# US 2022/0011663 A1 · Extreme ultraviolet mask absorber materials

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0011663 A1
- Document ID: US20220011663A1
- Status: Published application
- Kind: A1
- Application number: 17/370,406
- Filed: 2021-07-08
- Published: 2022-01-13
- Earliest claimed: 2020-07-13
- Assignees: Applied Materials, Inc.
- Applicants: Applied Materials, Inc.
- Inventors: Shuwei Liu; Shiyu Liu; Vibhu Jindal
- Web page: https://patentgrep.com/patent/US20220011663A1

## CPC

- G03F 1/24: Reflection masks; Preparation thereof
- G03F 1/54: Absorbers, e.g. of opaque materials
- G03F 1/58: having two or more different absorber layers, e.g. stacked multilayer absorbers
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)

## Abstract

Extreme ultraviolet (EUV) mask blanks, methods for their manufacture and production systems therefor are disclosed. The EUV mask blanks comprise a substrate; a multilayer stack of reflective layers on the substrate; and an absorber layer comprising tantalum and iridium or ruthenium and antimony.

## Claims

### Claim 1

A method of manufacturing an extreme ultraviolet (EUV) mask blank comprising:
forming on a substrate a multilayer stack which reflects EUV radiation, the multilayer stack comprising a plurality of reflective layer pairs; and
forming an absorber layer on the multilayer stack, the absorber layer selected from an alloy of tantalum and iridium; and an alloy of ruthenium and antimony.

### Claim 2 (depends on 1)

The method of claim 1, wherein the alloy of tantalum and iridium comprises from about 14 wt. % to about 86 wt. % tantalum and from about 14 wt. % to about 86 wt. % iridium.

### Claim 3 (depends on 1)

The method of claim 1, wherein the alloy of ruthenium and antimony comprises from about 4 wt. % to about 96 wt. % ruthenium and from about 4 wt. % to about 96 wt. % antimony.

### Claim 4 (depends on 2)

The method of claim 2, wherein the alloy of tantalum and iridium is amorphous.

### Claim 5 (depends on 3)

The method of claim 3, wherein the alloy of ruthenium and antimony is amorphous.

### Claim 6 (depends on 1)

The method of claim 1, wherein the alloy is formed by co-sputtered tantalum and iridium with a gas selected from one or more of argon (Ar), oxygen (O2), or nitrogen (N2) to form the absorber layer.

### Claim 7 (depends on 1)

The method of claim 1, wherein the alloy is deposited layer by layer as a laminate of alternate layers selected from tantalum and iridium layers and ruthenium and antimony layers using a gas selected from one or more of argon (Ar), oxygen (O2), or nitrogen (N2) to form the absorber layer.

### Claim 8 (depends on 1)

The method of claim 1, wherein the alloy is deposited using a bulk target having a same composition as the alloy and is sputtered using a gas selected from one or more of argon (Ar), oxygen (O2), or nitrogen (N2) to form the absorber layer.

### Claim 9 (depends on 2)

The method of claim 2, wherein the alloy of tantalum and iridium is doped with one of more of nitrogen or oxygen in a range of from 0.1 wt. % to 5 wt. %.

### Claim 10 (depends on 1)

The method of claim 1, wherein the alloy is doped with one of more of nitrogen or oxygen in a range of from about 0.1 wt. % to about 5 wt. %.

### Claim 11

An extreme ultraviolet (EUV) mask blank comprising:
a substrate;
a multilayer stack which reflects EUV radiation, the multilayer stack comprising a plurality of reflective layer pairs; and
an absorber layer on the multilayer stack selected from an alloy of tantalum and iridium; and an alloy of ruthenium and antimony.

### Claim 12 (depends on 11)

The extreme ultraviolet (EUV) mask blank of claim 11, wherein the alloy of tantalum and iridium comprises from about 14 wt. % to about 86 wt. % tantalum and from about 14 wt. % to about 86 wt. % iridium.

### Claim 13 (depends on 11)

The extreme ultraviolet (EUV) mask blank of claim 11, the alloy of ruthenium and antimony comprises from about 4 wt. % to about 96 wt. % ruthenium and from about 4 wt. % to about 96 wt. % antimony.

### Claim 14 (depends on 12)

The extreme ultraviolet (EUV) mask blank of claim 12, wherein the alloy of tantalum and iridium is amorphous.

### Claim 15 (depends on 13)

The extreme ultraviolet (EUV) mask blank of claim 13, wherein the alloy of ruthenium and antimony is amorphous.

### Claim 16 (depends on 11)

The extreme ultraviolet (EUV) mask blank of claim 11, wherein the absorber layer has a thickness of less than 60 nm.

### Claim 17 (depends on 11)

The extreme ultraviolet (EUV) mask blank of claim 11, wherein the absorber layer further comprises a range of from about 0.1 wt. % to about 5 wt. % of a dopant selected from one or more of nitrogen or oxygen.

### Claim 18 (depends on 11)

The extreme ultraviolet (EUV) mask blank of claim 11, wherein the absorber layer has a thickness of less than 60 nm.

### Claim 19 (depends on 11)

The extreme ultraviolet (EUV) mask blank of claim 11, wherein the absorber layer is etch selective relative to the capping layer.

### Claim 20

An extreme ultraviolet (EUV) mask blank comprising:
a substrate;
a multilayer stack which reflects EUV radiation, the multilayer stack comprising a plurality of reflective layer pairs including molybdenum (Mo) and silicon (Si); and
an absorber layer on the multilayer stack selected from an alloy of tantalum and iridium and an alloy of ruthenium and antimony.