# US 2022/0010456 A1 · Method for manufacturing transition metal chalcogenide and transition metal chalcogenide prepared thereby

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0010456 A1
- Document ID: US20220010456A1
- Status: Published application
- Kind: A1
- Application number: 16/925,674
- Filed: 2020-07-10
- Published: 2022-01-13
- Earliest claimed: 2020-07-10
- Assignees: Korea Advanced Institute of Science and Technology
- Applicants: Korea Advanced Institute of Science and Technology
- Inventors: Sung-Yool Choi; Woonggi Hong; Gi Woong Shim
- Web page: https://patentgrep.com/patent/US20220010456A1

## CPC

- C30B 31/18: Controlling or regulating
- C23C 16/305: {Sulfides, selenides, or tellurides}
- C30B 25/02: Epitaxial-layer growth
- C30B 29/46: Sulfur-, selenium- or tellurium-containing compounds
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

The present disclosure provides a method for preparing a transition metal chalcogenide including: a step of forming a transition metal chalcogenide thin film; and a step of controlling the defects of the transition metal chalcogenide thin film by injecting a processing gas including oxygen and nitrogen to the formed transition metal chalcogenide thin film.

## Claims

### Claim 1

A method for preparing a transition metal chalcogenide comprising:
a step of forming a transition metal chalcogenide thin film; and
a step of controlling the defects of the transition metal chalcogenide thin film by injecting a processing gas comprising oxygen to the formed transition metal chalcogenide thin film.

### Claim 2 (depends on 1)

The method for preparing a transition metal chalcogenide of claim 1, wherein the step of forming the transition metal chalcogenide thin film comprises:
a step of forming crystal nuclei of a transition metal chalcogenide on a substrate; and
a step of growing a transition metal chalcogenide from the crystal nuclei of a transition metal chalcogenide.

### Claim 3 (depends on 1)

The method for preparing a transition metal chalcogenide of claim 1, wherein the volume ratio of O2 in the processing gas is 1-10 wt %.

### Claim 4 (depends on 3)

The method for preparing a transition metal chalcogenide of claim 3, wherein the processing gas comprises O2 and N2.

### Claim 5

(canceled)

### Claim 6 (depends on 1)

The method for preparing a transition metal chalcogenide of claim 1, wherein chalcogenide vacancies are formed through the step of controlling the defects and oxygen is bound to the chalcogenide vacancies.

### Claim 7 (depends on 6)

The method for preparing a transition metal chalcogenide of claim 6, wherein the transition metal chalcogenide comprises one or more selected from a group consisting of MoS2, MoSe2, MoTe2, WS2, WSe2 and WTe2.

### Claim 8 (depends on 7)

The method for preparing a transition metal chalcogenide of claim 7, wherein the transition metal chalcogenide is MoS2 and sulfur vacancies are formed through the step of controlling the defects.

### Claim 9 (depends on 1)

A transition metal chalcogenide prepared by the method of claim 1.

### Claim 10 (depends on 9)

The transition metal chalcogenide of claim 9, wherein oxygen is located on chalcogenide vacancies of the transition metal chalcogenide.

### Claim 11

A method for preparing a transition metal chalcogenide comprising:
forming a transition metal chalcogenide thin film; and
controlling the defects of the transition metal chalcogenide thin film by injecting an oxygen-containing processing gas.

### Claim 12 (depends on 11)

The method for preparing a transition metal chalcogenide of claim 11, wherein the processing gas comprises O2 and N2.

### Claim 13 (depends on 12)

The method for preparing a transition metal chalcogenide of claim 12, wherein the volume ratio of O2 in the processing gas is 1-10 wt %.

### Claim 14 (depends on 11)

The method for preparing a transition metal chalcogenide of claim 11, wherein n-doping occurs in the transition metal chalcogenide through the control of the defects.

### Claim 15 (depends on 11)

The method for preparing a transition metal chalcogenide of claim 11, wherein the transition metal chalcogenide comprises one or more selected from a group consisting of MoS2, MoSe2, MoTe2, WS2, WSe2 and WTe2.

### Claim 16 (depends on 2)

The method for preparing a transition metal chalcogenide of claim 2, wherein a temperature of the defect control step is higher than room temperature and lower than a temperature of the growth step.

### Claim 17 (depends on 1)

The method for preparing a transition metal chalcogenide of claim 1, wherein n-doping occurs in the transition metal chalcogenide through the control of the defects.