroxides
- C22B 1/005: {Preliminary treatment of scrap (C22B1/02 - C22B1/26 take precedence)}
- C22B 7/007: {by acid leaching}
- C22B 23/043: {Sulfurated acids or salts thereof}
- C22B 23/0461: {by chemical methods}
- C22B 26/12: Obtaining lithium
- C22B 47/0063: {with acids or salt solutions (C22B47/0072 takes precedence)}
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 4/583: Carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/54: Reclaiming serviceable parts of waste accumulators
- Y02E 60/10: Energy storage using batteries
- Y02P 10/20: Recycling
- Y02W 30/84: Recycling of batteries or fuel cells
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

A process for recovering a nickel cobalt manganese hydroxide from recycled lithium-ion battery (LIB) material such as black mass, black powder, filter cake, or the like. The recycled LIB material is mixed with water and either sulfuric acid or hydrochloric acid at a pH less than 2. Cobalt, nickel, and manganese oxides from the recycled lithium-ion battery material dissolve into the acidic water with the reductive assistance of gaseous sulfur dioxide. Anode carbon is filtered from the acidic water, leaving the dissolved cobalt, nickel, and manganese oxides in a filtrate. The filtrate is mixed with aqueous sodium hydroxide at a pH greater than 8. Nickel cobalt manganese hydroxide precipitates from the filtrate. The nickel cobalt manganese hydroxide is filtered from the filtrate and dried. The filtrate may be treated ammonium fluoride or ammonium bifluoride to precipitate lithium fluoride from the filtrate. The composition ratio of nickel to cobalt to manganese in the acid filtrate may be adjusted to a desired ratio. The anode carbon is recovered and purified for reuse.

## Claims

### Claim 1

A process for recovering a nickel cobalt manganese hydroxide from a recycled lithium-ion battery material, comprising:
a. Mixing a recycled lithium-ion battery material with an acidic water having a pH less than 2, the acidic water including water and an acid from the group of sulfuric acid and hydrochloric acid;
b. Adding a reducing agent to the recycled lithium-ion battery material;
c. Dissolving normally acid insoluble manganese oxides from the recycled lithium-ion battery material into the acidic water;
d. Dissolving higher valent cobalt oxides and nickel oxides from the recycled lithium-ion battery material into the acidic water;
e. Filtering an anode carbon and other insoluble materials from the acidic water, where the dissolved cobalt, nickel, and manganese oxides remain in a filtrate;
f. Mixing the filtrate with an alkali metal hydroxide until the pH of the filtrate is greater than 8;
g. Precipitating a nickel cobalt manganese hydroxide from the filtrate; and
h. Filtering the nickel cobalt manganese hydroxide from the filtrate.

### Claim 2 (depends on 1)

The process of claim 1, where the acidic water has a pH in the range of 0.2 to 2.0.

### Claim 3 (depends on 2)

The process of claim 2, where the acidic water has a pH of 0.5.

### Claim 4 (depends on 1)

The process of claim 1, further comprising adding the reducing agent in a closed system to achieve an approximately stoichiometric addition, where the reducing agent is gaseous sulfur dioxide.

### Claim 5 (depends on 4)

The process of claim 4 further comprising determining of the approximately stoichiometric amount of sulfur dioxide by cessation of gas absorption in the range of 70° C. to 90° C. at a pH less than 2.

### Claim 6 (depends on 4)

The process of claim 4, further comprising adding the sulfur dioxide in the temperature range of 40° C. to 90° C.

### Claim 7 (depends on 6)

The process of claim 6, further comprising:
a. Adding a predetermined amount of sulfuric acid; and
b. Achieving a pH of 0.5 to 2 when essentially all of the nickel cobalt, and manganese oxides have dissolved in the presence of the reducing agent.

### Claim 8 (depends on 6)

The process of claim 6 further comprising adding sufficient sulfuric acid as needed to maintain a pH of 0.5 to 2 at room temperature when dissolution completed.

### Claim 9 (depends on 1)

The process of claim 1, further comprising:
a. Mixing the filtrate with the alkali metal hydroxide until the pH of the filtrate is in the range of 3 to 5;
b. Precipitating at least one of iron, phosphate, copper, and aluminum from the filtrate; and
c. Filtering the at least one iron, phosphate, copper, and aluminum from the filtrate.

### Claim 10 (depends on 1)

The process of claim 1, further comprising mixing the filtrate with the alkali metal hydroxide until the pH of the filtrate is in the range of 10 to 12.

### Claim 11 (depends on 9)

The process of claim 9, further comprising mixing the filtrate with the alkali metal hydroxide until the pH of the filtrate is 11.

### Claim 12 (depends on 1)

The process of claim 1, where the alkali metal hydroxide is aqueous sodium hydroxide.

### Claim 13 (depends on 1)

The process of claim 1, further comprising drying the nickel cobalt manganese hydroxide.

### Claim 14 (depends on 1)

The process of claim 1, further comprising adjusting a composition ratio of nickel to cobalt to manganese in the filtrate to a desired ratio″ prior to the precipitation of the nickel cobalt manganese hydroxide with alkali metal hydroxide.

### Claim 15 (depends on 14)

The process of claim 14, further comprising adding at least two metal sulfates from the group of cobalt sulfate, nickel sulfate, and manganese sulfate.

### Claim 16 (depends on 14)

The process of claim 14, further comprising adding at least the oxide or hydroxide of two metals while the pH of the filtrate is less than 2.5.

### Claim 17 (depends on 1)

The process of claim 1, further comprising screening the recovered anode carbon to −325 mesh.

### Claim 18 (depends on 1)

The process of claim 1, further comprising;
a. Screening the recovered anode carbon to −325 mesh; and
b. Heating the recovered anode carbon to more than 250° C.

### Claim 19 (depends on 1)

The process of claim 1, further comprising:
a. Treating the final filtrate from the nickel cobalt manganese hydroxide precipitate with a water-soluble fluoride compound; and
b. Precipitating lithium fluoride from the filtrate.

### Claim 20 (depends on 19)

The process of claim 19, where the water-soluble fluoride is one of ammonium fluoride and ammonium bifluoride.

### Claim 21 (depends on 1)

The process of claim 1, where the recycled lithium-ion battery material comprises black mass.

### Claim 22

A process for recovering a nickel cobalt manganese hydroxide from a recycled lithium-ion battery material, comprising:
c0 Mixing a recycled lithium-ion battery material with an acidic water having a pH in the range of 0.2 to 1.5, the acidic water including water and an acid from the group of sulfuric acid and hydrochloric acid;″
b. Adding gaseous sulfur dioxide to the acidic water in a closed system with an approximately stoichiometric addition in the temperature range of 40° C. to 90° C.;
c. Dissolving a cobalt oxide, a nickel oxide, and a manganese oxide from the recycled lithium-ion battery material into the acidic water;
d. Filtering an anode carbon and other insoluble materials from the acidic water, where the dissolved cobalt, nickel, and manganese oxides remain as sulfates in a filtrate;
e. Mixing the filtrate with an aqueous sodium hydroxide until the pH of the filtrate is in the range of 3 to 5;
f. Precipitating at least one of iron, phosphate, copper, and aluminum from the filtrate;
g. Filtering the at least one of iron, phosphate, copper, and aluminum from the filtrate;
h. Mixing the filtrate with the aqueous sodium hydroxide until the pH of the filtrate is greater than 10;
i. Precipitating a nickel cobalt manganese hydroxide from the filtrate;
j. Filtering the nickel cobalt manganese hydroxide from the filtrate; and
k. Drying the nickel cobalt manganese hydroxide.

### Claim 23 (depends on 21)

The process of claim 21, further comprising mixing the filtrate with the aqueous sodium hydroxide until the pH of the filtrate is 11.

### Claim 24 (depends on 21)

The process of claim 21, further comprising:
a. treating the final filtrate with a water-soluble fluoride compound, where the water-soluble fluoride is one of ammonium fluoride and ammonium bifluoride; and
b. precipitating lithium fluoride from the filtrate.

### Claim 25

A process for recovering a nickel cobalt manganese hydroxide from a recycled lithium-ion battery material, comprising:
a. Mixing a recycled lithium-ion battery material with an acidic water having a pH in the range of 0.2 to 1.0, the acidic water including water and an acid from the group of sulfuric acid and hydrochloric acid;
b. Adding gaseous sulfur dioxide to the acidic water in a closed system with an approximately stoichiometric addition in the temperature range of 40° C. to 90° C.;
c. Dissolving a cobalt oxide, a nickel oxide, and a manganese oxide from the recycled lithium-ion battery material into the acidic water;
d. Filtering an anode carbon and other insoluble materials from the acidic water, where the dissolved cobalt, nickel, and manganese oxides remain in a filtrate;
e. Mixing the filtrate with an aqueous sodium hydroxide until the pH of the filtrate is in the range of 3 to 5;
f. Precipitating at least one of iron, phosphate, copper, and aluminum from the filtrate;
g. Filtering the at least one iron, phosphate, and aluminum from the filtrate;
h. Adjusting a composition ratio of nickel to cobalt to manganese in the filtrate to a desired ratio.
i. Mixing the filtrate with the aqueous sodium hydroxide until the pH of the filtrate is greater than 10;
j. Precipitating a nickel cobalt manganese hydroxide from the filtrate;
k. Filtering the nickel cobalt manganese hydroxide from the filtrate; and
l. Drying the nickel cobalt manganese hydroxide.

### Claim 26 (depends on 24)

The process of claim 24, further comprising adding at least two metal sulfates from the group of cobalt sulfate, nickel sulfate, and manganese sulfate.

### Claim 27 (depends on 24)

The process of claim 24 further comprising, where the composition ration is an atomic ration, selecting the atomic ratio for a specific lithium-ion battery cathode composition.

### Claim 28 (depends on 24)

The process of claim 24, further comprising mixing the filtrate with the aqueous sodium hydroxide until the pH of the filtrate is 11.

### Claim 29 (depends on 24)

The process of claim 24, further comprising:
a. Treating the filtrate with a water-soluble fluoride compound, where the water-soluble fluoride is one of ammonium fluoride and ammonium bifluoride; and
b. Precipitating lithium fluoride from the filtrate.

### Claim 30 (depends on 24)

The process of claim 24 further comprising adjusting the composition ratio of nickel to cobalt to manganese to a desired ratio after a first filtration.