# US 2022/0013762 A1 · Lithium positive electrode active material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0013762 A1
- Document ID: US20220013762A1
- Status: Published application
- Kind: A1
- Application number: 17/289,313
- Filed: 2019-12-18
- Published: 2022-01-13
- Earliest claimed: 2018-12-19
- Assignees: Haldor TopsøE A/S
- Applicants: Haldor TopsøE A/S
- Inventors: Jonathan HØJBERG; Jakob Weiland HØJ; Christian Fink ELKJÆR; Lars Fahl LUNDEGAARD; Søren DAHL
- Web page: https://patentgrep.com/patent/US20220013762A1

## CPC

- C01G 53/52: of the type (Mn2O4)2-, e.g. Li2(NixMn2-x)O4 or Li2(MyNixMn2-x-y)O4
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- C01G 45/1242: of the type (Mn2O4)-, e.g. LiMn2O4 or Li(MxMn2-x)O4
- C01G 53/54: of the type (Mn2O4)-, e.g. Li(NixMn2-x)O4 or Li(MyNixMn2-x-y)O4
- H01M 4/485: of mixed oxides or hydroxides for inserting or intercalating light metals, e.g. LiTi2O4 or LiTi2OxFy (H01M4/505, H01M4/525 take precedence)
- C01P 2002/32: spinel-type (AB2O4)
- C01P 2002/76: by a space-group or by other symmetry indications
- C01P 2004/54: Particles characterised by their aspect ratio, i.e. the ratio of sizes in the longest to the shortest dimension
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2006/11: Powder tap density
- C01P 2006/12: Surface area
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The invention relates to a lithium positive electrode active material for a high voltage secondary battery: the lithium positive electrode active material comprising at least 94 wt % spinel, where the spinel has a net chemical composition of LixNiyMn2-yO4, wherein: 0.95≤x≤1.05; 0.43≤y≤0.47. The lithium positive electrode active material is made up of particles characterized by one or more of the following parameter ranges: the particles have average aspect ratio below 1.6, the particles have a roughness below 1.35, particles have a circularity above 0.55. Then invention also relates to a process for the preparation of the lithium positive electrode active material as well as a secondary battery comprising the lithium positive electrode active material.

## Claims

### Claim 1

A lithium positive electrode active material for a high voltage secondary battery, said lithium positive electrode active material comprising at least 94 wt % spinel, said spinel having a net chemical composition of LixNiyMn2-yO4, wherein:
0.95≤x≤1.05;
0.43≤y≤0.47; and
wherein said lithium positive electrode active material is made up of particles, said particles being characterized by one or more of the following parameter ranges: the particles have average aspect ratio below 1.6, the particles have a roughness below 1.35, particles have a circularity above 0.55.

### Claim 2 (depends on 1)

The lithium positive electrode active material according to claim 1, where at least 90 wt % of said spinel is crystallized in disordered space group Fd-3m.

### Claim 3 (depends on 1)

The lithium positive electrode active material according to claim 1, wherein said lithium positive electrode active material in a half-cell has a difference of at least 50 mV between the potentials at 25% and 75% of the capacity above 4.3 V during discharge with a current of around 29 mA/g.

### Claim 4 (depends on 1)

The lithium positive electrode active material according claim 1, wherein said lithium positive electrode active material is calcined so that the lattice parameter a is between 8.171 and 8.183 Å.

### Claim 5 (depends on 4)

The lithium positive electrode active material according to claim 4, wherein the lattice parameter a is between (−0.1932y+8.2613) Å and 8.183 Å.

### Claim 6 (depends on 4)

The lithium positive electrode active material according to claim 4, wherein the lattice parameter a is between (−0.1932y+8.2613) Å and (−0.1932y+8.2667) Å.

### Claim 7 (depends on 4)

The lithium positive electrode active material according to claim 4, wherein the lattice parameter a is between (−0.1932y+8.2613) Å and (−0.1932y+8.2641) Å.

### Claim 8 (depends on 1)

The lithium positive electrode active material according to claim 1, wherein said lithium positive electrode active material has a tap density equal to or greater than 2.2 g/cm3.

### Claim 9 (depends on 1)

The lithium positive electrode active material according to claim 1, wherein D50 of the particles of said lithium positive electrode active material satisfies: 3 μm<D50<12 μm.

### Claim 10 (depends on 1)

The lithium positive electrode active material according to claim 1, wherein the BET area of said lithium positive electrode active material is below 1.5 m2/g.

### Claim 11 (depends on 1)

The lithium positive electrode active material according to claim 1, wherein said particles are characterized by a solidity above 0.8.

### Claim 12 (depends on 1)

The lithium positive electrode active material according to claim 1, wherein said particles are characterized by a porosity below 3%.

### Claim 13 (depends on 1)

The lithium positive electrode active material according to claim 1, wherein 0.99≤x≤1.01.

### Claim 14 (depends on 1)

The lithium positive electrode active material according to claim 1, wherein the capacity of said material in a half cell decreases by no more than 4% over 100 cycles between 3.5 to 5.0 V at 55° C.

### Claim 15 (depends on 1)

The lithium positive electrode active material according to claim 1, wherein said lithium positive electrode active material has a capacity of at least 138 mAh/g.

### Claim 16 (depends on 1)

The lithium positive electrode active material according to claim 1, wherein said lithium positive electrode active material is synthesized from a precursor containing Li, Ni, and Mn in a ratio Li:Ni:Mn: X:Y:2-Y, wherein: 0.95≤X≤1.05; and 0.42≤Y<0.5.

### Claim 17 (depends on 1)

The lithium positive electrode active material according to claim 1, wherein y is determined by means of a method selected from the group consisting of electrochemical determination, X-ray diffraction and scanning transmission electron microscopy (STEM) in combination with energy dispersive X-ray spectroscopy (EDS).

### Claim 18 (depends on 1)

The lithium positive electrode active material according to claim 1, wherein 0.43≤y<0.45.

### Claim 19 (depends on 1)

A process for the preparation of a lithium positive electrode active material according to claim 1, said process comprising the steps of:
a. providing precursors for preparing said lithium positive electrode active material comprising at least 94 wt % spinel having a chemical composition of LixNiyMn2-yO4 wherein 0.95≤x≤1.05; and 0.43≤y≤0.47;
b. sintering the precursors of step a. by heating the precursors to a temperature of between 500° C. and 1200° C. to provide a sintered product,
c. cooling the sintered product of step b to room temperature.

### Claim 20 (depends on 19)

The process according to claim 19, wherein part of step b is carried out in a reducing atmosphere.

### Claim 21 (depends on 19)

The process according to claim 19, wherein said temperature of step b is between 850° C. and 1100° C.

### Claim 22 (depends on 19)

The process according to claim 19, wherein during the cooling of step c, the temperature is maintained in an interval between 750° C. and 650° C. for a sufficient amount of time to obtain at least 94% phase purity of said lithium positive electrode active material.

### Claim 23 (depends on 19)

The process according to claim 19, wherein at least one of the precursors is a precipitated compound.

### Claim 24 (depends on 19)

The process according to claim 19, wherein the precipitated compound is a co-precipitated compound of Ni and Mn formed in a Ni—Mn co-precipitation step.

### Claim 25 (depends on 24)

The process according to claim 24, wherein, said precursor in the form of a co-precipitated Ni—Mn has been prepared in a precipitation step, wherein a first solution of a Ni containing starting material, a second solution of a Mn containing starting material and a third solution of a precipitating anion are added simultaneously to a liquid reaction medium in a reactor in such amounts that in relation to the added Ni, each of Mn and the precipitating anion are added in a ratio of from 1:10 to 10:1, relative to the stoichiometric amounts of the precipitate.

### Claim 26 (depends on 25)

The process according to claim 25, wherein the first, second and third solutions are added to the reaction medium amounts calibrated so as to maintain the pH of the reaction mixture at alkaline pH of between 8.0 and 10.0.

### Claim 27 (depends on 25)

The process of any of claim 25, wherein said first, second and third solutions are added to the reaction mixture over a prolonged period of between 2.0 and 11 hours.

### Claim 28 (depends on 25)

The process of claim 25, wherein said first, second and third solutions are added to the reaction mixture under vigorous stirring providing a power input of from 2 W/L to 25 W/L.

### Claim 29 (depends on 1)

A secondary battery comprising the lithium positive electrode active material according to claim 1.

### Claim 30 (depends on 1)

Use of the lithium positive electrode active material according to claim 1 for reducing the degradation of the material during storage and use.